Skip Nav Destination
Close Modal
Search Results for
petroleum products
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 263 Search Results for
petroleum products
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1953) 2 (2): SA-7.
Published: 01 February 1953
... SICROMO 7M is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot...
Abstract
View article
PDF
SICROMO 7M is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot petroleum products and when a greater load-carrying ability is desired. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-7. Producer or source: Timken Roller Bearing Company.
Journal Articles
Alloy Digest (1955) 4 (3): SA-28.
Published: 01 March 1955
... SICROMO 7 is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot...
Abstract
View article
PDF
SICROMO 7 is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot petroleum products and when a greater load-carrying ability is desired. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-28. Producer or source: Timken Roller Bearing Company.
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production...
Abstract
View article
PDF
NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production and refinery equipment and marine equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-312. Producer or source: Vereingte Deutsche Metallwerke AG.
Journal Articles
Alloy Digest (1971) 20 (10): Pb-8.
Published: 01 October 1971
.... Tin is included in the composition to make the alloy resistant to humid air. Ahoy 5B is resistant to acetone. milk, mineral oils, motor fuels and petroleum products, and sea water. It is subject to moderate general attack by ammonium sulfate, photographic solutions, potassium and sodium chlorides...
Abstract
View article
PDF
LEAD-BASE SOLDER comprises a family of alloys, usually lead-tin alloys, with or without the addition of antimony, although there are other types including those containing silver. They are widely used in industrial applications. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance. Filing Code: Pb-8. Producer or source: Most lead producers.
Journal Articles
Alloy Digest (1985) 34 (4): Cu-496.
Published: 01 April 1985
... to attack by industrial, rural and marine atmospheres, saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides and ammonium compounds. Specification Equivalents: ASTM: B 121 and B 453. General Characteristics: Copper Alloy...
Abstract
View article
PDF
Copper Alloy No. C33500 is a brass containing 0.5% lead. It is used where moderate cold working and/or some machining is required. It possesses fair capacity for welding. It is used in a wide variety of hardware items. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-496. Producer or source: Brass mills.
Journal Articles
Alloy Digest (1986) 35 (11): Cu-517.
Published: 01 November 1986
.... It withstands attack from dry gases. fresh and seawater, petroleum products. organic solvents and sulfides. Prolonged contact with oxidizing acids. mercury compounds. moist ammonia. cyanides and strong bases should be avoided. Specification Equivalents: MILITARY MIL-T-46072. UNS No. C33100. SAE: 3461 (CA 331...
Abstract
View article
PDF
Copper Alloy No. C33100 is a free-cutting tube brass. It has a good combination of mechanical properties. It has excellent solderability and good brazeability. Its uses include general-purpose screw-machine products, pump and power cylinders, plumbing accessories and primers in the munitions industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-517. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1986) 35 (7): Cu-513.
Published: 01 July 1986
... and seawater. petroleum products. organic solvents and sulphides. Prolonged contact with oxidizing acids. mercury compounds. moist ammonia. cyanides and strong bases should be avoided. Specification Equivalents: A MS 4558. ASTM B 135 (332). Military: MIL-T-46072. UNS No.C33200. CDA Copper Alloy No. C33200...
Abstract
View article
PDF
Copper Alloy No. C33200 is a free-machining brass containing nominally 1.6% lead. Its machinability rating is 80% of that of Free-Cutting Brass. It has good resistance to corrosion in many environments. Alloy No. C33200 is used widely for general-purpose screw-machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-513. Producer or source: Brass mills.
Journal Articles
Alloy Digest (1980) 29 (4): Cu-393.
Published: 01 April 1980
... and seam resistance welding. Corrosion Resistance: Mueller alloy 3470 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water and seawater, petroleum products, organic solvents and sulfides. Prolonged contact with oxidizing acids...
Abstract
View article
PDF
MUELLER Alloy 3470 (formerly MBCo. Alloy 312) is a wrought medium-leaded brass alloy intended for screw-machine applications where excellent thread-rolling, knurling and cold-forming properties are required. It is characterized by an excellent combination of free-machining and cold-working properties. Typical applications include valve stems, threaded connectors and flare fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-393. Producer or source: Mueller Brass Company.
Journal Articles
Alloy Digest (1981) 30 (11): SS-395.
Published: 01 November 1981
... be used. Corrosion and Scaling Resistance: Carpenter Stainless Type 405 has corrosion resistance similar to Type 410. It will resist corrosion from mild atmospheres, fresh water, steam, ammonia, many petroleum products and organic materials, and several mild acid environments. For best results...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 405 is a 12% chromium stainless steel that does not harden appreciably. It was designed to allow its use in the as-welded condition. It is particularly desirable for welded applications which require finish machining. It has moderate tensile strength (70,000 psi) in the fully annealed condition and resists corrosion in mild environments. It is used for parts and structures that cannot be annealed after welding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-395. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1981) 30 (1): Cu-409.
Published: 01 January 1981
.... The lead content prevents successful welding. Corrosion Resistance: Anaconda Alloy 330 has good resistance to attack by industrial, rural, and marine atmospheres, saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides...
Abstract
View article
PDF
ANACONDA Alloy 330 is a low-leaded yellow brass that is produced only in tube form. It is both machinable and formable and it makes a utility tube that is suitable for a wide range of applications where corrosive conditions are not severe. Its uses include pump and power cylinders and liners, plumbing goods and munitions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-409. Producer or source: Anaconda American Brass Company.
Journal Articles
Alloy Digest (1979) 28 (9): Cu-379.
Published: 01 September 1979
...: Mueller alloy 3406 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water, seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury com- pounds, moist ammonia, cyanides...
Abstract
View article
PDF
MUELLER Alloy 3406 (formerly MBCo. Alloy 314) is a medium-leaded brass alloy intended for screw-machine applications where excellent thread-rolling, knurling and cold-forming properties are required. It is characterized by an excellent combination of cold-working and free-machining properties. Among its many applications are valve stems, gears, rivets and threaded connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-379. Producer or source: Mueller Brass Company.
Journal Articles
Alloy Digest (1980) 29 (7): Cu-398.
Published: 01 July 1980
.... It withstands attack from dry gases, fresh and sea- water, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM B 453, Copper Alloy 353. Federal QQ-B-626. UNS...
Abstract
View article
PDF
MUELLER Alloy 3530 (formerly MBCo. Alloy 254) is a high-leaded brass noted for its excellent thread-rolling and knurling properties; it has a machinability rating approaching that of free-cutting brass. Typical applications include adapters, gears and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-398. Producer or source: Mueller Brass Company.
Journal Articles
Alloy Digest (1981) 30 (4): Cu-415.
Published: 01 April 1981
... and marine atmospheres. It withstands attack from dry gases, fresh water, sea- water, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM: B 121 and B453...
Abstract
View article
PDF
Copper Alloy No. C34000 is a medium-leaded brass characterized by an excellent combination of free-machining and cold-working properties. It is intended for screw-machine applications where excellent thread-rolling, knurling, machining and cold-forming properties are required. Among its many applications are gears, nuts, rivets, screws and threaded connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-415. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1982) 31 (3): Cu-433.
Published: 01 March 1982
..., rural and marine atmo- sheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM: B 121...
Abstract
View article
PDF
Copper Alloy No. C35300 is a high-leaded brass (nominally 1.8% lead) that is noted for its excellent thread-rolling and knurling properties. It has a machinability rating approaching that of Free-Cutting Brass (Copper Alloy No. C36000). It is used in many screw-machine applications and has good resistance to corrosion in numerous environments. Among its many applications are clock and watch parts, wheels, gears and couplings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-433. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1987) 36 (6): Cu-524.
Published: 01 June 1987
... are not recommended. Corrosion Resistance: Copper Alloy No. C36500 has good resistance to attack by industrial, rural and marine atmospheres, fresh and saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides and ammonium compounds...
Abstract
View article
PDF
Copper Alloy No. C36500 is uninhibited leaded Muntz metal containing nominally 0.5% lead to provide fairly good machinability. It has moderate strength; the tensile strength of hot-rolled 1-inch thick plate is 54,000 psi (372 MPa). It has good resistance to corrosin in both fresh and salt water but is subject to dezincification. It is used for condensers and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-524. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1975) 24 (3): Cu-294.
Published: 01 March 1975
.... Coated-metal arc welding and seam resistance welding are not recommended. Corrosion Resistance: Copper Alloy No. 330 has good resistance to attack by industrial. rural. and marine atmospheres. saline waters. petroleum products. alcoliols. and dry gases. It lias fair resistance to corrosion by weak acids...
Abstract
View article
PDF
Copper Alloy No. 330 is a brass containing nominally 0.5% lead. It has good machinability, excellent cold-working properties, and a wide range of uses including general purposes, industrial applications, munitions and plumbing. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-294. Producer or source: Brass mills.
Journal Articles
Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
... this job. The soldering alloys, brazing alloys and fluxes are conventional products available through regular sources. Corrosion Resistance: Belmont ahoy 4582 has good resistance to industrial, rural and marine atmospheres, petroleum products, alcohols, dry gases and sea water. It has fairly good...
Abstract
View article
PDF
BELMONT Alloy 4582 is a alloy developed to meet the special needs of jewelers for a base-metal alloy suitable for casting centrifugally in refractory molds. It can be joined readily to itself and other alloys by soldering or brazing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-353. Producer or source: Belmont Metals Inc..
Journal Articles
Alloy Digest (1985) 34 (1): Cu-490.
Published: 01 January 1985
...: Copper Alloy No. C92800 has high resistance to many corrosive environments. It resists corrosion by petroleum products (hence its use for piston rings), many industrial chemicals, brackish waters, hydraulic fluids and most rural, industrial and marine atmospheres. Avoid prolonged contact with mercury...
Abstract
View article
PDF
Copper Alloy No. C92800 is a cast bronze containing nominally 16% tin and 5% lead. Former commercial names (not recommended) are (1) 295, (2) Leaded Tin Bronze, (3) Ring Metal and (4) 79-16-5-0. It has excellent machinability, moderate strength and good resistance to corrosion. A typical use is piston rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-490. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... excellent resistance to corrosion by most industrial, rural and marine atmospheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should...
Abstract
View article
PDF
Copper Alloy No. C34200 contains nominally 2% lead and has a machinability rating approaching that of Free-Cutting Brass. It is noted for its excellent thread-rolling and knurling properties. It is used for many screw-machine applications and it has good resistance to corrosion in many environments. Its many applications include channel plate, gears, wheels and components for clocks and watches. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-476. Producer or source: Brass mills.
Journal Articles
Alloy Digest (1980) 29 (7): SS-275.
Published: 01 July 1980
... for cold upsetting. Welding: Carpenter Stainless No. 5-F is not recommended for welding. Corrosion Resistance: Carpenter Stainless No. 5-F is suggested to resist corro- sion from mild atmospheres, fresh water, steam, am- monia, many petroleum products and organic materials, and several mild acid...
Abstract
View article
PDF
CARPENTER STAINLESS No. 5-F is a modification of AISI Type 416 stainless steel and was designed for an optimum combination of machinability and corrosion resistance. It comprises a specially balanced analysis and is essentially non-hardenable. It is recommended for all screw-machine applications, particularly those involving intricate machining operations or where superior finishes are required as-machined. Its uses include valve trim, carburetor needles and many other screw-machine parts. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-275. Producer or source: Carpenter. Originally published July 1972, revised July 1980.