Alloy Digest (1953) 2 (2): SA-7.
Published: 01 February 1953
... SICROMO 7M is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot...
Journal Articles
Alloy Digest (1955) 4 (3): SA-28.
Published: 01 March 1955
... SICROMO 7 is a low carbon, 7% chromium alloy steel possessing high temperature properties and high resistance to attack by hot petroleum products. It is suggested as a substitute for the 5% chromium type steels for those applications in which a greater resistance is required to corrosion by hot...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production...
Journal Articles
Alloy Digest (1971) 20 (10): Pb-8.
Published: 01 October 1971
.... Tin is included in the composition to make the alloy resistant to humid air. Ahoy 5B is resistant to acetone. milk, mineral oils, motor fuels and petroleum products, and sea water. It is subject to moderate general attack by ammonium sulfate, photographic solutions, potassium and sodium chlorides...
Journal Articles
Alloy Digest (1985) 34 (4): Cu-496.
Published: 01 April 1985
... to attack by industrial, rural and marine atmospheres, saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides and ammonium compounds. Specification Equivalents: ASTM: B 121 and B 453. General Characteristics: Copper Alloy...
Journal Articles
Alloy Digest (1986) 35 (11): Cu-517.
Published: 01 November 1986
.... It withstands attack from dry gases. fresh and seawater, petroleum products. organic solvents and sulfides. Prolonged contact with oxidizing acids. mercury compounds. moist ammonia. cyanides and strong bases should be avoided. Specification Equivalents: MILITARY MIL-T-46072. UNS No. C33100. SAE: 3461 (CA 331...
Journal Articles
Alloy Digest (1986) 35 (7): Cu-513.
Published: 01 July 1986
... and seawater. petroleum products. organic solvents and sulphides. Prolonged contact with oxidizing acids. mercury compounds. moist ammonia. cyanides and strong bases should be avoided. Specification Equivalents: A MS 4558. ASTM B 135 (332). Military: MIL-T-46072. UNS No.C33200. CDA Copper Alloy No. C33200...
Journal Articles
Alloy Digest (1980) 29 (4): Cu-393.
Published: 01 April 1980
... and seam resistance welding. Corrosion Resistance: Mueller alloy 3470 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water and seawater, petroleum products, organic solvents and sulfides. Prolonged contact with oxidizing acids...
Journal Articles
Alloy Digest (1981) 30 (11): SS-395.
Published: 01 November 1981
... be used. Corrosion and Scaling Resistance: Carpenter Stainless Type 405 has corrosion resistance similar to Type 410. It will resist corrosion from mild atmospheres, fresh water, steam, ammonia, many petroleum products and organic materials, and several mild acid environments. For best results...
Journal Articles
Alloy Digest (1981) 30 (1): Cu-409.
Published: 01 January 1981
.... The lead content prevents successful welding. Corrosion Resistance: Anaconda Alloy 330 has good resistance to attack by industrial, rural, and marine atmospheres, saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-379.
Published: 01 September 1979
...: Mueller alloy 3406 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water, seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury com- pounds, moist ammonia, cyanides...
Journal Articles
Alloy Digest (1980) 29 (7): Cu-398.
Published: 01 July 1980
.... It withstands attack from dry gases, fresh and sea- water, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM B 453, Copper Alloy 353. Federal QQ-B-626. UNS...
Journal Articles
Alloy Digest (1982) 31 (3): Cu-433.
Published: 01 March 1982
..., rural and marine atmo- sheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM: B 121...
Journal Articles
Alloy Digest (1981) 30 (4): Cu-415.
Published: 01 April 1981
... and marine atmospheres. It withstands attack from dry gases, fresh water, sea- water, petroleum products, organic solvents and sul- phides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should be avoided. Specification Equivalents: ASTM: B 121 and B453...
Journal Articles
Alloy Digest (1975) 24 (3): Cu-294.
Published: 01 March 1975
.... Coated-metal arc welding and seam resistance welding are not recommended. Corrosion Resistance: Copper Alloy No. 330 has good resistance to attack by industrial. rural. and marine atmospheres. saline waters. petroleum products. alcoliols. and dry gases. It lias fair resistance to corrosion by weak acids...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
... this job. The soldering alloys, brazing alloys and fluxes are conventional products available through regular sources. Corrosion Resistance: Belmont ahoy 4582 has good resistance to industrial, rural and marine atmospheres, petroleum products, alcohols, dry gases and sea water. It has fairly good...
Journal Articles
Alloy Digest (1985) 34 (1): Cu-490.
Published: 01 January 1985
...: Copper Alloy No. C92800 has high resistance to many corrosive environments. It resists corrosion by petroleum products (hence its use for piston rings), many industrial chemicals, brackish waters, hydraulic fluids and most rural, industrial and marine atmospheres. Avoid prolonged contact with mercury...
Journal Articles
Alloy Digest (1987) 36 (6): Cu-524.
Published: 01 June 1987
... are not recommended. Corrosion Resistance: Copper Alloy No. C36500 has good resistance to attack by industrial, rural and marine atmospheres, fresh and saline waters, petroleum products, alcohols, and dry gases. It has fair resistance to corrosion by weak acids and poor resistance to cyanides and ammonium compounds...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... excellent resistance to corrosion by most industrial, rural and marine atmospheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should...
Journal Articles
Alloy Digest (1981) 30 (11): Cu-425.
Published: 01 November 1981
... excellent solderabllity is of great importance in its use for plumbing goods and plumbing accessories. Corrosion Resistance: Mueller alloy 3300 has good resistance to attack by industrial, rural, and marine atmospheres, saline waters, petroleum products, alcohols, and dry gases. It has fair resistance...