Skip Nav Destination
Close Modal
Search Results for
red hardness
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 421
Search Results for red hardness
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
CIRCLE C (T-5): High Red Hardness Wear Resistant High-Speed Tool Steel
Available to Purchase
Alloy Digest (1990) 39 (10): TS-502.
Published: 01 October 1990
... CIRCLE C (AISI T5) tool steel combines increased wear resistance from higher vanadium and carbon contents with higher red hardness due to 8 to 9% cobalt content. This datasheet provides information on composition and hardness as well as fracture toughness, and deformation. It also includes...
Abstract
View articletitled, CIRCLE C (T-5): High <span class="search-highlight">Red</span> <span class="search-highlight">Hardness</span> Wear Resistant High-Speed Tool Steel
View
PDF
for article titled, CIRCLE C (T-5): High <span class="search-highlight">Red</span> <span class="search-highlight">Hardness</span> Wear Resistant High-Speed Tool Steel
CIRCLE C (AISI T5) tool steel combines increased wear resistance from higher vanadium and carbon contents with higher red hardness due to 8 to 9% cobalt content. This datasheet provides information on composition and hardness as well as fracture toughness, and deformation. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-502. Producer or source: Teledyne Vasco.
Journal Articles
CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
Available to Purchase
Alloy Digest (2021) 70 (9): TS-818.
Published: 01 September 2021
... Crucible CPM Rex 54 HS is a cobalt-bearing high speed tool steel that is produced by the proprietary Crucible Particle Metallurgy (CPM) process. It combines the wear properties of the popular high vanadium M4 grade with the red hardness of the cobalt-bearing M35/Crucible CPM Rex 45 HS grades...
Abstract
View articletitled, CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
View
PDF
for article titled, CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
Crucible CPM Rex 54 HS is a cobalt-bearing high speed tool steel that is produced by the proprietary Crucible Particle Metallurgy (CPM) process. It combines the wear properties of the popular high vanadium M4 grade with the red hardness of the cobalt-bearing M35/Crucible CPM Rex 45 HS grades. Crucible CPM Rex 54 HS may be used as an upgrade for improved red hardness over M3 or M4 without giving up the abrasion resistance, or as an upgrade for improved wear resistance over M35 or Crucible CPM Rex 45 HS without giving up the red hardness. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also includes information on wear resistance as well as heat treating and surface treatment. Filing Code: TS-818. Producer or source: Crucible Industries LLC.
Journal Articles
FAGERSTA WKE-45: Super High-Speed Steel
Available to Purchase
Alloy Digest (1977) 26 (4): TS-317.
Published: 01 April 1977
... FAGERSTA WKE-45 is a tungsten-molybdenum high-speed steel containing 11% cobalt. It has greater red hardness and more wear resistance than almost any other high-speed steel and has adequate (medium) toughness. It is used mainly for lathe tools (for example, tool bits) where maximum wear resistance...
Abstract
View articletitled, FAGERSTA WKE-45: Super High-Speed Steel
View
PDF
for article titled, FAGERSTA WKE-45: Super High-Speed Steel
FAGERSTA WKE-45 is a tungsten-molybdenum high-speed steel containing 11% cobalt. It has greater red hardness and more wear resistance than almost any other high-speed steel and has adequate (medium) toughness. It is used mainly for lathe tools (for example, tool bits) where maximum wear resistance and red hardness are required. It is particularly suitable for working very hard and wear-inducing materials, including stainless steels. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-317. Producer or source: Fagersta Steels Inc..
Journal Articles
AISI TYPE T5: Heavy Duty High-Speed Steel
Available to Purchase
Alloy Digest (1981) 30 (10): TS-389.
Published: 01 October 1981
... AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions...
Abstract
View articletitled, AISI TYPE T5: Heavy Duty High-Speed Steel
View
PDF
for article titled, AISI TYPE T5: Heavy Duty High-Speed Steel
AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions of speed, feed and depth of cut that would not be possible with ordinary high-speed steels. Typical applications of AISI Type T5 are lathe and planer tools, reamers, milling cutters and twist drills for heavy-duty cutting. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-389. Producer or source: Tool steel mills.
Journal Articles
RED CUT COBALT: High-Speed Tool Steel, Type T4
Available to Purchase
Alloy Digest (1980) 29 (8): TS-367.
Published: 01 August 1980
... RED CUT COBALT steel is made by adding 5% cobalt to the conventional 18% tungsten -4% chromium-1% vanadium high-speed steel. Cobalt increases hot or red hardness and thus enables the tool to maintain a higher hardness at elevated temperatures. This steel is best adapted for hogging cuts or where...
Abstract
View articletitled, <span class="search-highlight">RED</span> CUT COBALT: High-Speed Tool Steel, Type T4
View
PDF
for article titled, <span class="search-highlight">RED</span> CUT COBALT: High-Speed Tool Steel, Type T4
RED CUT COBALT steel is made by adding 5% cobalt to the conventional 18% tungsten -4% chromium-1% vanadium high-speed steel. Cobalt increases hot or red hardness and thus enables the tool to maintain a higher hardness at elevated temperatures. This steel is best adapted for hogging cuts or where the temperature of the cutting point of the tool in increased greatly. It is well adapted for tools to be used for reaming cast-iron engine cylinders, turning alloy steel or cast iron and cutting nonferrous alloys at high speeds. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-367. Producer or source: Teledyne Vasco.
Journal Articles
RED CUT SUPERIOR J: Hot Work Tool Steel, Type H26
Available to Purchase
Alloy Digest (1983) 32 (1): TS-410.
Published: 01 January 1983
... RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended...
Abstract
View articletitled, <span class="search-highlight">RED</span> CUT SUPERIOR J: Hot Work Tool Steel, Type H26
View
PDF
for article titled, <span class="search-highlight">RED</span> CUT SUPERIOR J: Hot Work Tool Steel, Type H26
RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended for applichations in which hardness must be maintained at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-410. Producer or source: Teledyne Vasco.
Journal Articles
PEERLESS A: Hot Work Steel, Type H21
Available to Purchase
Alloy Digest (1959) 8 (9): TS-85.
Published: 01 September 1959
... PEERLESS-A is a low carbon, medium tungsten hot work steel which possesses excellent red hardness. It is used in those applications where the tool operates a dull red heat. It conforms to AISI Type H21, SAE Type H21. This datasheet provides information on composition, physical properties, hardness...
Abstract
View articletitled, PEERLESS A: Hot Work Steel, Type H21
View
PDF
for article titled, PEERLESS A: Hot Work Steel, Type H21
PEERLESS-A is a low carbon, medium tungsten hot work steel which possesses excellent red hardness. It is used in those applications where the tool operates a dull red heat. It conforms to AISI Type H21, SAE Type H21. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-85. Producer or source: Crucible Steel Company of America.
Journal Articles
CRUCIBLE CPM REX 121: Vanadium-Cobalt Tool Steel
Available to Purchase
Alloy Digest (2001) 50 (10): TS-591.
Published: 01 October 2001
... CPM Rex 121 is a super high-speed steel with significantly higher wear resistance and red hardness than other high-speed steels. It is best suited for applications requiring high cutting speeds. It may provide an alternative to carbide where carbide cutting edges are too fragile. The annealed...
Abstract
View articletitled, CRUCIBLE CPM REX 121: Vanadium-Cobalt Tool Steel
View
PDF
for article titled, CRUCIBLE CPM REX 121: Vanadium-Cobalt Tool Steel
CPM Rex 121 is a super high-speed steel with significantly higher wear resistance and red hardness than other high-speed steels. It is best suited for applications requiring high cutting speeds. It may provide an alternative to carbide where carbide cutting edges are too fragile. The annealed hardness is approximately 350-400 HB, and maximum hardness is approximately 72 HRC. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance and wear resistance as well as heat treating and surface treatment. Filing Code: TS-591. Producer or source: Crucible.
Journal Articles
ELECTRITE DYNACUT: Super High-Speed Steel, Type M43
Available to Purchase
Alloy Digest (1974) 23 (11): TS-277.
Published: 01 November 1974
... ELECTRITE DYNACUT has a composition that enables it to attain higher hardnesses than previously obtainable in high-speed steel by normal heat treatment. This high hardness in combination with high cobalt content imparts an optimum balance between wear resistance and red hardness. It is recommended...
Abstract
View articletitled, ELECTRITE DYNACUT: Super High-Speed Steel, Type M43
View
PDF
for article titled, ELECTRITE DYNACUT: Super High-Speed Steel, Type M43
ELECTRITE DYNACUT has a composition that enables it to attain higher hardnesses than previously obtainable in high-speed steel by normal heat treatment. This high hardness in combination with high cobalt content imparts an optimum balance between wear resistance and red hardness. It is recommended for applications involving long production runs or heavy-duty machining. This datasheet provides information on composition and hardness. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-277. Producer or source: Latrobe Steel Company.
Journal Articles
CRUCIBLE CPM REX T15 (HS): High-Speed Steel
Available to Purchase
Alloy Digest (2007) 56 (3): TS-249.
Published: 01 March 2007
... CPM Rex T15 is a tungsten-type high-speed steel containing high carbon and vanadium for very high hardness and maximum wear resistance, and cobalt for good red hardness. It is now made exclusively by Crucible’s particle metallurgy process, resulting in improved quality and grindability. This alloy...
Abstract
View articletitled, CRUCIBLE CPM REX T15 (HS): High-Speed Steel
View
PDF
for article titled, CRUCIBLE CPM REX T15 (HS): High-Speed Steel
CPM Rex T15 is a tungsten-type high-speed steel containing high carbon and vanadium for very high hardness and maximum wear resistance, and cobalt for good red hardness. It is now made exclusively by Crucible’s particle metallurgy process, resulting in improved quality and grindability. This alloy was designed for use in difficult machining operations requiring heavy-duty cuts, high speeds and feeds, and for difficult-to-machine materials that are high in hardness and abrasion resistance. This datasheet revision updates chemistry, properties, and the benefits of high sulfur (HS). This datasheet provides information on composition, physical properties, hardness, elasticity, and bend strength as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-249. Producer or source: Crucible Service Centers. Originally published as CPM REX T15, January 1973, revised March 2007.
Journal Articles
AL TECH SUPER LMW-EXTRA: High-Speed Steel, Type M33
Available to Purchase
Alloy Digest (1981) 30 (10): TS-388.
Published: 01 October 1981
... AL Tech Super LMW-Extra is high-molybdenum high-speed steel containing 8.25% cobalt to improved red hardness. It is most useful for cutting-tool applications in which wear resistance and high-temperature hardness are important properties. This grade should not be use where excessive shock...
Abstract
View articletitled, AL TECH SUPER LMW-EXTRA: High-Speed Steel, Type M33
View
PDF
for article titled, AL TECH SUPER LMW-EXTRA: High-Speed Steel, Type M33
AL Tech Super LMW-Extra is high-molybdenum high-speed steel containing 8.25% cobalt to improved red hardness. It is most useful for cutting-tool applications in which wear resistance and high-temperature hardness are important properties. This grade should not be use where excessive shock or chatter are encountered. Super LMW-Extra is well suited to applications such as machining hard and heat-treated materials and machining both ferrous and nonferrous aircraft alloys. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as heat treating and machining. Filing Code: TS-388. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
AISI TYPE T4: Cobalt High-Speed Tool Steel
Available to Purchase
Alloy Digest (1982) 31 (3): TS-395.
Published: 01 March 1982
... chemical composition fracture toughness hardness heat treatability machinability physical properties red hardness workability UNS T12004 All Filing Code: TS-395 AIS1 Type T4 Tool Steel O8 MARCH 1982 PIGSST - DATA ON WORLD WIDE METALS AND ALLOYS @ might 1980. En&mering Pubiicotiom.Inc.A4Irights...
Abstract
View articletitled, AISI TYPE T4: Cobalt High-Speed Tool Steel
View
PDF
for article titled, AISI TYPE T4: Cobalt High-Speed Tool Steel
AISI Type T4 is made by adding 5% cobalt to the conventional 18% tungsten-4% chromium-1% vanadium (AISI Type T1) tool steel. The cobalt dissolves in the ferrite and strengthens the matrix of the steel whereas the other alloying elements form carbides. Thus the cobalt increases the hot or red hardness, thereby enabling the tool to maintain a higher hardness at elevated temperatures. Type T4 is well adapted for cutting hard, gritty materials such as cast iron or other abrasive materials and for cutting nonferrous alloys at high speeds. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-395. Producer or source: Tool steel mills.
Journal Articles
AISI TYPE M33: Molybdenum High-Speed Steel
Available to Purchase
Alloy Digest (1982) 31 (8): TS-402.
Published: 01 August 1982
... AISI Type M33 is a heavy-duty high-speed steel; it contains 8.00% cobalt to improved red hardness. It is recommended for cutting-tool applications in which wear resistance and high temperature hardness are important characteristics. It should not be used where excessive shock and/or chatter...
Abstract
View articletitled, AISI TYPE M33: Molybdenum High-Speed Steel
View
PDF
for article titled, AISI TYPE M33: Molybdenum High-Speed Steel
AISI Type M33 is a heavy-duty high-speed steel; it contains 8.00% cobalt to improved red hardness. It is recommended for cutting-tool applications in which wear resistance and high temperature hardness are important characteristics. It should not be used where excessive shock and/or chatter are encountered. AISI Type M33 is well suited to uses such as machining hard and heat-treated materials and machining both ferrous and nonferrous aircraft alloys. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-402. Producer or source: Tool steel mills.
Journal Articles
TATMO V-N: High-Speed Steel, Type M7
Available to Purchase
Alloy Digest (1985) 34 (12): TS-452.
Published: 01 December 1985
... TATMO V-N is an AISI Type M7 high-speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting-tool applications requiring an optimum balance of red hardness, edge toughness and wear resistance...
Abstract
View articletitled, TATMO V-N: High-Speed Steel, Type M7
View
PDF
for article titled, TATMO V-N: High-Speed Steel, Type M7
TATMO V-N is an AISI Type M7 high-speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting-tool applications requiring an optimum balance of red hardness, edge toughness and wear resistance, such as drills, taps, end mills, reamers and milling cutters. Its combination of outstanding properties and high hardness makes Tatmo V-N a logical alternate for cobalt high-speed steels in many cutting-tool applications. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-452. Producer or source: Latrobe Steel Company.
Journal Articles
ELECTRITE CO-6: Cobalt High-Speed Steel, Type M36
Available to Purchase
Alloy Digest (1963) 12 (6): TS-35.
Published: 01 June 1963
... ELECTRITE CO-6 is a high-speed steel of the 6 molybdenum-6 tungsten type to which 9% cobalt has been added. This cobalt addition increases the red hardness and permits a retention of greater cutting hardness at elevated temperatures. It is designated as SAE-M36 and AISI Type M36. This datasheet...
Abstract
View articletitled, ELECTRITE CO-6: Cobalt High-Speed Steel, Type M36
View
PDF
for article titled, ELECTRITE CO-6: Cobalt High-Speed Steel, Type M36
ELECTRITE CO-6 is a high-speed steel of the 6 molybdenum-6 tungsten type to which 9% cobalt has been added. This cobalt addition increases the red hardness and permits a retention of greater cutting hardness at elevated temperatures. It is designated as SAE-M36 and AISI Type M36. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-35. Producer or source: Latrobe Steel Company. Originally published July 1955, revised June 1963.
Journal Articles
MOLITE 42: High-Speed Steel, Type M42
Available to Purchase
Alloy Digest (1987) 36 (12): TS-487.
Published: 01 December 1987
... MOLITE 42 is a molybdenum-type super high-speed steel. It has a well-balanced composition designed to give superior performance when used for difficult machining operations. It can be heat treated to a hardness level of Rockwell C 68-70 giving excellent red hardness while maintaining moderate...
Abstract
View articletitled, MOLITE 42: High-Speed Steel, Type M42
View
PDF
for article titled, MOLITE 42: High-Speed Steel, Type M42
MOLITE 42 is a molybdenum-type super high-speed steel. It has a well-balanced composition designed to give superior performance when used for difficult machining operations. It can be heat treated to a hardness level of Rockwell C 68-70 giving excellent red hardness while maintaining moderate toughness. MOLITE is especially recommended for tools used in the machining of high-strength steels, prehardened steels and exotic ferrous and nonferrous alloys such as are used in aircraft and missile work. It is also recommended for ordinary machining jobs requiring long production runs. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-487. Producer or source: Columbia Tool Steel Company.
Journal Articles
WALLEX No. 50: Cobalt-Base Hard Surfacing Alloy
Available to Purchase
Alloy Digest (1974) 23 (9): Co-71.
Published: 01 September 1974
... WALLEX No. 50 is a hard-surfacing alloy with excellent resistance to a combination of abrasion and corrosion. It has good red hardness and excellent weldability. It is supplied as an atomized powder for application with Wall Colmonoy's SPRAY-WELD Process. This datasheet provides information...
Abstract
View articletitled, WALLEX No. 50: Cobalt-Base <span class="search-highlight">Hard</span> Surfacing Alloy
View
PDF
for article titled, WALLEX No. 50: Cobalt-Base <span class="search-highlight">Hard</span> Surfacing Alloy
WALLEX No. 50 is a hard-surfacing alloy with excellent resistance to a combination of abrasion and corrosion. It has good red hardness and excellent weldability. It is supplied as an atomized powder for application with Wall Colmonoy's SPRAY-WELD Process. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and powder metal forms. Filing Code: Co-71. Producer or source: Wall Colmonoy Corporation.
Journal Articles
AISI TYPE H26: Hot Work Tool Steel
Available to Purchase
Alloy Digest (1975) 24 (12): TS-294.
Published: 01 December 1975
... AISI Type H26 hot-work tool steel is the 18 tungsten-4 chromium-1 vanadium high-speed composition with lowered carbon to provide a high-degree of toughness. It has high red hardness and good resistance to abrasion. It is preferable to the conventional hot-work tool steels for applications in which...
Abstract
View articletitled, AISI TYPE H26: Hot Work Tool Steel
View
PDF
for article titled, AISI TYPE H26: Hot Work Tool Steel
AISI Type H26 hot-work tool steel is the 18 tungsten-4 chromium-1 vanadium high-speed composition with lowered carbon to provide a high-degree of toughness. It has high red hardness and good resistance to abrasion. It is preferable to the conventional hot-work tool steels for applications in which higher hardness must be maintained at elevated temperatures. It is also recommended in cold-work that involve long runs, but should not be used where liquid cooling is required. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-294. Producer or source: Tool steel mills.
Journal Articles
PANTHER 5: Cobalt High-Speed Steel
Available to Purchase
Alloy Digest (1976) 25 (5): TS-301.
Published: 01 May 1976
... Panther 5 is a 5% cobalt, high-carbon, high-vanadium, tungsten high-speed steel. Because of its excellent red hardness, higher cutting speeds can be used with Panther 5 than with the regular high-speed steels. Heat treating Panther 5 to its maximum hardness will provide long tool life...
Abstract
View articletitled, PANTHER 5: Cobalt High-Speed Steel
View
PDF
for article titled, PANTHER 5: Cobalt High-Speed Steel
Panther 5 is a 5% cobalt, high-carbon, high-vanadium, tungsten high-speed steel. Because of its excellent red hardness, higher cutting speeds can be used with Panther 5 than with the regular high-speed steels. Heat treating Panther 5 to its maximum hardness will provide long tool life. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-301. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
WALLEX No. 40: Cobalt-Base Hard Surfacing Alloy
Available to Purchase
Alloy Digest (1976) 25 (10): Co-74.
Published: 01 October 1976
... WALLEX No. 40 is a self-fluxing, cobalt-base hard-surfacing alloy with excellent resistance to a combination of corrosion and abrasion and relatively good impact properties. It has excellent red hardness and weldability. It is supplied only as atomized powder for application with Wall Colmonoy's...
Abstract
View articletitled, WALLEX No. 40: Cobalt-Base <span class="search-highlight">Hard</span> Surfacing Alloy
View
PDF
for article titled, WALLEX No. 40: Cobalt-Base <span class="search-highlight">Hard</span> Surfacing Alloy
WALLEX No. 40 is a self-fluxing, cobalt-base hard-surfacing alloy with excellent resistance to a combination of corrosion and abrasion and relatively good impact properties. It has excellent red hardness and weldability. It is supplied only as atomized powder for application with Wall Colmonoy's SPRAYWELD and FUSEWELD processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and powder metal forms. Filing Code: Co-74. Producer or source: Wall Colmonoy Corporation.