1-20 of 723 Search Results for

punches

Sort by
Journal Articles
Alloy Digest (1980) 29 (8): TS-368.
Published: 01 August 1980
... CARPENTER No. 408 Punch Steel was developed specifically to meet the needs of the pharmaceutical industry. It has the necessary wear resistance to withstand the severe conditions of handling the abrasive materials that must be pellitized. It also has high strength in combination with excellent...
Journal Articles
Alloy Digest (1984) 33 (1): TS-421.
Published: 01 January 1984
... AL TECH NAVAHO is an air-hardening punch and die steel with lower carbon than most cold-work steels; this provides an optimum combination of wear resistance and toughness for difficult cold-work applications. It also is used for abrasive hot-work requirements. This steel offers relatively...
Journal Articles
Alloy Digest (1968) 17 (4): TS-204.
Published: 01 April 1968
... La Belle-HT is a high toughness tool steel having remarkable resistance to impact and battering at high hardness levels. It is recommended for cold header punches, shear blades, rivet sets, and aluminum impact extrusion dies and punches. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1979) 28 (10): Bi-14.
Published: 01 October 1979
... BELMONT ALLOY 2481 is a bismuth-base, non-eutectic alloy that melts through the temperature range 218-440 F. It was developed and used originally for making punch dies to produce transformer laminations from silicon steel sheet. It is now also used to make a wide variety of punch dies and plates...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... WINDSOR is a medium-alloy, air-hardening tool steel possessing superior abrasion resistance for long service life. Its inherent wearability and toughness make it particularly adaptable for use in dies and punches in extended production runs. It also has excellent nondeforming characteristics. Its...
Journal Articles
Alloy Digest (1985) 34 (9): TS-447.
Published: 01 September 1985
... grindability. Among its many uses are punches and dies for blanking and forming thin sheet, milling cutters, twist drills, reamers, forming rolls, cold-extrusion punches and draw dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1987) 36 (4): TS-473.
Published: 01 April 1987
... high toughness with the advantages of oil-hardening non-deforming steels. Its relatively high hardenability coupled with high toughness makes it extremely useful for larges shear blades in severe service. Other applications include pneumatic tools, punches, hand chisels, rivet sets and pipe cutters...
Journal Articles
Alloy Digest (1987) 36 (5): TS-475.
Published: 01 May 1987
... is used for impact and shock-resisting tools. Its many uses include shear blades, chisels, punches, rivet sets and mold dies for plastics. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1987) 36 (9): TS-480.
Published: 01 September 1987
... CARPENTER O6 is an oil-hardening tool steel for cold-work applications. It is designed to have free graphite in the microstructure. This free graphite is responsible for the excellent machinability of this grade. Among the many applications of Carpenter O6 are dies for various uses, punches, gages...
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
...) for die work on long production runs. It has superior depth of hardening. Its many applications include cold trimmer dies, lamination dies, plug gages, slitting cutters and blanking, stamping and cold-forming dies and punches for long runs. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1987) 36 (10): TS-483.
Published: 01 October 1987
... variety of cutting-tool applications where improved resistance to abrasion is required. The many uses of Type M7 include twist drills, end mills, shear blades, punches, milling cutters, lathe tools, taps and reamers. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1987) 36 (10): TS-482.
Published: 01 October 1987
... strength and long runs between grinds are necessary. Among its many applications are blanking dies, burnishing tools, beading rolls, lathe centers, plug gages, spinning tools, slitters and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Journal Articles
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... where typical applications include extrusion dies for brass, hot-punch tools and forging-die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well...
Journal Articles
Alloy Digest (2021) 70 (4): TS-812.
Published: 01 April 2021
... Crucible REX M4 is a special-purpose high-speed tool steel that is designed to provide high wear resistance in tools. Its high vanadium and carbon content provides superior resistance to cratering and wear in cold work punches, die inserts, and cutting applications involving high speed and light...
Journal Articles
Alloy Digest (1967) 16 (10): TS-198.
Published: 01 October 1967
... HURON is an oil hardening high-carbon high-chromium die steel designed for cold work applications involging wear or abrasion. It is recommended for long run punch, blanking and stamping requirements. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1968) 17 (6): TS-207.
Published: 01 June 1968
... AIR HARD is an air or oil hardening, high-carbon tool and die steel for minimum distortion after hardening. It is used for blanking and forming dies, rolls, punches, and other such applications where a deep hardening, non-deforming steel with good resistance to wear is desired. (Also furnished...
Journal Articles
Alloy Digest (1968) 17 (8): TS-209.
Published: 01 August 1968
... Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1968) 17 (2): TS-202.
Published: 01 February 1968
... FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides...
Journal Articles
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information...
Journal Articles
Alloy Digest (1969) 18 (8): TS-222.
Published: 01 August 1969
... VAN LOM is a molybdenum type high-speed steel having excellent wear and cutting properties. It is recommended for cutting tools, punches, shear blades, blanking dies, etc. where improved toughness is desired. This datasheet provides information on composition, physical properties, hardness...