1-20 of 163 Search Results for

pipe fittings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1991) 40 (4): P-25.
Published: 01 April 1991
... MANGUM ABS FG960 is specifically designed for pipe fittings. MAGNUM ABS (acrylonitrile-butadiene-styrene) FG960 is a virgin, prime grade material, listed by the National Sanitation Foundation (NSF). It is available in black as a factory color mix product (natural resin with black color concentrate...
Journal Articles
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
.... Typical applications are pipe fittings, bushings, locknuts and unions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-450.
Published: 01 December 1982
... fixtures, general hardware, plumbing goods, small gears and pipe fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2016) 65 (2): CS-195.
Published: 01 February 2016
... Sulfide Stress Cracking (SSC). The NACE MR0175/ISO 15156 standard limits the use of L80-13CR steel pipe to a maximum H2S partial pressure of 1.5 psi (0.1 MPa) and pH 3.5. Various industry publications and internal test data showed that SSC resistance of 13Cr steels is widely dependent on other...
Journal Articles
Alloy Digest (2016) 65 (11): SS-1254.
Published: 01 November 2016
... containing environments. Copyright © 2016, ASM International®. All rights reserved. VALLOUREC VM 125 13Cr SS (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: SS-1254 Stainless Steel :: November 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542 :: www.asminternational.org...
Journal Articles
Alloy Digest (2016) 65 (10): SS-1251.
Published: 01 October 2016
... CO2 containing environments. They will suffer from various forms of corrosion such Copyright © 2016, ASM International®. All rights reserved. VALLOUREC VM 110 13Cr SSCY (Oil Country Tubular Goods (OCTG) Line Pipe) Filing Code: SS-1251 Stainless Steel :: October 2016 Materials Park, Ohio 44073-0002...
Journal Articles
Alloy Digest (2001) 50 (8): Ni-571.
Published: 01 August 2001
... chemical composition corrosion-resistant alloys creep properties ductility high-temperature alloys KUBOTA KHR45A LC physical properties pipe fittings tensile properties tubes thermal properties Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570) that changes either ductility or...
Journal Articles
Alloy Digest (1978) 27 (3): Cu-349.
Published: 01 March 1978
... permanent mold. Ingots. Applications: Small gears, pipe fittings, low-pressure valves, fittings for gasoline and oil lines, fireequipment fittings, small pump castings, ornamental fixtures, plumbing goods, general hardware, and general castings requiring fair strength, soundness and excellent machining...
Journal Articles
Alloy Digest (1985) 34 (9): Al-260.
Published: 01 September 1985
... corrosion-resistant alloys elasticity hardness heat treatability joinability machinability manifolds physical properties pipe fittings tensile properties valves UNS A07070 ALUMINUM 707.0 Filing Code: AI-260 Aluminum Alloy SEPTEMBER 1966 - DATA ON WORLD WIDE METALS AND ALLOYS a Copyrtgh! 1985...
Journal Articles
Alloy Digest (1967) 16 (8): Cu-179.
Published: 01 August 1967
.... Applications: Cold headed and roll threaded bolts, hardware, screws, marine fittings, tanks and piping. Manufacturer: Anaconda American Brass Co. Waterbury, Connecticut ...
Journal Articles
Alloy Digest (1999) 48 (10): Al-360.
Published: 01 October 1999
... superior to all other screw machine alloys, while strength of alloy 6061 is the lowest. Applications: Applications include heavy duty structures requiring good corro- sion resistance, marine applications, truck parts, railroad cars, furniture, and pipe lines. Producer: Tennalum A Division of Kaiser...
Journal Articles
Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... corrosion and stress-corrosion cracking, and (3) Good weldability. It can be hardened and strenghened by cold working and has good hot and cold workability. Forms Availabie: Seamless tube and pipe. fittings. and the following complementary products (by agreement): welding wire, electrodes, strip. wire, bar...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
... Kaiser Alloy 6063 is a magnesium/silicon alloy. One of the most popular of the heat treatable alloy group. Products include extruded and drawn tube, pipe, rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. This datasheet provides...
Journal Articles
Alloy Digest (1981) 30 (10): Cu-424.
Published: 01 October 1981
... dezincification and it is more resistant to stress-cor- rosion cracking than brasses with higher zinc contents. Forms Available: Pipe and tube. Applications: Condenser and heat-exchanger tubes, plumbing pipe and fittings, pump lines and tubing for instrumentation. Manufacturer: Mueller Brass Company Port Huron...
Journal Articles
Alloy Digest (1973) 22 (3): SA-286.
Published: 01 March 1973
... IN-787 is an age-hardenable, high-strength structural steel. It is characterized by low-temperature toughness, good atmospheric corrosion resistance and excellent weldability, even under adverse field conditions such as line-pipe welding. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1975) 24 (3): Co-41.
Published: 01 March 1975
...: United States Pipe and Foundry Company. Originally published January 1965, revised March 1975. Producer or Source: United States Pipe and Foundry Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys creep properties elasticity...
Journal Articles
Alloy Digest (1983) 32 (10): Bi-32.
Published: 01 October 1983
...-shrinkage characteristics make it of great use in industry for such applications as sprinkler and fire safety devices, support for bending pipe and tubing, anchoring aircraft parts for machining, and seals for annealing and nitriding furnaces. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1994) 43 (11): SS-575.
Published: 01 November 1994
... CND 17.12; Sweden SS 2375 pipe Fittings Seamless and welded b-w. ANSI B 16.9; forged S.W. ANSI B16.11; threaded NPT ANSI B16.3 General Characteristics: Sandvik 3R69 is a variant of type 316L and is used predominantly in the urea industry and guarantees a low ferrite content. The characteristics are...
Journal Articles
Alloy Digest (1995) 44 (5): SS-593.
Published: 01 May 1995
... Available: Seamless tube and pipe, seamless and welded pipe fit- tings, forged fittings, threaded fittings, flanges, welding wire, wire electrodes, covered electrodes, forgings and plate. Appiications: Typical urea plant applications of Sandvik Urea Grade iUC: l carbamate condensers, scrubbers, decomposers...
Journal Articles
Alloy Digest (2019) 68 (5): Cu-887.
Published: 01 May 2019
..., plate, profile or structural shape, flats/rectangular bar DOI: 10.31399/asm.ad.cu0887 Applications Typical uses include: Plumbing: faucets, pump components, pipe fittings, plumbing goods, water pump impellers Industrial: housings, small gears Producer Concast Metal Products Co. Wakeman, OH 44889...