Alloy Digest (1988) 37 (6): CS-121.
Published: 01 June 1988
... SAE 1070 is a high-carbon water or oil-hardening tool and spring steel of low hardenability. It is used for railroad and street railway rails, heavy machinery parts, shafts, springs and a wide variety of hand and machine tools requiring strength and wear resistance. This datasheet provides...
Journal Articles
Alloy Digest (1973) 22 (4): CS-51.
Published: 01 April 1973
... AISI 1070 is a high-carbon water or oil-hardening tool and spring steel of low hardenability. It is used for railroad and street railway rails, heavy machinery parts, shafts, springs and a wide variety of hand and machine tools requiring strength and wear resistance. This datasheet provides...