1-20 of 92 Search Results for

pump bodies

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
... MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-408.
Published: 01 December 1980
... AMPCOLOY 521 is a cast copper-nickel alloy with excellent resistance to many highly active corrosives, particularly saline waters and sulfuric and phosphoric acids. It has high strength and good ductility and can be welded readily. Its many applications include valves, pump bodies, steam fittings...
Journal Articles
Alloy Digest (1982) 31 (11): Al-241.
Published: 01 November 1982
... ALUMINUM 296.0 is an aluminum permanent-mold casting alloy that responds to an age-hardening heat treatment. It is recommended for applications that require a combination of high tensile properties and good machinability. Among its many uses are fuel pump bodies, aircraft fittings and seat frames...
Journal Articles
Alloy Digest (1984) 33 (4): Cu-475.
Published: 01 April 1984
... in the form of continuous castings and its uses include bearings, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining...
Journal Articles
Alloy Digest (1984) 33 (11): Cu-487.
Published: 01 November 1984
... Copper Alloy No. C93900 is a cast bronze of fairly low strength. It has good machinability and good resistance to corrosion. Its commercial names formerly used (not recommended) are: (1) High-Leaded Tin Bronze and (2) 79-6-15. Among its uses are bearings for general service and pump bodies...
Journal Articles
Alloy Digest (1976) 25 (9): Cu-319.
Published: 01 September 1976
... and pump bodies that must resist corrosion by seawater. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-319...
Journal Articles
Alloy Digest (1968) 17 (10): Cu-192.
Published: 01 October 1968
... PROMET No. 3 is a leaded tin bronze possessing a good combination of physical properties and corrosion resistance. It is recommended for bearings, gears, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1987) 36 (12): Al-285.
Published: 01 December 1987
... UNS No. A02060 is an aluminum-mold casting alloy that responds to an age-hardening heat treatment. It is recommended for applications that require a combination of high tensile properties and good machinability. Among its many uses are fuel pump bodies, aircraft fittings and seat frames...
Journal Articles
Alloy Digest (1963) 12 (8): Cu-132.
Published: 01 August 1963
... OUNCE Metal, also known as Composition Metal, is a cast 5% leaded bronze recommended for bearings, valves and pump bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1985) 34 (10): Al-261.
Published: 01 October 1985
... and bodies for fuel pumps. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as casting, heat treating, machining...
Journal Articles
Alloy Digest (1998) 47 (11): SS-724.
Published: 01 November 1998
... Type CG6MMN is a 22Cr-12.5Ni-5Mn-2.25Mo alloy that is the cast equivalent of Nitronic 50 (see Alloy Digest SS-304, revised April 1990). The alloy is used as castings for pump and valve bodies to resist a wide variety of environments that corrode type 316 (CF8M). This datasheet provides information...
Journal Articles
Alloy Digest (1968) 17 (8): Zn-11.
Published: 01 August 1968
... ILZRO-14 is a zinc-base die casting alloy developed with superior creep resistance at both ambient and elevated temperatures. It is recommended for carburetors, fuel pumps, valve bodies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1969) 18 (8): Ni-146.
Published: 01 August 1969
... investment castings and centri- fugal castings. Applications: Chemical plant equipment, pump bodies, pump impel- lers, valves and fuctures, thrust and rotary bearings, cutter blades where corrosion is a problem. An inter- esting application of this alloy involves its use in handling molten lead and other low...
Journal Articles
Alloy Digest (1955) 4 (5): Cu-26.
Published: 01 May 1955
... or medium loads, pump bodies. Ampco Metal, Inc Mihvauk~ wkonsin ...
Journal Articles
Alloy Digest (2022) 71 (12): CI-100.
Published: 01 December 2022
... microstructure in the center area (Etched in 5% Nital. 100├Ś) Flood gates; food service equipment; insecticide pumps; piston ring inserts; pump bodies; sea water valve bodies; valve guides. Supplier Dura-Bar Metal Services 2195 West Lake Shore Drive Woodstock, Illinois 60098, USA Tel: +1 888 387 2277 Web...
Journal Articles
Alloy Digest (1970) 19 (7): Cu-218.
Published: 01 July 1970
... will tolerate higher loads and speeds and resist pounding to a greater degree then PROMET 6. Forms Available: Sand and centrifugal castings. Applications: Bearings for machine tools, paper machinery, pump bodies and mine water pump parts. mill bearings and general purpose wear parts. Manufacturer: The American...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-380.
Published: 01 September 1979
... of the requirements of the copper-nickel alloys but at a lower cost than that of the 70% copper- 30% nickel alloy. Forms Available: Castings: sand and centrifugal. Applications: Parts that must resist corrosion by seawater; such parts comprise valves, pump bodies, pump impellers, propeller sleeves, flanges and elbows...
Journal Articles
Alloy Digest (1961) 10 (1): Cu-96.
Published: 01 January 1961
... hydrochloric acid at room temperatute. Specification Equivalents: Navy 46B18C1.4 MIL 16033 ASTM 148 Alloy 9D Forms Available: Sand castings and ceottifugal castings; forgings. Applications: Ship propellers, bearings, valves and valve seats, impellers, pump bodies, molds and dies. Manufacturer: Baldwin-Lima...
Journal Articles
Alloy Digest (2010) 59 (5): Ta-13.
Published: 01 May 2010
... for use in steam heating in corrosive atmospheres Heat exchangers, condensers and coils Thermocouple protection sheaths, loose lines or machined from solid Pumps, bodies or cases, shafts and impellers, for corrosive chemical solutions ...
Journal Articles
Alloy Digest (1959) 8 (5): Mg-41.
Published: 01 May 1959
... be avoided. Forms Available: Extruded bars and sections, extruded tubes, plate, sheet and strip. Applications: Bearing housings, rocker arm supports, valve and pump bodies, control levers, brackets, fittings, hydraulic cylinders, aircraft wings, canoes, bus and trailer bodies, stampings requiring subsequenr...