Alloy Digest (1957) 6 (8): Fe-14.
Published: 01 August 1957
... ISO-ELASTIC is an iron-nickel alloy having low temperature coefficient of the modulus of elasticity. It is suitable for precision instrument springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2010) 59 (12): Co-120.
Published: 01 December 2010
... Applications: Applications include electrical components, springs, and instruments parts in medical, chemical food processing, and marine environments. Producer: Hamilton Precision Metals Lancaster, PA 17601-2334 USA Tel: (800) 476-7065 and (717) 569-7061 Fax: (717) 569-7642 www.hp-metals.com ISSN: 002-614X...
Journal Articles
Alloy Digest (1963) 12 (6): Co-16.
Published: 01 June 1963
.... Round wire requires a cold reduc- cion of 4548% in cross-sectional area Forms Available: Strip and wire. Applications: Watch springs, main springs, power springs, pen nibs, corrosion resistanr ball bearings, flapper valves, textile thread guides, drawing instruments, sewing machine parts, cutlery, valve...
Journal Articles
Alloy Digest (1986) 35 (10): Cu-516.
Published: 01 October 1986
... instrument parts and electromechanical spring components. Manufacturer: Brush Wellman Inc. Alloy Division Cleveland. Ohio 441 IO. ...
Journal Articles
Alloy Digest (2011) 60 (2): Ni-686.
Published: 01 February 2011
... (12.0 in A foil product is available in thicknesses down to .00254 mm (0.0001 in.) and a maximum width of 102 mm (4.0 in The material corresponds to UNS N02270. Applications: Applications include electrical components, springs, and instruments parts in medical, chemical food processing, and marine...
Journal Articles
Alloy Digest (2006) 55 (12): Co-115.
Published: 01 December 2006
... industries, aeronautical and aerospace equipment, automotive injection systems, various diaphragms, naval equipment, weaponry, prostheses for osteosynthesis, pacemaker electrodes, special collars for missiles, automotive ABS systems, surgical implants and medical instruments, and printer springs. Producer...
Journal Articles
Alloy Digest (2017) 66 (6): SS-1265.
Published: 01 June 2017
... of instruments to be exposed to magnetic fields, e.g., surgery under MRI. Further uses include spring components in generators or nonmagnetic housing in measuring instruments. Producer: Lamineries MATTHEY SA 2520 La Neuveville, Switzerland Tel: +41 (0)32 752 32 32 Fax: +41 (0)32 752 32 00 www.matthey.ch ISSN...
Journal Articles
Alloy Digest (1968) 17 (1): Fe-32.
Published: 01 January 1968
... filters, tuning fork. end vibrating reed.; spring applications such 8. Bourbon tubes, eneroid cap.ule., geophysical instruments, hair spying. for timhrg device.. diaphragms. end weighing instrument.; and sppli- cstions requiring low coefficient of thermal ew~nsion and high strength. Manufacturer...
Journal Articles
Alloy Digest (1956) 5 (9): Ag-2.
Published: 01 September 1956
... conductivity spring clips for miniature vacuum tubes, instrument and relay springs requiring high electrical con- ductivity and/or at high ambient temperature. Manufacturer: Handy % Harman New York 38, New York ...