1-20 of 57 Search Results for

resistors

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1966) 15 (10): Cu-170.
Published: 01 October 1966
...-170 Copper Alloy OCTOBER 1966 -DATA ON WORLD WIDE METALS AND ALLOYS COPEL (Copper-Nickel Resistor Alloy) Pvblisbed by Engineering Alloys Digest, Inc. Upper Montclair. New Jersq COPEL is a copper-nickel alloy having excellent mechanical and electrical properties. !t is recommended for use in elecuical...
Journal Articles
Alloy Digest (1989) 38 (6): Ni-372.
Published: 01 June 1989
... EVANOHM alloy R is an electrical resistance alloy with exceptional stability. Its resistivity increases during heat treatment and once obtained does not change significantly even when used at temperatures as high as 392 F (200 C). Resistors made with EVANOHM alloy R show a maximum drift of 5ppm...
Journal Articles
Alloy Digest (1968) 17 (3): Cu-186.
Published: 01 March 1968
... EXCELSIOR is a copper-nickel resistance alloy recommended for low temperature resistors and heavy duty rheostats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1969) 18 (10): Fe-39.
Published: 01 October 1969
... Niromet 46 is a 46% nickel-iron alloy having low and controlled coefficient of expansion. It is recommended for metal-to-glass seals and terminal bands in vitreous enameled resistors. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1962) 11 (9): Cu-120.
Published: 01 September 1962
... LOHM is a copper-nickel alloy recommended for resistors where low specific resistance is desired. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Cu-120. Producer or source: Driver-Harris Company. Producer or Source: Driver-Harris...
Journal Articles
Alloy Digest (1963) 12 (3): Cu-126.
Published: 01 March 1963
... MANGANIN is an alloy of copper, manganese and nickel recommended for resistors in precision built electrical apparatus and for shunts for D.C. ammeters. This datasheet provides information on composition and physical properties. Filing Code: Cu-126. Producer or source: Driver-Harris Company...
Journal Articles
Alloy Digest (1962) 11 (5): Cu-117.
Published: 01 May 1962
... Midohm is a copper-nickel, heat resistant alloy having a maximum operating temperature of 400 deg F. It is normally used for resistor and potentiometer applications where low specific resistance is required. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1967) 16 (1): Fe-30.
Published: 01 January 1967
... Tophet-D is an iron-nickel-chromium alloy recommended for electric furnace heating elements and electrical resistors operating up to 1600 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (1975) 24 (10): Cu-301.
Published: 01 October 1975
... it highly useful in sizes for instruments and resistors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-301. Producer...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1030.
Published: 01 February 2009
... Alkrothal 3 is a ferritic FeCrAl alloy that is recommended for use at temperatures up to 1000 deg C (1830 deg F). Typical applications are in rheostats and braking resistors. It is also used as electrical heating elements in industrial applications. This datasheet provides information...
Journal Articles
Alloy Digest (2010) 59 (6): Cu-784.
Published: 01 June 2010
... Cuprothal 49/49TC is a very clean alloy with high electrical resistance. Uses include precision resistors. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming. Filing Code: CU-784. Producer or source...
Journal Articles
Alloy Digest (2021) 70 (6): Ni-772.
Published: 01 June 2021
... VDM HT 80 is an austenitic, Ni-20Cr-1.25Si alloy that is typically used for the manufacture of resistors and heating conductors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-791.
Published: 01 October 2010
... properties of Konstantan have made this alloy the classic material for all types of resistors, especially for precision resistors for measurement purposes; these include series resistors for measuring devices, shunt resistors for ammeters, potentiometers, and slide, control and series resistors of all types...
Journal Articles
Alloy Digest (1996) 45 (2): SS-639.
Published: 01 February 1996
... Temperature ( C) 1200 1400 16001800 2000 22co 2400 Temperature (OF) rypical cyclic oxidation dam Ohmaloy 30 alloy is used in many applications requiring dissipa- tion of electtical energy. Some examples are grid resistors for mine locomotives, crane statters. and the Largest application, braking resistors...
Journal Articles
Alloy Digest (1996) 45 (4): SS-641.
Published: 01 April 1996
...). This Ohmaloy resistant alloy is classified as UNS K91470. Ohmaloy 40 alloy is used in many applications requiring dissipa- tion of electrical energy. Some examples are grid resistors for mine locomotives, crane starters. and the largest application. braking resistors for railroad diesel locomotives. This alloy...
Journal Articles
Alloy Digest (1970) 19 (6): Cu-216.
Published: 01 June 1970
...-magnetic and corrosion resistant. Its maximum operating temperature as a resistor is about SOOoC (932oF). Its high electrical resistance, great ductility and non-corroding properties make it particularly useful for winding heavy-duty industrial rheostats. Both wire and ribbon (strip) are used...
Journal Articles
Alloy Digest (1991) 40 (12): Cer-8.
Published: 01 December 1991
... a consistently smooth flat working surface which aids in achieving fine line widths and spacing. It meets electrical, thermal and me- chanical performance parameters required by thick film circuit processors. It provides consistent resistor perfor- mance over a range of resistor lengths and it demonstrates high...
Journal Articles
Alloy Digest (2009) 58 (4): Cu-768.
Published: 01 April 2009
... mm and a maximum width of 20 mm The ratio of thickness to width must be smaller than 10/1. Applications: The alloy is suitable for the production of precision, normal, and shunt resistors. This alloy is merchandised under the family brand RESISTAN, which includes all Wieland products for resistors...
Journal Articles
Alloy Digest (1989) 38 (7): Ni-373.
Published: 01 July 1989
... in precision resistors. Forms Available: Bare wire: insulated wire (polyester imide HR enamel, polyurethane enamel, ML polyimide enamel, cotton, silk aramid, glass insulations). Applications: In fine wire sizes, used for precision wound resistors over the temperature range -67 to +438 F (-55 to +220┬░C...
Journal Articles
Alloy Digest (1992) 41 (9): SS-534.
Published: 01 September 1992
... and toasters, blowers and catalytic con- vertors. Aluchrom W is the economical choice and is also used as heavy-duty resistors, brake resistors, elecui- cal heating elements for domestic and industrial uses, and waste-gas detoxication units. Forms Available: Strip, wire, ribbon and heating elements...