Alloy Digest (1981) 30 (10): Cu-424.
Published: 01 October 1981
... with higher zinc contents. Typical uses are plumbing pipe and condenser and heat-exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-400.
Published: 01 August 1980
... International air-conditioning ANACONDA COPPER 122 chemical composition corrosion-resistant alloys ductility elasticity fatigue properties hardness heat treatability joinability machinability physical properties pipes plumbing applications tensile properties tubes workability wrought...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-450.
Published: 01 December 1982
... fixtures, general hardware, plumbing goods, small gears and pipe fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1961) 10 (7): Cu-103.
Published: 01 July 1961
... and Red Brass, but the latter names are no longer used. This alloy,nored for its rich golden color, is frequently used to imitate gold in costume jewelry and related products. Extensively used for plumbing and indusaial piping, ir has excellent corrosion resistance to water. It withstands repetitive...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-455.
Published: 01 March 1983
... zinc contents. It is used in such applications as condenser tubes, architectural trim, plumbing lines and costume jewelry. Forms Available: Sheet, strip, plate, wire, rod, bar and tube. Applications: Anaconda Alloy 230 is used in a wide range of applications: commercial water pipe, architectural...
Journal Articles
Alloy Digest (1972) 21 (3): Cu-252.
Published: 01 March 1972
... tubes, architectural trim, plumbing lines and costume jewelry. Forms Available: Bar. rod, true. plate. sheet. strip, pipe, tube. extrusions. Applications: Conden>er and heat exchanger tubes, tlcvibls hose, pickling irale). plumbing pipe. pump lutes, architectural trun, tire eutlnguishers, iahteners...
Journal Articles
Alloy Digest (1972) 21 (3): Cu-253.
Published: 01 March 1972
... and water lines, tanks, oil coolers, hydraulic and oil lines, gage lines, oil burner tubes, plumbing pipe and tube, rotating bands. Manufacturer: Practically all copper mills. ...
Journal Articles
Alloy Digest (1973) 22 (12): Cu-273.
Published: 01 December 1973
... are available from major mills throughout the world. Applications: Refrigerator and air conditioner tubing and components, commutators, clad products, gas and burner lines and units, oil burner tubes, condenser and heat exchanger tubes, pulp and paper lines, steam and water lines, tank gage lines, plumbing pipe...
Journal Articles
Alloy Digest (1996) 45 (7): Cu-606.
Published: 01 July 1996
.../selenium-containing Se- BiLOY are essentially equivalent to standard plumbing brasses. Therefore, plumbing goods currently made in leaded brasses should not have to be redesigned when cast in the new alloy. The mechanical properties listed in Table I were derived 6om stand- ard test bars cast according...
Journal Articles
Alloy Digest (1996) 45 (6): Cu-605.
Published: 01 June 1996
.... (b) Bi:Se ratio 2 2: 1 Mechanical Properties: The mechanical properties of bismuth/selenium-containing Se- BiLOY are essentially equivalent to standard plumbing brasses. That means plumbing goods currently made in leaded brasses should not have to be redesigned when cast in the new alloy...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-662.
Published: 01 March 2001
... properties of bismuth/selenium-containing EnviroBrass alloys are functionally equivalent to those of stan- dard plumbing brasses. Specifically, the ductility of EnviroBrass III is marginally lower than that of leaded yellow brass. Its strength increases and ductility decreases with increasing zinc...
Journal Articles
Alloy Digest (2019) 68 (5): Cu-887.
Published: 01 May 2019
..., plate, profile or structural shape, flats/rectangular bar DOI: 10.31399/asm.ad.cu0887 Applications Typical uses include: Plumbing: faucets, pump components, pipe fittings, plumbing goods, water pump impellers Industrial: housings, small gears Producer Concast Metal Products Co. Wakeman, OH 44889...
Journal Articles
Alloy Digest (1975) 24 (3): Cu-294.
Published: 01 March 1975
... resistance is good to most atmospheres (including marine) and to dry gases, alcohols, petroleum products and saline waters. Alloy No. 330 enjoys a wide range of applications. Forms Available: Pipe and tube. Applications: Plumbing brass goods and accessories. pump and power cylinders and liners. primers...
Journal Articles
Alloy Digest (1978) 27 (3): Cu-349.
Published: 01 March 1978
... and permanent mold. Ingots. Applications: Small gears, pipe fittings, low-pressure valves, fittings for gasoline and oil lines, fireequipment fittings, small pump castings, ornamental fixtures, plumbing goods, general hardware, and general castings requiring fair strength, soundness and excellent machining...
Journal Articles
Alloy Digest (1978) 27 (1): Cu-346.
Published: 01 January 1978
... such applications as plumbing goods, ornaments and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining...
Journal Articles
Alloy Digest (2014) 63 (6): Cu-831.
Published: 01 June 2014
... a weighted average of 0.25% lead when used with respect to the wetted surfaces of pipes, plumbing fittings and fixtures. With this in mind, Alloy C37000 provides a low lead alloy that aids in the compliance to this legislation, while maintaining machinability ratings and forging performance near...
Journal Articles
Alloy Digest (2013) 62 (2): Cu-815.
Published: 01 February 2013
... will be manufactured to the latest revision of the following specifications: ASTM B151 for rod ASTM B124 for forging rod ASTM B466 for seamless pipe and tube Military specifications MIL-C-15726 and MIL-T-16420 Federal specifications Table 1 Mechanical properties Size, mm (in.) Temper Tensile strength, MPa...
Journal Articles
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
... made by the following methods: Sand, cen- trifugal and continuous. Ingots. Applications: Pipe fittings, elbows, tees, couplings, bushings, lock- nuts, plugs, low-pressure valves, small gears, fM- hires, unions, plumbing goods and general hardware. Manufacturers: Copper alloy foundries. ...
Journal Articles
Alloy Digest (2021) 70 (10): Cu-925.
Published: 01 October 2021
...; costume jewelry; Industrial dials; fire extinguisher cases; lipstick containers; Wieland Rolled Products NA (formerly Olin Brass) medallions; nameplates; plaques; rouge boxes; 4801 Olympia Park Plaza, Suite 3500 Other tokens; zippers. Louisville, Kentucky 40241, USA Plumbing Tel: +1 502 873 3000 AC motors...
Journal Articles
Alloy Digest (1973) 22 (12): Al-31.
Published: 01 December 1973
... Available: Sheet. plate, wire, rod, bar, extruded shapes and tube and pipe, drawn tube and pipe, forgingr Clad material also is availabk as sheet, plate and drawn tube and pipe. Applications: Cooking utensils, heat exchangers, pressure and storage tanks, chemical equipment, refiectoa, duct work. truck...