Journal Articles
Alloy Digest (1980) 29 (9): Ti-79.
Published: 01 September 1980
... are rocket engine cases and ordnance components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (1974) 23 (5): SA-304.
Published: 01 May 1974
... UNIMAR 250 is a maraging alloy steel having high strength, good notch toughness, excellent cryogenic properties and deep hardenability. It is recommended for pressure vessels, solid-fuel rocket cases and pressure bottles, landing-gear components, processing equipment operating in the temperature...
Journal Articles
Alloy Digest (1991) 40 (8): Ti-98.
Published: 01 August 1991
... and jet engine components, rocket engine cases, ord- nance components. Producer: Teledyne Allvac Monroe, North Carolina 281 lo-0531 ...
Journal Articles
Alloy Digest (2023) 72 (2): Ti-189.
Published: 01 February 2023
... but with lower ductility and toughness; limited weldability. Product Forms Bars; forgings. Applications Airframe and jet engine parts; ordnance components; rocket engine cases. Supplier ATI 2021 McKinney Avenue Suite 1100 Dallas, Texas 75201, USA Tel: +1 800 289 7454 Web: www.atimaterials.com All data from ATI 6...
Journal Articles
Alloy Digest (1992) 41 (3): Ti-99.
Published: 01 March 1992
... environments is excellent. Forms Available Forging stock, bars, billee. forgings. Applications: Compressor blades, discs and rings for jet engines, air frame and spacecapsulecomponents. pressure vuscls, rocket engine cases, helicopter rotor blades, fasteners, critical forgings where high strength to weight...
Journal Articles
Alloy Digest (2020) 69 (10): Ti-171.
Published: 01 October 2020
... capsule components; compressor blades, discs, and rings for jet engines; critical forgings re- quiring a high strength-to-weight ratio; fasteners; helicopter rotor hubs; pressure vessels; rocket engine cases Supplier ATI 1000 Six PPG Place Pittsburgh, Pennsylvania 15222, USA Tel: +1 800 289 7454 Web...
Journal Articles
Alloy Digest (2011) 60 (9): Ti-148.
Published: 01 September 2011
... characteristics. Products Available: Bars, forgings, sheet, strip, and plate Applications: Some applications include: armor, compressor blades, discs, and rings for jet engines; airframe and space capsule components; pressure vessels; rocket engine cases; helicopter rotor hubs; fasteners; critical forgings...
Journal Articles
Alloy Digest (1987) 36 (9): Ti-88.
Published: 01 September 1987
..., sheet, strip, wire and extrusions. Applications: Compressor blades, discs, rings forjct engines, aircraft components. pressure vessels and rocket engine cases. Manufacturer: RMI Company Niks, Ohio 44446. ...
Journal Articles
Alloy Digest (1968) 17 (4): SA-225.
Published: 01 April 1968
... for applications such as rocket motor cases and accessories, bolts and fasteners and aircraft structural components- particularly landing gear. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
... Republic RSM-300 alloy is an 18% nickel-cobalt-molybdenum age-hardening steel designed to develop up to 300,000 psi yield strength with good toughness. It is recommended for landing gears extrusion dies, rocket motor cases, high-strength bolts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1963) 12 (5): SA-146.
Published: 01 May 1963
... with excellent ductiliry and norchediunnocched ratios. Superior hot and cold workability, ease of heat rrear- ment weldability and adequate properties at cryogenic temperatures, make this material suitable for wide ap- plications in aircraft and rocket engines, airframe and missile systems. Srrength...
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... strength levels of the controlled-expansion high-temperature alloys, later-generation alloys should be con- sidered for applications involving elevated-temperature trans- verse stress conditions. Pyromet CIX-1 has been evaluated in applications such as casings. seals, and other gas turbine engine...
Journal Articles
Alloy Digest (1963) 12 (10): SA-156.
Published: 01 October 1963
... ALMAR 18 is a high-nickel martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as solid fuel rocket cases and aircraft landing gears...
Journal Articles
Alloy Digest (1970) 19 (4): TS-229.
Published: 01 April 1970
..., aircraft nose wheels, transmission cases, rocket components, and jet engine parts. Manufacturer: Magnesium Elektron Ltd. Manchester, England Magnesium Elektron, Inc. New York, New York ...
Journal Articles
Alloy Digest (1987) 36 (7): Fe-78.
Published: 01 July 1987
... and can be plated with chromium. CTX-3 uses comprise compressor and exhaust casings, seals and other components for gas turbine engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion...
Journal Articles
Alloy Digest (2014) 63 (6): Fe-163.
Published: 01 June 2014
..., billet, and ingot. For further information contact the producer. Applications: Jet engine and gas turbine components, rocket motor cases, landing gear, high-strength shafting, and other critical components requiring high-strength, high toughness, and minimal heat treatment distortion. Producer: Latrobe...
Journal Articles
Alloy Digest (1960) 9 (10): Ti-27.
Published: 01 October 1960
... 8 wide can be supplied in either the annealed; cold-rolled; or cold-rolled and aged condition. Applications: Rocket motor cases, solid rocket pressure chambers, airframe components, welded pressure vessels, fasren- ers, bonded and brazed honeycomb cover sheets. Manufacturer: Titanium Metals...
Journal Articles
Alloy Digest (1990) 39 (1): Fe-89.
Published: 01 January 1990
...: Pyromet alloy CTX-909 has been used in compressor and exhaust casings, seals, and other gas turbine engine com- ponents. Could be considered for ordnance hardware, gauge blocks, rocket engine thrust chambers, steam tur- bine blades, springs and die-casting dies. Applications re- quiring thermal fatigue...
Journal Articles
Alloy Digest (1967) 16 (6): Mg-63.
Published: 01 June 1967
.... Forms Available: Sand castings, Applications: Transmission cases, missile components, aircraft nose wheels, rockets, racing auromobile pistons, components of hydraulic units. Manufacturer: J. Stone 8~ Co. (Charlron) Ltd. London, England Magnesium Elektron Lrd. Manchester, England ...
Journal Articles
Alloy Digest (1995) 44 (1): Ni-476.
Published: 01 January 1995
... metal yield at room and elevated temperatures. Also the joint strength and ductility will be sufficient to withstand me- chanical and fatigue stresses. On hardenable base metals, joint strength is widely vi- able depending on base metal composition, joint design and brazing operation. In many cases...