Alloy Digest (2011) 60 (9): SA-633.
Published: 01 September 2011
... SA-633 JFE880NH is a 900 MPa (131 ksi) microalloyed steel used as an alternative material, for a variety of uses, to 900 MPa grade quenched and tempered steels. JFE 880NH (Micro-Alloyed Steel Rods) JFE 880NH Chemical Composition, wt (Typical values) JFE880NH SCM 435 Carbon 0.46 0.50 0.33 0.38 Silicon...
Journal Articles
Alloy Digest (1991) 40 (1): SS-518.
Published: 01 January 1991
... STAVAX WELD ELECTRODE is a basic coated electrode and STAVAX TIG-WELD is a TIG bare filler rod. Both are specially composed to be compatible with the Uddeholm stainless mold steel, STAVAX ESR (Alloy Digest SS-507, June 1989). This datasheet provides information on composition and hardness. It also...
Journal Articles
Alloy Digest (1991) 40 (12): TS-508.
Published: 01 December 1991
... QRO 90 Weld coated electrode and QRO 90 TIG-Weld filler rod are especially composed to be compatible with these Uddeholm hot work steels: ORVAR (all grades), QRO 80 Microdized and QRO 90 Supreme. This datasheet provides information on composition and hardness. It also includes information on...
Journal Articles
Alloy Digest (1991) 40 (9): TS-505.
Published: 01 September 1991
... IMPAX WELD COATED ELECTRODE and IMPAX TIG-WELD TIG FILLER ROD give a deposited weld metal almost identical in composition to IMPAX SUPREME parent metal. Both the electrode and the filler rod are also suitable for welding standard AISI P20 tool steel grades and Uddeholm Holder grades. Composed to...
Journal Articles
Alloy Digest (1993) 42 (12): Fe-103.
Published: 01 December 1993
... CARPENTER LOW EXPANSION 42 DUMET CORE ROD possesses a nearly constant expansion rate to 650 F. Use is as a core rod in copper coated wire. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (2010) 59 (1): Cu-778.
Published: 01 January 2010
... alloy safe for humans and the environment, particularly potable water. ECO BRASSĀ® (Lead-Free Silicon Brass Rod and Ingot) ECO BRASSĀ® Chemical Composition, wt See Table 1. Table 1 Chemical composition, wt.% Sand casting Nominal Permanent mold casting Nominal Wrought alloy Copper 74 78 76 74 78 77 73.0...
Journal Articles
Alloy Digest (1977) 26 (4): TS-316.
Published: 01 April 1977
... GREEN LABEL DRILL ROD is a high-quality, tough, fine-grain, straight-carbon, water-hardening tool steel with a medium hardness penetration. It is supplied with a smooth, decarburization-free surface and can be used with very little machining for applications such as shafts. This datasheet provides...
Journal Articles
Alloy Digest (1998) 47 (3): Ni-538.
Published: 01 March 1998
... NI-ROD FC 55 cored wire is used for flux-cored-arc and submerged-arc welding of gray, malleable, and ductile cast irons. It is also used for surfacing of cast irons and for joining cast irons to various wrought materials such as carbon steels and low-alloy steels. The cored wire combines the...
Journal Articles
Alloy Digest (2002) 51 (4): TS-598.
Published: 01 April 2002
... CALMAX/CARMOWELD coated electrode and CALMAX/CARMOTIG-WELD tungsten inert gas (TIG) filler rod give a deposited weld metal almost identical in composition to CALMAX (Alloy Digest TS-177, March 1966) and CARMO (Alloy Digest TS-597, March 2002) tool steels. This datasheet provides information on...
Journal Articles
Alloy Digest (2003) 52 (10): Ni-615.
Published: 01 October 2003
... NI-ROD 44HT is designed for joining iron castings to similar materials and to dissimilar materials such as carbon and stainless steels and nickel-base alloys. The product is similar to NI-ROD Filler Metal 44 (see Alloy Digest Fe-114, November 1996), but is modified to significantly improve its...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-490.
Published: 01 November 1995
... NI-ROD Welding Electrode is used for shielded-metal-arc welding of gray, ductile, and malleable cast irons. It is also used for joints between cast irons and carbon steel or low-alloy steel. The electrode is particularly useful for thin sections and for joints to be machined. NI-ROD welding...
Journal Articles
Alloy Digest (1996) 45 (2): Ni-499.
Published: 01 February 1996
... NI-ROD 55 Welding Electrode is used for shielded-metal-arc welding of gray, ductile, malleable, and Ni-Resist cast irons. It is also used for welding cast irons to various wrought materials, including carbon steels, low-alloy steels, and nickel alloys. The electrode is especially useful for...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-501.
Published: 01 March 1996
... NI-ROD 99X is an out-of-position welding electrode for welding cast iron. It has a core wire of commercially pure nickel. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on joining. Filing Code: Ni-501. Producer...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-507.
Published: 01 April 1996
... NI-Rod Filler Metal 99 is a commercially pure nickel solid wire developed for weld deposition on as-welded cast irons by automatic or semiautomatic processes. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on joining. Filing Code...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-510.
Published: 01 May 1996
... NI-ROD 55X is an out-of-position welding electrode for welding cast iron and various alloyed irons to themselves or to each other. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on joining. Filing Code: Ni-510...
Journal Articles
Alloy Digest (1996) 45 (9): Fe-112.
Published: 01 September 1996
... NI-Rod 44 Welding Electrode is a product specifically designed to attain 100% joint efficiency in the common grades of ductile iron while maintaining both strength and ductility through a metallurgically unique nickel-iron-manganese system. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1996) 45 (11): Fe-114.
Published: 01 November 1996
... Ni-Rod Filler Metal 44 is a solid, nickel-iron-manganese wire designed for automatic and semiautomatic welding of ductile, malleable, and gray cast irons in all positions. NI-Rod Filler Metal 44 offers high-speed, high-quality welds and can be used with all robotics, automatic, and semiautomatic...
Journal Articles
Alloy Digest (2010) 59 (9): Al-431.
Published: 01 September 2010
... (Extruded Rod & Bar) KAISER ALLOY 6005 Chemical Composition, wt (Nominal) Silicon 0.60 0.90 Iron 0.35 max Copper 0.10 max Manganese 0.10 max Magnesium 0.40 0.60 Chromium 0.10 max Zinc 0.10 max Titanium 0.10 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density...
Journal Articles
Alloy Digest (2010) 59 (10): Al-432.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum October 2010 Al-432 Kaiser Alloy 6041 is a lead-free alternative to 6262 with good corrosion resistance. KAISER ALLOY 6041 (Extruded Rod & Bar) KAISER ALLOY 6041 Chemical Composition, wt (Nominal) Silicon 0.50...
Journal Articles
Alloy Digest (2010) 59 (11): Al-433.
Published: 01 November 2010
...-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum November 2010 Al-433 Kaiser Alloy 6082 is a high strength alloy used in structures requiring good corrosion resistance. KAISER ALLOY 6082 (High Strength Extruded Rod & Bar) KAISER...