1-20 of 1757 Search Results for

rolled bars

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1966) 15 (10): SA-202.
Published: 01 October 1966
... can be obtained with castings or by fabrication from rolled bars, sheets or plates. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing...
Journal Articles
Alloy Digest (1990) 39 (6): CS-127.
Published: 01 June 1990
... UNS G10370 is a medium carbon, plain carbon steel. In bar form the steel is often used in the as-hot rolled condition. Cold drawn bars have attractive combinations of mechanical and dimensional properties and are widely used in mass production of machined and other parts. UNS G10370 is also used...
Journal Articles
Alloy Digest (1980) 29 (5): SA-372.
Published: 01 May 1980
... REPUBLIC X-80-W is a high-strength, low-alloy steel developed to achieve a minimum yield strength of 80,000 psi in the as-hot-rolled condition. It also exhibits good fatigue performance, good bendability, and good weldability. It is available as bars and can be used in various automotive...
Journal Articles
Alloy Digest (1989) 38 (5): CS-124.
Published: 01 May 1989
... UNS G10370 is a medium carbon, plain carbon steel. In bar form the steel is often used in the as-hot rolled condition. Cold drawn bars have attractive combinations of mechanical and dimensional properties and are widely used in mass production of machined and other parts. UNS G10370 is also used...
Journal Articles
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-85.
Published: 01 August 2000
... CMW 3 is an age-hardenable copper-base alloy combining high mechanical and electrical properties. The alloy is typically used for spot and seam welding cold and hot-rolled steels and coated materials, current carrying shafts and arms, back-up bars, back-up bars for arc welding, electrical current...
Journal Articles
Alloy Digest (2017) 66 (1): SA-777.
Published: 01 January 2017
... properties This datasheet applies to thermomechanically rolled flat plate products in thicknesses up to 60 mm (2.4 in This steel grade is distinguished by testing by notch-bar impact test to 20 °C (-4 °F) minimum. Chemical Composition, wt (Maximum) Carbon 0.13 Silicon 0.50 Manganese 1.60 Phosphorus 0.025...
Journal Articles
Alloy Digest (2017) 66 (2): SA-778.
Published: 01 February 2017
... properties This datasheet applies to thermomechanically rolled flat plate products in thicknesses up to 60 mm (2.4 in This steel grade is distinguished by testing by notch-bar impact test to 20 °C (-4 °F) minimum. Chemical Composition, wt (Maximum) Carbon 0.14 Silicon 0.50 Manganese 1.70 Phosphorus 0.025...
Journal Articles
Alloy Digest (2017) 66 (6): SA-786.
Published: 01 June 2017
... to thermomechanically rolled flat plate products in thicknesses up to 60 mm (2.4 in This steel grade is distinguished by testing by notch-bar impact test to 20 °C ( 4 °F) minimum. Chemical Composition, wt (Maximum) Carbon 0.15 Silicon 0.60 Manganese 1.80 Phosphorus 0.025 Sulfur 0.015 Copper 0.40 Niobium 0.05 Nickel...
Journal Articles
Alloy Digest (1983) 32 (9): SS-432.
Published: 01 September 1983
..., it can be used in bar form on automatic screw machines on parts where thread rolling or cold form tapping operations are critical. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1967) 16 (9): SA-216.
Published: 01 September 1967
... ELASTUF PB is a hot rolled, heat treated, free-machining, leaded alloy steel recommended for gears, shafts, bolts and fasteners. It is furnished as preheat treated, machine straightened and stress relieved bars. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1998) 47 (9): Al-353.
Published: 01 September 1998
... Alcoa C238 is a cold-finished aluminum wrought product developed for applications requiring postbrazing and welding strength. The alloy has good machinability and roll-threading characteristics. It has slightly lower corrosion resistance as compared to 6xxx series alloys. Alloy C238 has excellent...
Journal Articles
Alloy Digest (1996) 45 (9): Be-8.
Published: 01 September 1996
... AlBeMet AM 162 is a beryllium, 38% aluminum alloy produced in extruded bar, rolled sheet, and hot isostatic pressed (HIP) billets that combines the high-modulus and low-density characteristics of beryllium with the fabrication and mechanical behavior of aluminum. The alloy is weldable, can...
Journal Articles
Alloy Digest (2014) 63 (3): Ti-152.
Published: 01 March 2014
... + 593 ºC (1100 ºF)/24 h/ AC, GPa (106 psi) 24 ºC (75 ºF) 135 (20) 380 ºC (716 ºF) 113 (16) Ultimate tensile strength, forgings and rolled bar, MPa (ksi) 896 (130) 0.2% yield strength, forgings and rolled bar, MPa (ksi) 827 (120) Elongation, forgings and rolled bar, % 10 Reduction in area, % Forgings 20...
Journal Articles
Alloy Digest (2014) 63 (2): Ti-151.
Published: 01 February 2014
... (0.123) Thermal conductivity, , 24 °C (75 °F), W/m·K (Btu/(h·ft·°F)) 6.1 (3.5) Coefficient of thermal expansion, RT 454 °C (850 °F), 10 6/K (10 6/°F) 9.7 (5.4) Mechanical Properties: Tensile modulus at RT, GPa (106 psi) Annealed 111 (16.1) Solution treated and aged 116 (16.8) Forgings and rolled bar...
Journal Articles
Alloy Digest (1961) 10 (10): Mo-3.
Published: 01 October 1961
... 2 - MECHANICAL PROPERTIES AT ROOM TEMPERATURE Table 3 - HOT HARDNESS DATA Tensile Yield Reduction (As-cast samples) Condition Strength psi Strength psi (0.2%) Elongation % io 2 2-in. -dia. rolled bar as rolled 101000 88200 28 suess relieved (2100OF) 104400 86400 18 recrystallized 76900 64700 11 l...
Journal Articles
Alloy Digest (1964) 13 (8): Mo-5.
Published: 01 August 1964
... 55000 45000 2800 25000 15000 3000 15000 8000 PROPERTIES Condition Stress-relieved Recrysrallised Tesr Stress, psi to Produce Temperature, OF Rupture in 100 hrs. 1800 70000 2000 52000 1800 39000 2000 30000 Toble 5 - EFFECT OF TEMPERATURE ON PROPERTIES - Rolled Bar Te.X Tensile Temperarure OF R.T. 200 G4...
Journal Articles
Alloy Digest (1955) 4 (1): SS-23.
Published: 01 January 1955
... - 1600 deg. F. Table 1 - ROOM TEMPERATURE MECHANICAL PROPERTIES (TYPICAL) Size Tensile strength, psi Yield strength, psi ( 0.2$% ) Elongation, percent in 2 Reduction of area l 3/4 bars finished at 1300°F. 32 Rolled 4 Forged Bars* Bars*+ 135,000 125,000 100,000 851000 20 25 45 50 *Forged bars warm...
Journal Articles
Alloy Digest (1965) 14 (2): Co-42.
Published: 01 February 1965
... creacmenc should be done in a protective atmosphere such as hydrogen. Heavy sections, such as hoc-rolled bar, place or castings, should be quenched in oil co obtain a rapid cool co room temperature. Machinability: In the hoc rolled or cold rolled condition this alloy has a satisfactory machinability racing...
Journal Articles
Alloy Digest (1958) 7 (1): SA-65.
Published: 01 January 1958
... ( Water quenched and tempered) Tensile Yield Reduction Strength Strength Elongation of Area psi psi (0.2%) 70 in 2 % 150000 140000 14 55 140000 134000 16 3 20 7 2; 115000 100000 18 65 Table 3 -TYPICAL PROPERTIES-HOT ROLLED BARS Condition Tensile StXllgth DSi As RoIled 1000 F. stress relief 1100 F. stress...