1-20 of 375

Search Results for plastic molds

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... BOFORS BP20-2 is a vacuum-degassed (BOVAC) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat...
Journal Articles
Alloy Digest (2007) 56 (1): TS-640.
Published: 01 January 2007
... Boehler M238 VMR is a hardened and tempered plastic mold steel with excellent cleanliness for best polishability, making it ideal for lens mold tooling. The hardness is consistent over the entire cross section of the steel block, even in large sizes, due to the addition of nickel. This datasheet...
Journal Articles
Alloy Digest (1957) 6 (6): TS-59.
Published: 01 June 1957
... FORMA is a very low carbon carburizing steel recommended for cold hubbing of compression and multi-cavity molds for plastics. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: TS-59...
Journal Articles
Alloy Digest (2012) 61 (2): TS-700.
Published: 01 February 2012
... Formadur 2311 is a plastic mold steel with good polishability. It is comparable to P-20. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on surface qualities as well as heat treating and joining. Filing Code...
Journal Articles
Alloy Digest (2012) 61 (9): TS-707.
Published: 01 September 2012
... Formadur 2312 is a plastic mold steel with good polishability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: TS-707. Producer or source: Schmolz...
Journal Articles
Alloy Digest (2012) 61 (11): TS-710.
Published: 01 November 2012
... Formadur 2316 is a plastic mold steel (modified Type 420) with good polishability. It is used for molds for processing plastics with corrosive reactions. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing...
Journal Articles
Alloy Digest (2015) 64 (2): TS-729.
Published: 01 February 2015
... Boehler M333 Isoplast is a plastic mold steel with low levels of impurities to meet high gloss surfaces at low costs. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating, machining, and joining. Filing Code: TS-729...
Journal Articles
Alloy Digest (2015) 64 (4): TS-730.
Published: 01 April 2015
... Böhler (or Boehler) M461 Extra is a precipitation hardening steel grade for plastic molds with good machinability in the precipitation hardened condition. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on machining. Filing Code...
Journal Articles
Alloy Digest (2015) 64 (12): TS-732.
Published: 01 December 2015
... Böhler (or Boehler) M261 Extra is a precipitation hardening steel grade for plastic molds with good machinability in the precipitation hardened condition. It is used in the processing of plastics by offering high compressive stress and high wear resistance. This datasheet provides information...
Journal Articles
Alloy Digest (2016) 65 (1): TS-733.
Published: 01 January 2016
... Böhler (or Boehler) M268 VMR is a hardened and tempered plastic mold steel with excellent cleanliness for best polishing. This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on forming, heat treating, and joining...
Journal Articles
Alloy Digest (2016) 65 (9): TS-736.
Published: 01 September 2016
... Böhler (or Boehler) M261 Extra is a precipitation hardening steel grade for plastic molds featuring excellent machinability in the solution annealed and aged condition. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information...
Journal Articles
Alloy Digest (2017) 66 (3): SS-1260.
Published: 01 March 2017
.../kg·K (Btu/lb·°F) 460 (0.110) Mechanical Properties: Tensile strength, MPa (ksi) Hardness, 32 HRC 1100 (160) Copyright © 2017, ASM International®. All rights reserved. S-STAR (Plastic Mold Steel) Filing Code: SS-1260 Stainless Steel :: March 2017 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax...
Journal Articles
Alloy Digest (2017) 66 (4): SS-1261.
Published: 01 April 2017
... Superplast is a plastic mold steel with a high chromium content for corrosion resistance and a high sulfur content for good machinability. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1976) 25 (7): TS-305.
Published: 01 July 1976
... MIRROMOLD Filing Code: TS-305 Tool steel JULY 1976 - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbd by Engineering Alloys Digest, Inc Upper Mona& New Jersey MIRROMOLD* (Plastic Mold Steel; AISI Type Pl) MIRROMOLD is a casehardening mold steel designed expressly for cold-hobbed cavities. It is a vanadium...
Journal Articles
Alloy Digest (1976) 25 (8): SS-331.
Published: 01 August 1976
... UHB STAVAX ESR is a high-chromium (13.6%) martensitic stainless plastic-mold steel. It is Electro-Slag Refined (ESR) to provide the best polishability. It is characterized by good hardenability, high hardness, excellent polishability and fair resistance to corrosion. It is used for both injection...
Journal Articles
Alloy Digest (1982) 31 (8): TS-403.
Published: 01 August 1982
... CARPENTER SAMSON EXTRA is a case-hardening alloy mold steel expressly developed to give an excellent combination of easy hobbing, good machinability, and high strength for long runs in the molding of plastics. It is ESR melted which makes it outstanding for its cleanliness; therefore, it has...
Journal Articles
Alloy Digest (1966) 15 (11): TS-185.
Published: 01 November 1966
... Thermold Z is a tool steel quality mold grade expressly designed for maximum production at moderate cost for zinc and other low temperature casting metals; and for injection molded and compression molded plastics. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1969) 18 (7): TS-221.
Published: 01 July 1969
... DURAMOLD N is a low-carbon, nickel-chromium type of plastic-molding die steel capable of developing a deep carburized case combined with exceptional core strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1970) 19 (4): TS-230.
Published: 01 April 1970
... AISI Type P2 is a cold hobbing alloy mold steel exhibiting a combination of ease in hobbing and good core strength. It is recommended for case hardened molds for plastics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1971) 20 (11): TS-238.
Published: 01 November 1971
... THERMOLD P20 is a tool steel designed expressly for molds for zinc and other low-melting casting alloys and for injection and compression molded plastics. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating...