1-20 of 390

Search Results for pump parts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1980) 29 (5): Cu-394.
Published: 01 May 1980
... by high elastic and fatigue strengths, excellent resistance to wear and high resistance to general corrosion. Its many uses include springs, fuse clips, switch parts, pump parts and welding equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1984) 33 (10): Ni-304.
Published: 01 October 1984
... NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers...
Journal Articles
Alloy Digest (1975) 24 (7): Cu-299.
Published: 01 July 1975
... ATLANTIC 25 Alloy is a heat-treatable aluminum-nickel-iron bronze for castings that combine high strength with excellent resistance to corrosion. It is wear and abrasion resistant. It is also nonmagnetic and resistant to sparking. Its uses include gears, bearings, pump parts and other corrosion...
Journal Articles
Alloy Digest (1979) 28 (1): CI-47.
Published: 01 January 1979
... it has a tensile strength of about 95,000 psi and a compressive strength of 360,000 psi. Typical applications are pump parts, mixers and coal-gasification components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1983) 32 (5): Cu-458.
Published: 01 May 1983
... Copper Alloy No. C61000 is an aluminum bronze containing nominally 92% copper and 8% aluminum. It is characterized by medium strength, medium ductility and a good capacity for being hot formed or cold worked. It has good resistance to corrosion. Its many uses include shafts, pump parts and bolts...
Journal Articles
Alloy Digest (1984) 33 (1): Cu-465.
Published: 01 January 1984
... suitable for decorative applications. Its engineering uses include shafts, bolts and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1984) 33 (8): Cu-481.
Published: 01 August 1984
... and good resistance to corrosion. Its uses include bushings gears, bearings and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1984) 33 (11): Cu-486.
Published: 01 November 1984
... and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-486. Producer or source: Mueller Brass...
Journal Articles
Alloy Digest (1985) 34 (2): Cu-491.
Published: 01 February 1985
... include bearings, gears, pump parts, connecting rods, marine hardware and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production...
Journal Articles
Alloy Digest (1986) 35 (9): Cu-514.
Published: 01 September 1986
... many applications are bearings, bushings, connecting rods, pump parts, gears, cams and seal rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1967) 16 (5): Cu-176.
Published: 01 May 1967
... COPPER ALLOY No. 630 is a heat treatable aluminum bronze combining wear resistance with high strength and good corrosion resistance. It is recommended for propellers, pump parts, and valves, gears, shafts and pickling equipment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1969) 18 (1): Cu-195.
Published: 01 January 1969
... Mueller 6730 is a forgeable (leaded) bronze bearing alloy possesing good machinability for use with hard or soft mating members where moderate strength will suffice. It is recommended for gears, pump parts, thrust bearings, valve seats, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1993) 42 (9): SS-550.
Published: 01 September 1993
..., bushings, valve components, cutlery and pump parts. Designers may also consider Type 440C vacuum are remelted (VAR) for aerospace and small precision bearings. In these applications improved cleanliness, superior fatigue properties, high strength and corrosion resistance are critical design considerations...
Journal Articles
Alloy Digest (1997) 46 (11): SS-702.
Published: 01 November 1997
... types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1997) 46 (12): SS-704.
Published: 01 December 1997
..., and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance, and corrosion resistance. Filing Code: SS-704. Producer or source: Central Iron...
Journal Articles
Alloy Digest (1998) 47 (1): SS-705.
Published: 01 January 1998
..., and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS...
Journal Articles
Alloy Digest (1998) 47 (2): SS-706.
Published: 01 February 1998
..., and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS...
Journal Articles
Alloy Digest (1966) 15 (8): SS-185.
Published: 01 August 1966
... ENDURO S-1 is a chromium type stainless steel providing high strength, toughness and resistance to impact when heat treated. It shows resistance to wet and dry corrosion. It is recommended for steam turbine parts, valves, cutlery, pump components, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1984) 33 (10): Cu-484.
Published: 01 October 1984
.... Applications: Mueller Alloy 6733 is used for pump parts, clutch bearings. shaft bushings, lead screw nuts, cams, pump parts and seal rings. Manufacturer: Mueller Brass Company Port Huron. Michigan 48060. Specification Equivalents: UNS No. C67300. SAE 5461 and 5463. ...