Alloy Digest (2005) 54 (12): SA-553.
Published: 01 December 2005
... Ferrium C69 is a case/core steel with a case hardness of 69 HRC and a core hardness of 50 HRC. It is used in racing applications, where rolling contact fatigue is an issue, and will be undergoing testing by the National Aeronautics and Space Administration (NASA) for aerospace gear applications...
Journal Articles
Alloy Digest (2005) 54 (11): SA-551.
Published: 01 November 2005
... Ferrium C61 is a case/core alloy with ultrahigh strength and excellent fracture toughness. It is used in gears and a number of automotive racing applications. This datasheet provides information on tensile properties. It also includes information on forming and heat treating. Filing Code: SA-551...
Journal Articles
Alloy Digest (2009) 58 (6): Fe-148.
Published: 01 June 2009
... Carpenter AerMet 340 Alloy possesses high hardness and strength while exhibiting exceptional toughness and ductility, and can be considered for a variety of automotive, racing, aerospace, and defense applications. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2018) 67 (9): SA-822.
Published: 01 September 2018
... and plate are also available upon request Applications M54 steel is being used in demanding applications in the aerospace, energy, oil and gas, and racing industries as an upgrade in performance from Maraging 250, 4340, 300M (BS S155), and other steels to reduce component weight or size or increase service...
Journal Articles
Alloy Digest (2020) 69 (11): Ti-172.
Published: 01 November 2020
... racing applications; underground tubes and casing equipment for gas and oil well operations. Supplier Carpenter Technology Corporation 1735 Market Street, 15th Floor Philadelphia, Pennsylvania 19103, USA Tel: +1 610 208 2000 Web: www.carpentertechnology.com For additional information consult the CarTech...
Journal Articles
Alloy Digest (2002) 51 (9): Ti-130.
Published: 01 September 2002
...- ground tubes and casing equipment for gas- and oil-well operations. It is also used in fasteners and high-performance auto racing applications. Producer: Carpenter Technology Corporation Reading, PA 19612-4662 (610) 208-2000 Dynamet Inc. Washington, PA (800) 237-9655 (724) 228-1000 ISSN: 002-614X Ti-130B...
Journal Articles
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... with 0.25 inch maximum depth of cut and a maximum race of feed of 10 sfpm are used for rough milling; while cuaing speeds of 500-700 sfpm with 0.02 inch maxi- mum of cut and a maximum race of feed of 10 sfpm are used for finish milling. In lathe rough turning, cuccing speeds of 500-1,000 sfpm are used...
Journal Articles
Alloy Digest (1968) 17 (6): Cu-188.
Published: 01 June 1968
... strength will actually show a slight decrease. Forms Available: Sand and Centrifugal Castings Applications: Gears, worm wheels, slides, nuts, rolling mill bearings and slippers, ball bearing races are among some of the applications for this alloy. Manufacturer: American Gucible Products Co. Lorain, Ohio t...
Journal Articles
Alloy Digest (1967) 16 (12): TS-200.
Published: 01 December 1967
... through, and cool slowly in the Iumace (4O F per hour) to about lOOOeF, after which the cooling race may be increased. Suitable pre- cautions must be taken to prevent excessive carburi- rarion or decarburization. Strain Relieving: When desirable co relieve the strains of machining, heat slowly co...
Journal Articles
Alloy Digest (1972) 21 (10): SA-281.
Published: 01 October 1972
... STROLOY 503-A is a through-hardening steel developed for bearing races. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-281. Producer or source...
Journal Articles
Alloy Digest (1962) 11 (10): SA-135.
Published: 01 October 1962
... VascoMax 300 CVM is an 18% nickel alloy steel having superior toughness and ductility at yield strength levels up to 300,000 psi. It is recommended for high strength applications in the temperature range -320 F to 900 F. It is a martensitic steel strengthened by precipitation and an ordering...
Journal Articles
Alloy Digest (1963) 12 (1): TS-128.
Published: 01 January 1963
... deg F, quench in a salt bath at 425 deg F, hold ac temperatore for 40 minutes, cool in air or water. Machinability: For most machining operations a fully spheroidized rather than pearlicic scruccure is preferred. Spheroidixe annealed, cold drawn bar has a machi- oabilicy racing of 37% of AISI B1112...
Journal Articles
Alloy Digest (1963) 12 (12): Al-132.
Published: 01 December 1963
...-700 sfpm with 0.02 maximum depth of cut and a maximum race of feed of 10 sfpm are used for finish milling. In lathe rough turning, cutting speeds of 500-1000 sfpm are used with 0.12 inch maximum depth of cut and a maximum race of feed of 0.008 per rev., while in lathe finish turning, cutting speeds...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1968) 17 (9): TS-210.
Published: 01 September 1968
... 165O F. air cool, then anneal. Critical Temperature: AC, 1405┬░F. Stress Relieving: Low-hardness dies for 200 Brinell. Hear at a race of 1 hour per inch of maximum chick- ness co 1250-i30O F, soak for hour per inch, cool in furnace until black, then air cool. High hardness dies for 300 Brinell, heat...
Journal Articles
Alloy Digest (1965) 14 (12): TS-172.
Published: 01 December 1965
... AIRVAN is an air-hardening alloy steel possessing excellent non-deforming properties. It is particularly adapted to applications requiring toughness and fairly high abrasion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1961) 10 (9): SA-120.
Published: 01 September 1961
... Unimach No. 2 is a deep-hardening 5% chromium alloy steel recommended for structural applications in the temperature range of 400-1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (2006) 55 (7): Fe-139.
Published: 01 July 2006
... Metglas 2605 SA1 is an amorphous iron-base soft magnetic alloy designed for extremely low core loss at distribution and power transformer frequencies and inductions. Applications include high-frequency inductors and current transformers. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (3): TS-190.
Published: 01 March 1967
..., heat slowly and evenly to I620-1640oF at a race nor exceeding 2000F per hour. When the steel is co be cooled in still air or by an air blast, hear co 1650- 16700F. Hold ac this temperature for approximately l/2 hour per inch of cross section. Cool small, thin and incricacely shaped sections in still...
Journal Articles
Alloy Digest (1963) 12 (9): SA-154.
Published: 01 September 1963
... ALMAR 25 is a maraging alloy steel having an excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as fuel rocket cases and aircraft landing gears. This datasheet provides information on composition, physical...