Alloy Digest (1983) 32 (11): Ni-294.
Published: 01 November 1983
... MAGNIFER 75 is a soft magnetic nickel-iron alloy containing about 5% copper and 2% chromium. It offers very high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound toroids, laminations, shielding and relay parts. This datasheet...
Journal Articles
Alloy Digest (1984) 33 (2): Ni-291.
Published: 01 February 1984
... MAGNIFER 7904 is a soft magnetic nickel-iron alloy containing about 5% molybdenum. It offers extremely high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound troids, laminations, shielding and relay parts. This datasheet provides...
Journal Articles
Alloy Digest (1984) 33 (5): Fe-70.
Published: 01 May 1984
... (Coils), (3) Relay parts and (4) Integrating current transformers for Fi-protective switches. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... ferritic alloy specifically developed for solenoid valve magnetic core components and relay parts which must operate in corrosive environments. Car- penter 430FR exhibits the following three advantages over 430F Solenoid Quality (Rockwell B 75/82 or 82/91) stainless and other commercially available 430F...
Journal Articles
Alloy Digest (2015) 64 (6): Cu-838.
Published: 01 June 2015
... Wieland-K50 (C70260) is copper alloyed with low nickel for good fabricability for parts in the electrical industry, such as stamped parts, connectors, and relay springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend...
Journal Articles
Alloy Digest (1966) 15 (7): Cu-166.
Published: 01 July 1966
... Revere No. 145 is a free-cutting grade of copper recommended for high conductivity parts, such as electrical connectors, relays, fasteners, contacts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
... ULTRONZE is a copper alloy also known as Olin Alloy 654. It bridges the gap between standard high-performance copper alloys and beryllium-copper alloys, thus enabling the design of parts with properties previously only attainable with more expensive materials. The alloy has superior stress...
Journal Articles
Alloy Digest (1984) 33 (12): Cu-488.
Published: 01 December 1984
... Copper Alloy No. C43400 is a copper-zinc-tin alloy that can be cold worked readily by all conventional processes. It has moderate strength and good ductility. This alloy is used typically for electrical switch parts, contacts and relay springs. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2018) 67 (6): Cu-873.
Published: 01 June 2018
... Alloy CuSn6 (UNS C51900) is a high-performance copper alloy. Typical uses include components for the electronics industry such as connector springs, relays, leaf springs, and switches as well as machine parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (1): Fe-10.
Published: 01 January 1963
... field of applications. Its uses range from tele- phone and telegraph wires and small relay parts to huge magnetic cores for cyclotrons. Beta ray spectrographs and other equipment for nuclear research are constructed from rolled or forged sections. Armco Magnetic Ingot Iron is not recommended...
Journal Articles
Alloy Digest (2001) 50 (1): Fe-4.
Published: 01 January 2001
... grade with an 8 9 grain size and transformer grade with a 2 cm grain size. Applications: Magnetic relay parts, magnetic shielding, pole pieces, specialty motor stators and rotors, electric transformers, magnetic amplifiers Producer: Allegheny Ludlum Corporation Pittsburgh, PA 16222-6479 (800) 258-3586...
Journal Articles
Alloy Digest (2023) 72 (12): Cu-943.
Published: 01 December 2023
... and relay blades; fuse clips; navigational instruments; relay parts; switch parts. Bolts; lock washers; retaining rings; roll pins; screws; washers. Bearings; bellows; bourdon tubes; bushings; diaphragms; electrochemical springs; flexible metal hose; housings for instruments; non-sparking safety tools...
Journal Articles
Alloy Digest (2001) 50 (12): Fe-123.
Published: 01 December 2001
...-Ni-Cr alloy with about 40% Ni and about 8% Cr. It has a saturation induction of about 0.8 T, high permeability values, a very low coercive force, and good corrosion resistance. Product Forms Available: Strip Applications: Applications for Magnifer 4008 include relay parts, stepping motors...
Journal Articles
Alloy Digest (1987) 36 (1): Fe-75.
Published: 01 January 1987
... and iorgings. Rod is available our-of-stock in most common iraclional diamerers IO 2 3 -I Inch on a I-2 Meek delivery. Larger si7es also are available. Applications: Solenoid and rela! cores. plungers and pole pieces: relay parts and cores of magnetic control de\ Ices: generalor and molar field frames...
Journal Articles
Alloy Digest (1996) 45 (6): Fe-110.
Published: 01 June 1996
...-wound cores. core sheets. and relay parts. The producer can also undertake job-annealing of Par=. Applications: Producer: KRUPP VDM GmbH D-58778 WerdohVGerman) (2392) 55-O In USA: VDM Technologies Corp. Parsippany. NJ 07051 (201) 167-8515 Typical applications of Magnifer 36 are: l LF transducers l...
Journal Articles
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
... is relatively 10~. Available Forms: Semis. Strip, ribbon. sheet. bar. and wire are available. Sizes and tolerances are available from the producer Fabricated. Toroidal tape-wound cores, core sheets. and relay parts. The producer can also undertake job-annealing of parts. DOI: 10.31399/asm.ad.fe0111 Table 2...
Journal Articles
Alloy Digest (2012) 61 (4): Fe-159.
Published: 01 April 2012
... circuit inductances circuits and transformers (perfectly adapted for 400 Hz) Electrical engineering: massive relay parts and pole-piece for electro-magnets. Producer: Aperam Alloys USA Norristown, PA 19403 USA Tel: (800) 523-1777 Fax: (610) 666-1815 France: Aperam Alloys Service F-78680 Epône France Tel...
Journal Articles
Alloy Digest (1992) 41 (4): Fe-97.
Published: 01 April 1992
... (lOlO C), 4h in dry hydrogen. Cool in each case to below 700°F (376°C) @ 50 to 100°F (10 to 38°C) per hour, then in air to room tem- perature. Lime, magnesium oxide or alumina may be used to prevent parts from sticking. Forming and Machining: Allegheny Ludlum Relay No. 2 and No. 5 supplied in the mill...
Journal Articles
Alloy Digest (1977) 26 (5): Cu-333.
Published: 01 May 1977
... can be made from this alloy to advantage. Forms Available: Bar, forgings, plate, rod, shapes, sheet, strip, tube, wire and foil. Applications: Fuse clips, fasteners, springs, switch parts, relay parts, welding equipment, reeds, valves for musical instru- ments, slip rings and collector rings in high...
Journal Articles
Alloy Digest (1980) 29 (5): Cu-394.
Published: 01 May 1980
... parts, electromechanical springs, diaphragms, contact bridges, fasteners, switch parts, relay parts, roll pins, electrical and electronic components and welding equipment. Manufacturers: Specialty copper alloy mills. ...