Journal Articles
Alloy Digest (1976) 25 (3): SS-326.
Published: 01 March 1976
... treatability joinability machinability physical properties tensile properties wear resistance workability AQUAMET 17 Filing Code: SS-326 Stainless Steel MARCH 1976 - DATA ON WORLD WIDE METALS AND ALLOYS AQUAMET* 17 (Shafting Material for Boats, Pumps and Valves) AQUAMET 17 is a precipitation-hardening...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... physical properties tensile properties AQUAMET 18 Filing Code: SS-332 Stainless Steer AUGUST 1976 - DATA ON WORLD WIDE METALS AND ALLOYS ACNJAMET* 18 (Shafting Material for Boats, Pumps and Valves) +blisbed by EagkmngAUoysDigut,IIK. Upper Monalair, New Jersey AQUAMET 18 is a low-nickel austenitic...
Journal Articles
Alloy Digest (1956) 5 (10): SA-48.
Published: 01 October 1956
... NITRALLOY 225 is a special alloy steel which can be nitrided, that is, surface hardened, without final quenching, by the action of ammonia gas at relatively low temperatures. It is used for pump shafts, bearing bushings, connecting rods, press rolls, steam valves, sreel stamping dies. and hot work...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1982) 31 (1): SS-400.
Published: 01 January 1982
... pump shafts, gears, cams and pivots. This alloy is not usually recommended for vessels containing gases or liquid under high pressure. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... of media. Its many uses include scrapper blades, screw conveyor flights and sleeves for seawater pump shafts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (2014) 63 (4): Ni-666.
Published: 01 April 2014
... 200 °F) 14.19 (7.88) 25 204 °C (77 400 °F) 14.36 (7.98) 25 316 °C (77 600 °F) 14.69 (8.16) Mechanical Properties: Young s modulus, GPa (106 psi) 200.8 (29.1) Mechanical properties of aged round bar of 945X, pump shafts grade 945X and limiting properties are shown compared to 945 and 925 in Tables 1 4...
Journal Articles
Alloy Digest (1979) 28 (5): Cu-373.
Published: 01 May 1979
... BUNTING Alloy 937 is a cast bushing and bearing bronze. It is one of the most satisfactory materials to use where shaft alignments or shaft wear is a problem. It has a good load capacity and excellent anti-friction characteristics. Its many uses include pressure-tight castings, corrosion-resistant...
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
... MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder...
Journal Articles
Alloy Digest (1967) 16 (5): Cu-176.
Published: 01 May 1967
... COPPER ALLOY No. 630 is a heat treatable aluminum bronze combining wear resistance with high strength and good corrosion resistance. It is recommended for propellers, pump parts, and valves, gears, shafts and pickling equipment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-495.
Published: 01 January 1996
... Colmonoy No. 635, a Nickel-base hard surfacing Alloy, contains a formulated mixture of both crushed and atomized powders. It achieves a hardness of RC 58-63 with tungsten carbide particles. Typical applications include hardfacing of pump components and shaft sleeves. It is supplied as a powder...
Journal Articles
Alloy Digest (1983) 32 (5): Cu-458.
Published: 01 May 1983
... Copper Alloy No. C61000 is an aluminum bronze containing nominally 92% copper and 8% aluminum. It is characterized by medium strength, medium ductility and a good capacity for being hot formed or cold worked. It has good resistance to corrosion. Its many uses include shafts, pump parts and bolts...
Journal Articles
Alloy Digest (1984) 33 (1): Cu-465.
Published: 01 January 1984
... suitable for decorative applications. Its engineering uses include shafts, bolts and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1991) 40 (8): Cer-6.
Published: 01 August 1991
... and wear resistance. Dies and rollers used in aluminum steel forming, pump shafts and bearings. Producers: Kyocera Industrial Ceramics Corp. Vancouver. Cl ashington 98661. DOI: 10.31399/asm.ad.cer0006 Copyright © ASM International® 1996 ...
Journal Articles
Alloy Digest (2006) 55 (3): Cu-741.
Published: 01 March 2006
... machinability Fully weldability Superior galling resistance compared to nickel-aluminum bronze Table 2 shows a comparison of this grade to two other alloys with similar applications and uses. ! Bars and sections " Applications include pump shafts, valve spindles, bushes for heavy equipment...
Journal Articles
Alloy Digest (2006) 55 (6): Cu-744.
Published: 01 June 2006
...-Al bronze 247 36 0.075 4.3 Hiduron 191 425 62 0.02 4.8 DOI: 10.31399/asm.ad.cu0744 Applications: Defense applications include control elements of submarines, pump shafts, mechanical seals, gears, hose couplings, propeller shafts, and drive bushes. The alloy is used as tubes and tube plates for heavy...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... exchangers. propeller and pump shafts, transfer piping for petroleum refineries, cladding for refinery crude columns, sulfuric and hydrofluoric acid plants, sheathing for offshore structures and similar applications. Manufacturer: Vereingte Deutsche Metallwerke AG Duisburg/ Werdohl. Federal Republic...
Journal Articles
Alloy Digest (2006) 55 (2): Cu-740.
Published: 01 February 2006
... 0.005 0.010 Tips Carbide tipped using water-soluble lubricant DOI: 10.31399/asm.ad.cu0740 ! Bars and sections " Pump shafts, valve stems and trim, flanges and pipe fittings, fasteners, bearing and bushes, gears, worm wheels, marine propeller shafts, springs wear plates, deep-drawing dies...
Journal Articles
Alloy Digest (1961) 10 (4): CS-15.
Published: 01 April 1961
..., spring clips, turbine and pump shafts, worms, crane and mine car axles, lead screws, racks. printing press parts, conveyor pins and rollers, piston rods, line shafts, impeller shafts, welded shanks on high speed twist drills. Manufacturer: Reed in. /rev. 0.015 0.015 0.015 0.030 0.030 0.030 Depth of Cut...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... mesh (63 m) + 15 m Applications: Coatings of Colmonoy 63HV are used for hard surfacing petroleum industry components such as gate valves, pump sleeves, pump shafts, bushings, wear rings, and compressor rods; they can also be used to restore dimensions. Coatings of Colmonoy 63HV are also used...