Alloy Digest (1969) 18 (4): Cu-198.
Published: 01 April 1969
... Elkaloy-A is a copper-base alloy having high strength and toughness coupled with high electrical and thermal conductivity. It is recommended for springs, electrical contacts and resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1992) 41 (7): Ni-407.
Published: 01 July 1992
... INCONEL WELDING ELECTRODE 122 is a highly alloyed product used for joining Inconel alloy 622 (See Alloy Digest Ni-382, May 1990) and similar corrosion resistant grades. In dissimilar welding, it can be used to prevent preferential weld metal attack. This datasheet provides information...
Journal Articles
Alloy Digest (1982) 31 (6): Cu-438.
Published: 01 June 1982
... ANACONDA Alloy 182 is a copper-base alloy containing nominally 0.85% chromium. It offers relatively high electrical conductivity, good strength and hardness and some resistance to softening at elevated temperatures. Among its uses are resistance welding electrodes, switchgear, and electrical...
Journal Articles
Alloy Digest (1988) 37 (2): Cu-535.
Published: 01 February 1988
... UNS No. C16200 is a copper-cadmium alloy with high electrical and thermal conductivities combined with high strength and toughness. It is recommended for resistance-welding electrodes, back-up bars and current carrying rings. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1968) 17 (5): Cu-187.
Published: 01 May 1968
... BRUSH Alloy 10 is a low beryllium, cobalt-bearing copper alloy offering an excellent combination of strength, toughness and conductivity due to an age-hardening heat treatment. It is recommended for springs, clutch rings, resistance welding electrodes and tips, etc. This datasheet provides...
Journal Articles
Alloy Digest (1972) 21 (8): Cu-257.
Published: 01 August 1972
... MUELLER ALLOY 1820 (formerly MBCo 902) is a chromium-copper alloy with high electrical conductivity, high mechanical strength, and superior creep, fatigue and wear properties. It is used for resistance welding electrodes, switchgear, and electrical and electronic parts. This datasheet provides...
Journal Articles
Alloy Digest (1974) 23 (12): Cu-289.
Published: 01 December 1974
... COPPER ALLOY No. 162 is a copper-cadmium alloy with high electrical and thermal conductivities combined with high strength and toughness. It is recommended for resistance-welding electrodes, back-up bars and current-carrying rings. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1976) 25 (7): Cu-315.
Published: 01 July 1976
... AMPCOLOY is a copper-cadmium alloy with high electrical and thermal conductivities in combination with high strength and toughness. Among its many applications are current-carrying rings, resistance-welding electrodes and back-up bars. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1964) 13 (3): Cu-139.
Published: 01 March 1964
... Mallory 150 is a heat treatable, high strength, high conductivity copper-base alloy. It is recommended for resistance welding electrodes, dies, circuit breakers, leaf springs, and current carrying structural parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1983) 32 (11): Cu-466.
Published: 01 November 1983
... and as a result, has greater ductility and uniformity. Typical applications of AMCROM include resistance welding electrode tips and wheels, electrical contacts and connectors and high-temperature wire. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1967) 16 (6): Cu-177.
Published: 01 June 1967
... Mallory 22 is a high strength, high conductivity copper-base alloy supplied in the form of forgings. It is heat treatable and is recommended for resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1985) 34 (6): Ni-316.
Published: 01 June 1985
... alloys. The weld metal deposited from Nickel Welding Electrode 141 has good resistance to corrosion, especially in alkalies. The electrode can be operated in all positions. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1982) 31 (1): SA-384.
Published: 01 January 1982
...-resistant alloys elasticity heat treatability joinability machinability physical properties VERTI-COR WELDING ELECTRODE welding electrodes 11 Or VERTI-COR Welding Electrode EEZ~ sA-384 JANUARY 1982 bICIST - DATA ON WORLD WIDE METAL!! AND ALLOYS @ Copyright 1980. Engineering Publications, Inc. All...
Journal Articles
Alloy Digest (1996) 45 (2): Ni-499.
Published: 01 February 1996
... NI-ROD 55 Welding Electrode is used for shielded-metal-arc welding of gray, ductile, malleable, and Ni-Resist cast irons. It is also used for welding cast irons to various wrought materials, including carbon steels, low-alloy steels, and nickel alloys. The electrode is especially useful...
Journal Articles
Alloy Digest (1985) 34 (11): Ni-325.
Published: 01 November 1985
...; nickel joined to stainless steels, and stainless steels joined to carbon steels. Electrode 182 can be operated in all welding positions. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1985) 34 (10): Ni-323.
Published: 01 October 1985
... chemical composition corrosion-resistant alloys heat treatability INCONEL WELDING ELECTRODE 132 joinability machinability oxidation resistance tensile properties welding electrodes workability I 1 a- INCONEL Welding Electrode 132 kBelcAqfIff Ni-323 OCTOBER 1985 --I- -I- -1--I -1.11 l-u...
Journal Articles
Alloy Digest (1981) 30 (7): SA-381.
Published: 01 July 1981
... is attacked readily by acids. but is somewhat resistant to alkalies at ordinary temperatures. Specification Equivalent: Airco Metal-Cor 6 electrode may be ordered to AWS AS.20 E70T-G. General Characteristics: The composition and mechanical properties of the weld metal produced by Airco MeralCor 6...
Journal Articles
Alloy Digest (1977) 26 (12): SA-339.
Published: 01 December 1977
... Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity fracture toughness heat treatability joinability machinability physical properties shipbuilding tensile properties UNIFLUX V100 welding electrodes All Filing Code: SA...
Journal Articles
Alloy Digest (1978) 27 (1): SA-340.
Published: 01 January 1978
... penetration with uniform mechanical and chemical properties. The recommended operating parameters for Uniflux VCM 125 are given in Table 2. Weld metal deposited from the Uniflux VCM 125 electrode typically has good mechanical properties as shown in Table 1. Corrosion Resistance: The corrosion resistance...
Journal Articles
Alloy Digest (1984) 33 (3): SA-399.
Published: 01 March 1984
... International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability machinability physical properties tensile properties TUF-COR 1 WELDING ELECTRODE welding electrodes MARCH 1984 PIGILT - DATA ON WORLD WIDE METAlS AND AUOYS @ Copyright 1980...