1-20 of 206 Search Results for

pressure die casting

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2020) 69 (10): Al-469.
Published: 01 October 2020
... Alcoa EZCast-NHT A152 and A153 are proprietary, non-heat-treatable, high-pressure die casting (HPDC) aluminum alloys in which magnesium is the principal alloying element. These alloys develop the required strength and toughness in the as-cast condition, thus eliminating or minimizing numerous...
Journal Articles
Alloy Digest (1995) 44 (2): Al-332.
Published: 01 February 1995
.... tnc. All rghls r(LFBNBd. Publrshedby: Alloy DigesI. Inc. IZO1-677.9161 L?afashwnivattobsusedlor 27 Canfield SIreel. Orange. N.J. 07U50 / U.S.A Jpecrication or fmt desgn. DURALCAN F3N.l OS/F3N.20S (Aluminum metal matrix composite for pressure die castings) DURALCAN F3N.xxS is an aluminum composite...
Journal Articles
Alloy Digest (2023) 72 (4): Al-497.
Published: 01 April 2023
... BSI LM2 is an aluminum-silicon-copper casting alloy (3xx.x series). It is essentially a pressure die casting alloy with excellent casting characteristics. Castings made from BSI LM2 have a higher tensile strength and better machinability than pressure die castings made from either BSI LM6 or BSI...
Journal Articles
Alloy Digest (2023) 72 (8): Al-501.
Published: 01 August 2023
... Raffmetal EN AB-Al Si10Mg(Fe) (EN AB-43400) is an aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing high pressure die castings and low pressure die castings for applications requiring a combination of excellent casting characteristics, good...
Journal Articles
Alloy Digest (2021) 70 (10): Al-481.
Published: 01 October 2021
... Rheinfelden Castasil-37 (AlSi9MnMoZr) is an aluminum-silicon-manganese-molybdenum-zirconium high pressure die casting (HPDC) alloy. It was developed by Rheinfelden Alloys GmbH for the production of large and complex high pressure die castings for automotive structural applications. This alloy...
Journal Articles
Alloy Digest (1977) 26 (5): TS-318.
Published: 01 May 1977
... POTOMAC M is a chromium-molybdenum-vanadium hot-work tool steel developed as a die material for aluminum-base die casting. Its superiority in pressure die casting is due to its excellent mechanical properties at elevated temperatures, its excellent machinability and its freedom from scaling...
Journal Articles
Alloy Digest (2021) 70 (5): Al-476.
Published: 01 May 2021
... Rheinfelden Castasil-21 (Ci-21, AlSi9Sr) is an aluminum-silicon-iron-strontium high pressure die casting (HPDC) alloy. It was developed by Rheinfelden Alloys GmbH and Co. KG for castings that require an outstanding combination of electrical and/or thermal conductivity. This datasheet provides...
Journal Articles
Alloy Digest (2021) 70 (7): Al-478.
Published: 01 July 2021
... Alcoa 560 is a proprietary, non-heat-treatable, aluminum-magnesium-manganese alloy developed by Alcoa in the late 1990s for high pressure die cast structural components. This alloy develops the required strength and toughness in the as-cast condition, thus eliminating or minimizing numerous...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
... on machinability as does lead. EnviroBrass III contains up to 1.2% Bi and 0.1% Se and is suitable for permanent mold and pressure die castings. SeBiLOY was the original name used to represent these alloys (see SeBiLOY I, Alloy Digest Cu-605, June 1996, and SeBiLOY II, Alloy Digest Cu-606, revised October 1996...
Journal Articles
Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... Alcoa EZCast 370 is a heat-treatable, aluminum-silicon-magnesium-manganese high-pressure die casting (HPDC) alloy which is widely used for thin-walled, crash-resistant, structural components for automotive applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2022) 71 (5): Al-487.
Published: 01 May 2022
... of aging temperature on the properties of Anticorodal-04. Aging time of 7 h each. Table 1 Mechanical properties at room temperature Casting method Sand casting Sand casting Gravity die casting Gravity die casting High pressure die casting Temper F T7 F T7 F 0.2% proof strength MPa ksi 60 100 9 15 160 180...
Journal Articles
Alloy Digest (1965) 14 (12): Al-150.
Published: 01 December 1965
... at 165-185oC (329-3650F) for 5-7 hours, air cool. Stabilizing Treatment: For dimensional stability, heat at 220-2300C (428-446oF) for 4-6 hours, air cool. (Pressure die castings cannot be solution heat treated on account of blistering.) Mochinobility: This alloy is rather difficult to machine because...
Journal Articles
Alloy Digest (1955) 4 (7): Al-29.
Published: 01 July 1955
... strength, psi TENSILE PROPERTIES* - CASTINGS Sand Cast 16900-19100 7550-8950 3s 8950 13500 Permanent Mold 20200-22400 8950-10100 45 11200 18000 * (Tensile properties from British D.T.D. machined bars. As-cast ASTM bars may give slightly higher properties). TYPICAL PRESSURE DIE CAST PROPERTIES TYPICAL DIE...
Journal Articles
Alloy Digest (1968) 17 (2): Al-172.
Published: 01 February 1968
.... (Pressure die castings may blister on heat treat- ment) Machinability: This alloy is rather difficult to machine because of the rapid tool wear caused by the high silicon content and because of its tendency to drag. Carbide-tipped tools with large rake angles and relatively low cutting speeds give...
Journal Articles
Alloy Digest (1956) 5 (11): Al-45.
Published: 01 November 1956
...-10100 Elongation, 70 in 2 ;zo 5-o-10.0 BrineIl hardness Ixod impact, ft. Ibs. 5i25 Endurance limit, psi (5 x 108 @es) 6t;O 11;oo Shear strength, psi 18000 Table 2 - TYPICAL PRESSURE DIE CAST PROPERTIES Tensile strength, psi 39000 Yield strength, psi (0.2%) 21000 Elongation, 70 in 2 2.0 Endurance...
Journal Articles
Alloy Digest (2023) 72 (3): Al-495.
Published: 01 March 2023
... for Sand casting Permanent mold casting Gravity die casting Low pressure die castings Pressure die casting Fluidity Resistance to hot tearing Pressure tightness Machinability Resistance to corrosion Anodizing against corrosion Anodizing against dyeing Bright anodizing Electro plating Vitreous enamelling...
Journal Articles
Alloy Digest (2023) 72 (6): TS-835.
Published: 01 June 2023
... Applications Extrusion; fasteners (bolts and nuts); fine blanking, stamping, and blanking; forging (hot or semi-hot); general components for mechanical engineering; gravity or low pressure die casting; high pressure die casting; hot runner systems; injection molding; press hardening or hot stamping; rolling...
Journal Articles
Alloy Digest (2023) 72 (8): TS-837.
Published: 01 August 2023
.... 3 Tempering chart Applications Automotive components (piston rings, sensors, turbochargers, etc blow molding; extrusion; forging (hot/semi-hot); general components for mechanical engineering; gravity/ low pressure die-casting; high pressure die-casting; injection molding; machine knives; press...
Journal Articles
Alloy Digest (1991) 40 (1): Al-311.
Published: 01 January 1991
... obtained from ASTM standard round die cast specimens, l/4 diam., produced on a cold chamber (high-pressure) die casting machine. Designers often use 65-75% of these small specimen properties in evaluating actual casting properties. Table 2 - TENSILE PROPERTIES AT VARIOUS TEMPERATURES Test temperature, F...
Journal Articles
Alloy Digest (1990) 39 (10): Al-308.
Published: 01 October 1990
... cast test specimens, l/4 diameter, produced on a cold chamber (high pressure) die casting machine. Designers often use 65-75% of the small specimen properties in evaluating actual casting properties. 0.095 1105-1035 37 0.27 65.21 113.05 11.6 x 106 Table 2 -ELEVATED TEME%RATURE TENSILE PROPERTIES Test...