Journal Articles
Alloy Digest (1999) 48 (7): SS-745.
Published: 01 July 1999
... Sumitomo weldable seamless 13Cr-S is a corrosion-resistant line pipe with very low carbon for weldability. The addition of molybdenum to the composition provides resistance to corrosive environments containing small amounts of hydrogen sulfide. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1999) 48 (7): SS-752.
Published: 01 July 1999
... Sumitomo weldable seamless 13Cr-M is a corrosion-resistant oil country tubular goods line pipe product that resists wet hydrocarbon products containing carbon dioxide. Increased weldability is developed by modifying the chemistry to ultralow carbon content. This datasheet provides information...
Journal Articles
Alloy Digest (2006) 55 (1): SS-952.
Published: 01 January 2006
... Sumitomo SM13CR is the basic 13 Cr alloy that has been widely used to handle both CO2 and chlorides in line pipe. See Alloy Digest SS-745, revised July 1999, and SS-752, July 1999, for information on weldable and more corrosion-resistant versions with lower carbon and also molybdenum...
Journal Articles
Alloy Digest (1966) 15 (4): SS-180.
Published: 01 April 1966
... Croloy 16-1 is a stainless steel, available as tubing or pipe, and recommended as a substitute for Type 300 stainless steels for applications where chloride stress-corrosion cracking is a problem. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2016) 65 (3): CS-197.
Published: 01 March 2016
... 2 for L80-13CR. This material is also available with high collapse performance (VM 90 13CRHC). Field Records. Over the past 30 years, the producer has supplied more than 150,000 tons of pipe of API L80-13CR and VM 80 13CR grades to hundreds of operators in most regions of the world for pipe from...
Journal Articles
Alloy Digest (2016) 65 (2): CS-195.
Published: 01 February 2016
... to Sulfide Stress Cracking (SSC). The NACE MR0175/ISO 15156 standard limits the use of L80-13CR steel pipe to a maximum H2S partial pressure of 1.5 psi (0.1 MPa) and pH 3.5. Various industry publications and internal test data showed that SSC resistance of 13Cr steels is widely dependent on other...
Journal Articles
Alloy Digest (2016) 65 (4): CS-198.
Published: 01 April 2016
... TM0177 General Characteristics: VM 85 13Cr is a martensitic OCTG steel (also called 13% Cr steel) for sweet wet CO2 corrosive environments. This alloy offers a minimum yield strength of 586 MPa (85 ksi) to maximize the pipe capacity (burst, tensile, collapse) as well as better toughness, tighter chemical...
Journal Articles
Alloy Digest (2016) 65 (5): CS-199.
Published: 01 May 2016
... is limited to small amounts of H2S and also depends on in-situ pH and chloride. Contact the producer for more SSC and corrosion test data on 13Cr steels. Copyright © 2016, ASM International®. All rights reserved. VALLOUREC VM 95 13Cr (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: CS-199 Carbon...
Journal Articles
Alloy Digest (2016) 65 (7): CS-200.
Published: 01 July 2016
... 13Cr SS (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: CS-200 Carbon Steel :: July 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: MemberServiceCenter@asminternational.org Published by ASM International® :: Data shown are typical...
Journal Articles
Alloy Digest (2016) 65 (8): CS-201.
Published: 01 August 2016
... Country Tubular Goods (OCTG) Line Pipe) Filing Code: CS-201 Carbon Steel :: August 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org :: MemberServiceCenter@asminternational.org Published by ASM International® :: Data shown are typical, not to be used...
Journal Articles
Alloy Digest (2016) 65 (11): SS-1254.
Published: 01 November 2016
... environments. Copyright © 2016, ASM International®. All rights reserved. VALLOUREC VM 125 13Cr SS (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: SS-1254 Stainless Steel :: November 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1195.
Published: 01 January 2015
... Resistance: General Corrosion. Pressurfect has good resistance in: Organic acids at moderate temperatures Salt solutions, e.g., sulfates, sulfides, and sulfites Caustic solutions at moderate temperatures SANDVIK PRESSURFECT (Seamless Pipe and Tubing) Filing Code: SS-1195 Stainless Steel :: January 2015...
Journal Articles
Alloy Digest (2015) 64 (3): CS-185.
Published: 01 March 2015
... from the producer s know-how in manufacturing sour service materials and excellent quality control. This alloy offers a tighter quality control compared to API L80 and is manufactured based on API 5CT / ISO 11960 PSL2 requirements. Product Forms Available: Pipe and tubing with diameters 60 406 mm (2.4...
Journal Articles
Alloy Digest (2015) 64 (4): CS-187.
Published: 01 April 2015
... with temperature. Production Process Description Pipe making Seamless Heat treatment Quenched and tempered Corrosion Resistance: While the increase of temperature minimizes SSC susceptibility as outlined in Fig. 2, SM90XS remains SSC resistant at all temperatures. See Fig. 3 for H2S partial pressure. In addition...
Journal Articles
Alloy Digest (2015) 64 (5): CS-188.
Published: 01 May 2015
... within Regions 1, 2, and 3 of ISO 15156- 2 pH versus H2S partial pressure diagram, that is any combination of ppH2S and temperature under in situ pH occurring in production environments. SUMITOMO SM110XS (Ferritic Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: CS-188 Carbon Steel :: May 2015...
Journal Articles
Alloy Digest (2015) 64 (6): CS-190.
Published: 01 June 2015
... inclusions was achieved through utilizing multicomponent inclusion technology to suppress inclusion growth. Multicomponent inclusion SUMITOMO SM125ES (Ferritic Oil Country Tubular Goods (OGTG) Line Pipe) Filing Code: CS-190 Carbon Steel :: June 2015 Published by ASM International® :: Data shown are typical...
Journal Articles
Alloy Digest (2015) 64 (7): CS-191.
Published: 01 July 2015
... pH/H2S domain diagram. Reference conditions (H2S partial pressure = 0.03 bar and pH = 3.5) used as a QC acceptance criteria for each manufactured SM125S heat are indicated as well. SUMITOMO SM125S (Ferritic Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: CS-191 Carbon Steel :: July 2015...
Journal Articles
Alloy Digest (1991) 40 (4): P-25.
Published: 01 April 1991
... MANGUM ABS FG960 is specifically designed for pipe fittings. MAGNUM ABS (acrylonitrile-butadiene-styrene) FG960 is a virgin, prime grade material, listed by the National Sanitation Foundation (NSF). It is available in black as a factory color mix product (natural resin with black color concentrate...
Journal Articles
Alloy Digest (2019) 68 (8): SS-1308.
Published: 01 August 2019
... corrosion due to high Copyright © 2019, ASM International®. All rights reserved. SANDVIK HIGH-N (Medical Pipe and Tube) Filing Code: SS-1308 Stainless Steel :: August 2019 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.4634 :: www.asminternational.org :: MemberServiceCenter...
Journal Articles
Alloy Digest (2016) 65 (10): SS-1251.
Published: 01 October 2016
... CO2 containing environments. They will suffer from various forms of corrosion such Copyright © 2016, ASM International®. All rights reserved. VALLOUREC VM 110 13Cr SSCY (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: SS-1251 Stainless Steel :: October 2016 Materials Park, Ohio 44073-0002...