Alloy Digest (1971) 20 (7): Ni-165.
Published: 01 July 1971
... HYTEMCO is a nickel-iron alloy with a high temperature coefficient of electrical resistance. It is recommended for electrical instruments and controls, such as ballistic devices and resistance thermometers, operating in air up to 1100 F. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1962) 11 (4): Ni-71.
Published: 01 April 1962
... BALCO is a nickel-iron alloy recommended for applications operating in air at 1100 deg. F. It is used in electrical instruments and controls such as resistance thermometers and ballistic devices. This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... electrical device across a fluctuating voltage source. Kanthal 70 has a maximum recommended operating temperature of 600 C and is used widely in resistance thermometers and in various appliance and automotive applications. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1984) 33 (4): SS-443.
Published: 01 April 1984
... stainless and heat-resisting steels. In the annealed condition it is austenitic. non-magnetic. extremely tough and ductile and it has excellent resistance to corrosion. .Among its many uses are springs. woven screens. cables. salt-water fishing tackle. thermometers and camera parts. *CARPENTER...
Journal Articles
Alloy Digest (1962) 11 (11): Ni-76.
Published: 01 November 1962
... Durco D-10 is a nonferrous, non-magnetic alloy containing nickel and chromium totaling about 80%. It is recommended for corrosion resisting castings where a higher corrosion resistance is required than that of stainless steel. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (3): Ni-143.
Published: 01 March 1969
... conductivity at cryogenic temperatures. Forms Available: Rod, bar, sheet and strip, wire rod, tube, tlats, rounds and plater cores. Applications: Plater bars, passive cathodes, fluorescent lamp components, resistance thermometers, hydrogen thyratron components, cathode shanks, plates (anodes), and electrolytic...
Journal Articles
Alloy Digest (1952) 1 (3): Ni-1.
Published: 01 November 1952
... ILLIUM is a nickel-base alloy containing high percentages of chromium, molybdenum, copper and iron. It has unusual corrosion resistance, high strength, machinability, and ability to resist erosion. It is an excellent alloy where extreme heat and corrosion are encountered. Illium is marketed in two...
Journal Articles
Alloy Digest (1977) 26 (7): Ni-247.
Published: 01 July 1977
.... This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-247. Producer or source: Techalloy Company Inc...
Journal Articles
Alloy Digest (1978) 27 (10): Bi-8.
Published: 01 October 1978
..., Btu/lb/oF (Liquid) (Solid) Latent heat of fusion, Btu/lb Thermal coef. expansion/oF 0.32 8.9 117 0.035 * 0.035 * 6* 14*x 10-6 Electrical conductivity, % IACS Electrical resistivity Ohms/mm2/meter Volume change (Liquid to solid), % Volume change (Linear growth after solidification), % *Approximate...
Journal Articles
Alloy Digest (1979) 28 (9): Bi-13.
Published: 01 September 1979
.../oF (Liquid) (Solid) Latent heat of fusion, Btu/lb Thermal coef. expansion/oF Electrical conductivity, % IACS 2.43 Electrical resistivity Ohms/mm2/meter 0.7081 Volume change (Liquid to solid), % -1.35 Volume change (Linear growth after solidification), % co.05 *Approximate. **Ohms based on volume standard...
Journal Articles
Alloy Digest (1978) 27 (4): Bi-4.
Published: 01 April 1978
...) 9.5 Tin 14.5 Melting range, oF 21840 Antimony 9.0 Yield temperature, oF 240 Specific heat, Btu/lb/oF (Liquid) 0.04* (Solid) 0.045* Thermal coef. expansion/oF (60-l 300F) 12; x 10-a (13@2180F) Zero* Electrical conductivity, % IACS 2.57 Electrical resistivity , ** Ohms/mm2/meter 0.6696 Volume change...
Journal Articles
Alloy Digest (1994) 43 (12): SA-481.
Published: 01 December 1994
... NAK 55 is a very clean steel for use in plastic and rubber molds were impact resistance is not critical in design. Its age-hardening gives very high strength and good wear resistance. Tight tolerance are obtained with consistent expansion and contraction properties. This datasheet provides...
Journal Articles
Alloy Digest (1979) 28 (4): Bi-11.
Published: 01 April 1979
... Electrical conductivity, % IACS Electrical resistivity, ** Ohms/mm2/meter Volume change (Liquid to solid), % Volume change (Linear growth after solidification), % *Approximate. **Ohms based on volume standard (meter, mm2). PROPERTIES Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi...
Journal Articles
Alloy Digest (1979) 28 (12): Bi-15.
Published: 01 December 1979
... Electrical resistivity, ** Ohms/mm2/meter Volume change (Liquid to solid), % Volume change (Linear growth after solidification), % *Approximate. **Ohms based on volume standard (meter, mm2). 0.05* 5.00 0.3445 +0.77 0.05 Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi Elongation (2...
Journal Articles
Alloy Digest (1981) 30 (5): Bi-24.
Published: 01 May 1981
...) 0.032* Latent heat of fusion, Btu/lb l3* Thermal coef. expansion/OF (At 680F) 12.8*x 10-6 Electrical conductivity, % IACS 2.43 Electrical resistivity Ohms/mm2/meter 0.708 Volume change (Liquid to solid), % -1.35 Volume change (Linear growth after solidification), % < 0.05 *Approximate. **Ohms based...
Journal Articles
Alloy Digest (1981) 30 (9): Bi-26.
Published: 01 September 1981
..., lb/cu in. (At 680F) Specific gravity Melting temperature, oF (oC) Specific heat, Btu/lb/oF (Liquid or solid) Latent heat of fusion, Btu/lb Thermal coef. expansion/OF 032 117 0.035+ 6* 14*x 10-6 Electrical conductivity, % IACS Electrical resistivity, ** Ohms/mm2/meter Volume change (Liquid to solid...
Journal Articles
Alloy Digest (1981) 30 (7): Bi-25.
Published: 01 July 1981
... in melting, pouring and casting OstalIoy 255 are few and simple. They com- prise the following: (1) Use a clean ladle over a gas burner or other heat source, (2) Use a thermometer to check pouring temperature which should be about 275 3OOoF, (3) Reheat parts surrounding cavity into which Ostalloy 255...
Journal Articles
Alloy Digest (1984) 33 (2): Bi-35.
Published: 01 February 1984
... resistivity, ** Ohms/mm2/meter Volume change (Liquid to solid), yc Volume change (Linear growth after solidification), Ye *Approximate. **Ohms based on volume standard (meter, mm2). PROPERTIES Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi 6300 Elongation (2 in % (Slow loading...
Journal Articles
Alloy Digest (1982) 31 (9): Bi-29.
Published: 01 September 1982
... Electrical resistivity Ohms/mm2/meter Volume change (Liquid to solid), Qo Volume change (Linear growth after solidification), Qo *Approximate. **Ohms based on volume standard (meter, mm2). PROPERTIES Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi 8ooO Elongation (2 in Qo (Slow...
Journal Articles
Alloy Digest (1983) 32 (6): Bi-31.
Published: 01 June 1983
... Electrical conductivity, % IACS Electrical resistivity, ** Ohms/mmZ/meter Volume change (Liquid to solid), % Volume change (Linear growth after solidification), J$c *Approximate. **Ohms based on volume standard (meter, mm 0.342 9.45 142- 149 147 0.040* 0.039* 7 12*x lo+ 0.045* 3.27 0.5282 - I. 7 0. 6...