Skip Nav Destination
Close Modal
Search Results for
resistance wires
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 2000 Search Results for
resistance wires
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1988) 37 (2): Ni-355.
Published: 01 February 1988
... Copyright 1988. Alloy hgal. Inc. All qhts reserved. Publishrd by. Alloy Digs. Inc. ISSN:OO2414X 27 canfield srrca Dora shown are rypical. nor IO be used Orange. New Jersey 07050 for sprcrficcuion or final dmgn. (201) 677-9161 BRIGHTRAY ALLOY C (Electrical Resistance wire) BRIGHTRAY alloy C is an 80/20...
Abstract
View article
PDF
BRIGHTRAY alloy C is an 80 20 nickel chromium alloy containing long-life additions which make it suitable for applications subject to frequent switching and wide temperature fluctuations. It may be used at operating temperatures up to 1150 C (2100 F). It has a relatively low temperature coefficient of resistance coupled with high resistivity. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-355. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1988) 37 (8): Fe-85.
Published: 01 August 1988
... (36300) 195 (28300) 160 (23200) lSO(21800) lOO(l4500) u)( -1 Table 2 -- RESISTANCE DATA FOR DESIGN* B&S Resistance at Wire Diametez 2o c, ohms Length/weight Gage mm( in.) per meter (per ft) macdkg (ftAb) 4 5.19 (0.204 ) 0.0482 (0.0147) 5.9 ( 8.87) 6 4.11 (0.162 ) 0.0769 (0.0234) 9.51( 14.2) 8 3.26 (0.128...
Abstract
View article
PDF
BRIGHTRAY Alloy 35 is an iron-nickel-chromium alloy containing long-life rare-earth additions. It is suitable for applications subject to frequent switching and wide temperature fluctuations to a maximum operating temperature of 1050 C(1920 F). It has a relatively large temperature coefficient of resistance which must be taken into account in design calculations. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Fe-85. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1988) 37 (9): Ni-362.
Published: 01 September 1988
... BRIGHTRAY Alloy B is an electrical resistance wire which contains rare-earth long-life additions. It is useful up to 1100 C (2010 F). It has a greater temperature coefficient of resistance than the essentially binary 80/20 nickel chromium resistance grade. It is suitable for less exacting...
Abstract
View article
PDF
BRIGHTRAY Alloy B is an electrical resistance wire which contains rare-earth long-life additions. It is useful up to 1100 C (2010 F). It has a greater temperature coefficient of resistance than the essentially binary 80/20 nickel chromium resistance grade. It is suitable for less exacting applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low and high temperature performance. Filing Code: Ni-362. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1989) 38 (7): Ni-373.
Published: 01 July 1989
... EVANOHM alloy S offers optimum stability and flexibility with regard to both size and required temperature coefficient of resistance. Its extremely low electromotive force vs copper together with its high electrical resistivity are highly desirable properties in a precision resistance wire...
Abstract
View article
PDF
EVANOHM alloy S offers optimum stability and flexibility with regard to both size and required temperature coefficient of resistance. Its extremely low electromotive force vs copper together with its high electrical resistivity are highly desirable properties in a precision resistance wire. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-373. Producer or source: Wilbur B. Driver Company.
Journal Articles
Alloy Digest (2010) 59 (6): Cu-784.
Published: 01 June 2010
...-338-8542 www.asminternational.org Filing Code: Copper June 2010 Cu-784 Cuprothal 49/49TC is a very clean alloy with high electrical resistance. Uses include precision resistors. CUPROTHAL 49 & 49TC (Resistance Wire) CUPROTHAL 49 & 49TC Chemical Composition, wt (Nominal) Nickel 44 Manganese 1 Iron 0.5...
Abstract
View article
PDF
Cuprothal 49/49TC is a very clean alloy with high electrical resistance. Uses include precision resistors. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming. Filing Code: CU-784. Producer or source: Kanthal Corporation.
Journal Articles
Alloy Digest (1968) 17 (2): Cu-185.
Published: 01 February 1968
... COPPER Alloy No. 770 is a spring quality copper-nickel zinc alloy having high resistance to corrosion. It is recommended primarily for optical goods, springs, resistance wire, hardware and similar products. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
COPPER Alloy No. 770 is a spring quality copper-nickel zinc alloy having high resistance to corrosion. It is recommended primarily for optical goods, springs, resistance wire, hardware and similar products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-185. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... Nikrothal 30 is one of a family of austenitic alloys used in resistance wires for electric heating. It has good ductility after use, good corrosion resistance except in sulfur-containing atmospheres and certain controlled atmospheres, and excellent weldability. This datasheet provides information...
Abstract
View article
PDF
Nikrothal 30 is one of a family of austenitic alloys used in resistance wires for electric heating. It has good ductility after use, good corrosion resistance except in sulfur-containing atmospheres and certain controlled atmospheres, and excellent weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: SS-1039. Producer or source: Kanthal AB.
Journal Articles
Alloy Digest (2013) 62 (2): SS-1136.
Published: 01 February 2013
... Alkrothal 720 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well...
Abstract
View article
PDF
Alkrothal 720 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming. Filing Code: SS-1136. Producer or source: Kanthal AB.
Journal Articles
Alloy Digest (1985) 34 (12): Cu-504.
Published: 01 December 1985
... comprise electrical parts that meet RWMA (Resistance Wire Manufacturer's Association) Class II standards. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining...
Abstract
View article
PDF
Copper Alloy No. C81400 is a precipitation-hardenable alloy of moderate hardness and strength. Its common name is beryllium-modified chromium copper and a previous trade name was Beryllium Copper 70C. Because of its beryllium content, its manufacture may present a health hazard. Typical uses comprise electrical parts that meet RWMA (Resistance Wire Manufacturer's Association) Class II standards. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: Cu-504. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (2009) 58 (3): SS-1032.
Published: 01 March 2009
... Alkrothal 14 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low temperature performance as well as forming...
Abstract
View article
PDF
Alkrothal 14 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low temperature performance as well as forming. Filing Code: SS-1032. Producer or source: Kanthal AB.
Journal Articles
Alloy Digest (1981) 30 (4): Cu-416.
Published: 01 April 1981
..., such as drawing, forming and bending, heading and upsetting, piercing and punching. Joining: Joining by soldering or brazing is entirely satisfactory. Resistance flash butt welding of redraw rod and wire is commonly practiced. Applications of Hitenso 162 rarely require gas or arc welding, and only fair joints...
Abstract
View article
PDF
HITENSO 162 is a copper-cadmium alloy that offers a unique combination of high tensile strength and high electrical conductivity in wire where ordinarily these properties are incompatible. It also is noted for its malleability and toughness. Among its many uses are heating pads, electric blankets, current-carrying rings and electrical contacts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-416. Producer or source: Anaconda Industries.
Journal Articles
Alloy Digest (1966) 15 (10): Cu-170.
Published: 01 October 1966
... current at 600°F. At 800°F.. bright wire will oxidize slightly and its current-lemperoture relationship will be the same OS for oxidized wire. DOI: 10.31399/asm.ad.cu0170 Copyright © ASM International® 1996 Table 3 - RESISTANCE - OHMS PER FOOT _- T - 34 ziii .m540 z lwub %i mn8 mm XF mm m937 IQ170 .02450...
Abstract
View article
PDF
COPEL is a copper-nickel alloy having excellent mechanical and electrical properties. It is recommended for use in electrical instruments and similar apparatus where mechanical stability and a known low coefficient of resistance are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-170. Producer or source: Hoskins Manufacturing Company.
Journal Articles
Alloy Digest (1959) 8 (6): Cu-76.
Published: 01 June 1959
...- phrams, optical goods, dairy and sterilizer equipment, ornamental grills, screw machine products, hospital equipment, resistance wire. Manufacturer: Riverside Alloy Metal Division H. K. Porter Company, Inc. Riverside, New Jersey ...
Abstract
View article
PDF
RIVERSIDE No. 4 is a spring quality nickel silver alloy having high resistance to corrosion and tarnish. It is used primarily for springs and electrical resistances. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-76. Producer or source: H. K. Porter Company Inc..
Journal Articles
Alloy Digest (2009) 58 (9): SS-1044.
Published: 01 September 2009
... of austenitic alloys used in resistance wires for electric heating. Nikrothal is a registered trademark of Kanthal AB. Chemical Composition, wt (Nominal) Carbon 0.08 max Silicon 2.3 2.5 Manganese 0.5 max Chromium 23.0 25.0 Nickel 19.0 21.0 Iron bal Trace elements added Physical Properties: Density, kg/m3 (lb...
Abstract
View article
PDF
Nikrothal 20 is an austenitic nickel-chromium alloy (NiCr alloy) for use at temperatures up to 1050 C (1920 F). The alloy is characterized by high resistivity and moderate oxidation resistance. It has good ductility after use and excellent weldability. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming. Filing Code: SS-1044. Producer or source: Kanthal AB.
Journal Articles
Alloy Digest (1958) 7 (3): Cu-61.
Published: 01 March 1958
..., optical goods, dairy and sterilizer equipment, orna- mental grills, screw machine products. hospital equip- inent, resistance wire. Weldability: Manufacturer: Readily welded by the gas, carbon-arc and metallic arc methods; also spot and seam welding for thin gauge. its weldatdiy is good by gas or metallic...
Abstract
View article
PDF
NICKEL SILVER, 55-18 is a spring quality nickel silver alloy having high resistance to corrosion and tarnish. It is used primarily for springs and electrical resistances. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-61. Producer or source: Copper alloy mills.
Journal Articles
Alloy Digest (2001) 50 (12): Ni-576.
Published: 01 December 2001
... properties and machinability for low-alloy steels, and increased consistency in resistance wire alloys. Product Forms Available: The alloy is available as silver-gray pieces approximately 1.4 kg (3 lb) each. It is packaged in 345.25 kg (761 lb) steel drums, 4 drums per pallet, strapped, with a net weight...
Abstract
View article
PDF
Incocal Alloy 10 is a direct melt additive alloy of nickel with calcium to scavenge deleterious elements and improve ambient and high-temperature properties of both iron- and nickel-base alloys. This datasheet provides information on composition and physical properties. Filing Code: Ni-576. Producer or source: International Nickel Inc.
Journal Articles
Alloy Digest (2017) 66 (11): Ni-739.
Published: 01 November 2017
... Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Abstract
View article
PDF
Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni-739. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (2016) 65 (8): Al-445.
Published: 01 August 2016
.... It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-445. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2016 2016 ASM International ALCOTEC WELD FILLER WIRE 5356...
Abstract
View article
PDF
Alcotec weld filler wire 5356 is a non-heat-treatable aluminum welding wire whose principal alloying elements are magnesium, manganese, and chromium. It is similar to the European wire AlMg5Cr(A). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-445. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Alloy Digest (2016) 65 (9): Al-446.
Published: 01 September 2016
... properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-446. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2016 2016 ASM International Alcotec weld filler wire...
Abstract
View article
PDF
Alcotec weld filler wire 5554 is a non-heat-treatable aluminum welding wire whose principal alloying elements are magnesium, manganese, chromium, and titanium. It is similar to the European wire AlMg2.7Mn. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-446. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Alloy Digest (2002) 51 (6): Al-378.
Published: 01 June 2002
.... It also includes information on corrosion resistance as well as joining. Filing Code: AL-378. Producer or source: AlcoTec Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International AlcoTec Weld Filler Wire 5556 aluminum brazing...
Abstract
View article
PDF
AlcoTec Weld Filler Wire 5556 is a non-heat-treatable wire with very high strength capabilities. The principal alloying elements are magnesium, manganese, chromium, and titanium. This datasheet provides information on composition, physical properties, tensile properties, and shear strength. It also includes information on corrosion resistance as well as joining. Filing Code: AL-378. Producer or source: AlcoTec Wire Corporation.