Alloy Digest (1997) 46 (3): Cu-611.
Published: 01 March 1997
... Federalloy I-844 (C89831) is a lead-free bronze casting alloy that is machinable by alloying additions of bismuth. Applications include bearings (high speed and heavy pressure), pumps, impellers, and corrosion-resistant and pressure-tight castings. This datasheet provides information...
Journal Articles
Alloy Digest (2021) 70 (5): CI-81.
Published: 01 May 2021
... produced parts for automobiles as well as for small hydraulic bodies that must be pressure tight. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on low and high temperature performance as well as casting, heat treating...
Journal Articles
Alloy Digest (1953) 2 (8): Mg-6.
Published: 01 August 1953
... ELEKTRON ZRE1 is a magnesium-base casting alloy which combines excellent creep resistance up to about 500 F with good room temperature properties. It is completely free from microporosity and very suitable for applications requiring pressure tightness. This datasheet provides information...
Journal Articles
Alloy Digest (1954) 3 (7): Al-18.
Published: 01 July 1954
... ALUMINUM 355 is a heat treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for light weight, high strength, pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1954) 3 (9): Al-20.
Published: 01 September 1954
... ALCAN 135 is a heat treatable aluminum casting alloy having high strength, pressure tightness, and is capable of being cast in intricate shapes. It has high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1954) 3 (10): Al-21.
Published: 01 October 1954
... ALUMINUM 356 is a heat treatable aluminum casting alloy recommended for high strength, pressure-tight castings, and intricate shapes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1954) 3 (12): Mg-14.
Published: 01 December 1954
... ELEKTRON MCZ is a magnesium base casting alloy having excellent creep resistance up to 500 F. It is suitable for applications where pressure tightness is required, and has good resistance to corrosion. Its properties are generally similar to those of Elektron ZRE1. This datasheet provides...
Journal Articles
Alloy Digest (1955) 4 (3): Al-24.
Published: 01 March 1955
... BA.46 is a heat treatable aluminum casting alloy. It is recommended for high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating...
Journal Articles
Alloy Digest (1955) 4 (7): Al-29.
Published: 01 July 1955
... ALAR 00.5 is a 5% silicon-aluminum casting alloy having high corrosion resistance. It is suitable for pressure-tight and thin-walled castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1955) 4 (12): Mg-21.
Published: 01 December 1955
... parts which might not be made pressure tight in an alloy such as Dowmetal C. It is used in the artificially aged condition (T5). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
... ALLCAST 41A is an aluminum-silicon-copper casting alloy. It responds to an age-hardening heat treatment and is recommended for light weight, high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1968) 17 (10): Al-180.
Published: 01 October 1968
... FEDERATED F460 is a heat treatable, aluminum-base, sand and permanent mold casting alloy having good foundry characteristics and pressure tightness. It is recommended for general purpose castings in either the as-cast or heat treated condition. The F460PT grade is specially processed during...
Journal Articles
Alloy Digest (1969) 18 (1): Al-183.
Published: 01 January 1969
... ALUMINUM F214 is an aluminum-magnesium-silicon sand casting alloy having good resistance to hot cracking and fair resistance to pressure tightness. It is recommended for ornamental hardware and architectural castings requiring anodizing. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
... Rio Tinto 319.2 is a heat-treatable, Al-Si-Cu casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. Alloy 319.0 exhibits very good castability and pressure tightness, moderate strength, and good high-temperature...
Journal Articles
Alloy Digest (1986) 35 (8): Al-270.
Published: 01 August 1986
... AA B443.0 is an aluminum-5% silicon casting alloy recommended for castings of intricate design and thin walls. It is pressure-tight and has good corrosion resistance and good ductility and toughness. Its wide range of uses include architectural, marine and ornamental components. This datasheet...
Journal Articles
Alloy Digest (1986) 35 (12): Al-274.
Published: 01 December 1986
... UNS No. A03560 is a heat-treatable aluminum casting alloy. Normally it is used only when heat-treated (aged) strengths are required. It is recommended for high-strength, pressure-tight castings, intricate shapes and where good resistance to corrosion is needed. Its many applications include crank...
Journal Articles
Alloy Digest (1988) 37 (9): Al-291.
Published: 01 September 1988
... AA 355.0 is a general-purpose, high-strength casting alloy containing silicon and copper as the major alloying elements. Its casting characteristics are excellent and it is recommended for pressure-tight castings. It can be age hardened and has good resistance to corrosion. This datasheet provides...
Journal Articles
Alloy Digest (1989) 38 (1): Al-294.
Published: 01 January 1989
... AA 308.0 is a heat-treatable sand and permanent-mold aluminum casting alloy recommended for general-purpose castings. It has good casting characteristics and pressure tightness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1991) 40 (2): Al-312.
Published: 01 February 1991
... UNS No. A03840 is a general-purpose alloy for making intricate die castings. It has good castability and foundry characteristics good machinability and good strength. It is an excellent alloy for large thin-walled castings, and is suitable for castings requiring pressure tightness. This datasheet...
Journal Articles
Alloy Digest (1965) 14 (11): Al-149.
Published: 01 November 1965
... Alcan 143 is a copper-silicon type aluminum die casting alloy having excellent fluidity, castability and improved machinability. It is recommended for pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...