1-20 of 368 Search Results for

plastic mold applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1993) 42 (8): SA-466.
Published: 01 August 1993
... THYSSEN STRIPPER MATERIAL is ideally suited for a stripper material for plastic molding applications of all kinds. It is supplied preheat treated to Rc 38/42 (352-388 BHN), and has a high impact strength with good temper resistance. Hardness loss due to mass effects is very low. This datasheet...
Journal Articles
Alloy Digest (2020) 69 (2): TS-787.
Published: 01 February 2020
... Uddeholm Vidar 1 ESR is a medium-carbon, chromium-molybdenum-vanadium, hot-work tool steel that is produced using the electroslag remelting (ESR) process. Its good toughness in combination with very good polishability and texturing properties makes it a suitable steel in plastic mold applications...
Journal Articles
Alloy Digest (1994) 43 (6): TS-527.
Published: 01 June 1994
... warmth, the cunponent should be tempered immediately. 8. For die casting applications, tempering should be at 1OWF for 1 hour/inch. For plastic molding applications tempering should be at 480┬░F. 9. When cooled in air to room temperature, component should be hardness tested. 10. Plastic molding components...
Journal Articles
Alloy Digest (2005) 54 (4): TS-562.
Published: 01 April 2005
... to conventional S7. Typical applications include plastic injection molds, punches and dies by wire EDM, and heavy impact tools. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well...
Journal Articles
Alloy Digest (2023) 72 (5): SS-1358.
Published: 01 May 2023
... for demanding applications such as molds for medical parts, parts made of corrosive plastics, and parts made of rubber. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2004) 53 (6): Al-390.
Published: 01 June 2004
... Giantal is a wrought aluminum alloy for mold applications such as low-pressure plastic and composite molding, including thermoforming and resin transfer molding that require the material to have excellent corrosion resistance and weldability. The 5xxx aluminum alloys are preferred for this type...
Journal Articles
Alloy Digest (1979) 28 (8): SS-367.
Published: 01 August 1979
... corrosive plastics, and (3) Corrosion problems when molds are used in hot, humid climates. In addition to resisting the above corrosive conditions, users have found that this steel has many other cost-reducing advantages for applications where corrosion is not involved. This datasheet provides information...
Journal Articles
Alloy Digest (2000) 49 (1): SS-774.
Published: 01 January 2000
... steel that may be used for many demanding applications. Its superior resistance to corrosion, com- bined with a hardness of up to 50 HRC, makes it well suited for molds making medical parts, all molds running in a clean-room environment, parts made of corro- sive plastics (such as polyvinyl chloride...
Journal Articles
Alloy Digest (1997) 46 (2): TS-550.
Published: 01 February 1997
... withconsistentmacllinabilityandminimalilltanalstKsses. Lukens A2 is an air&rdenable 1.0% C, 5% Cr-MO-V tool steel with high wear rcsistmw even at high working tempera- and deep-hardening capability. It is popular in a variety of tooling and plastic molding applications including wear insetts. blanking dies, and forming tools. Lukens Df is an air...
Journal Articles
Alloy Digest (2009) 58 (9): TS-683.
Published: 01 September 2009
... FINKL LR, HB, and HI-HARD P-20 are part of a series of mold materials offering a range of properties for various molding applications. The increasing success and popularity of plastic products over the years has led to more sophisticated tooling and constantly evolving resin. These forces have...
Journal Articles
Alloy Digest (2007) 56 (2): SS-987.
Published: 01 February 2007
... in. in thickness with widths from 10-60 in. Bar is available as ground, machined, and peeled for different sizes. Contact the producer. Applications: Holder/mold frames, backing plates, and bolsters for plastic mold tooling; structural components and fixtures that required corrosion resistance; tooling...
Journal Articles
Alloy Digest (1994) 43 (7): TS-528.
Published: 01 July 1994
... . General Characteristics: Thyssen Thyroplast 2798 (AISI P20 Special) is an electric arc melted, vacuum degassed P20 type steel which has been specially created for plastic molding applications of all types. Supplied preheat treated to Rc 28/34 (265-325 BHN). it is capable of providing a lens quality polish...
Journal Articles
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... of chromium and molybdenum. It is used for both cold and hot tooling applications. Its many uses include shear blades, swaging dies, chisels and dies for molding plastics below 1000 F (538 C). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1984) 33 (1): TS-421.
Published: 01 January 1984
... favorable size stability and exceptional secondary hardness characteristics. NAVAHO has a broad application range from shear blades and punches to molds for plastics ad hot-work tooling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... requirements-95,000 psi tensile strength, 90 Rockwell B hardness and 45% IACS electrical conductivity. Potential applications include resistance welding tips, wheels and fixtures. A major use is in plastic injection molding. AMPCO-TRODE 940 is used for repair welding and overlays. This datasheet provides...
Journal Articles
Alloy Digest (1994) 43 (3): TS-524.
Published: 01 March 1994
... polishability. It will meet the Chrysler N.P. 2080 specifications. Thyrotherm 2344 EFS (AK1 H.13) is produced in round bars up to 24 diameter and has the ability to be heat treated to RcW54 for plastic molding. Applications: The Die Casting Industry Thyrotherm 2344 EFS (AISI H.13) can be used in all die cast...
Journal Articles
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... (BOVAC*) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat treated for a number of applications...
Journal Articles
Alloy Digest (1974) 23 (2): SA-301.
Published: 01 February 1974
... CRUCIBLE HOLDER BLOCK is a medium-carbon chromium-molybdenum steel which affords superior machinability because of its sulfur content. It is used in such applications as holders or backers for forging dies and frames for plastic molds. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
...-work applications where machinability is of primary importance. Its many uses include forging and heading dies, aluminum extrusion dies, mandrels and mold dies for plastics. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information...
Journal Articles
Alloy Digest (1989) 38 (4): P-2.
Published: 01 April 1989
.... They are readily molded. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. Filing Code: P-2. Producer or source: The Dow Chemical Company, Dow Plastics. Producer or Source: The Dow Chemical Company, Dow Plastics...