Alloy Digest (1962) 11 (12): Ni-77.
Published: 01 December 1962
... RAonel 600 is a corrosion and heat resisting nickel-base alloy having a combination of high strength and oxidation resistance along with hot and cold workability. It is recommended for component parts in the aircraft, chemical, petroleum and paper pulp industries. This datasheet provides...
Journal Articles
Alloy Digest (1954) 3 (12): SS-22.
Published: 01 December 1954
... USS 5, Type 501, and 5S, Type 502, contain approximately 5% chromium and 0.50% molybdenum. They resist corrosion and oxidation at elevated temperatures and are particularly adaptable to applications in the petroleum refinery industry. Type 502 contains slightly lower carbon and is used...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
.... This alloy has been used in condensers and heat exchangers for the processing of fatty acids, dye-stuffs, pure oils, pectin. citrus juices, milk products, and in pharmaceuticals where product purity is essential such as penicillin and streptomycin fermentation. Petroleum and Chemical Industry: Nickel AUoy...
Journal Articles
Alloy Digest (1982) 31 (6): SS-410.
Published: 01 June 1982
... for highly stressed components in the 1800-2000 F temperature range. It is used in the aircraft, automotive, petroleum, petrochemical and power industries for a wide range of components and parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1975) 24 (12): SS-322.
Published: 01 December 1975
... ductility at all temperatures. The iron content enhances resistance to sulfur attack and internal oxidation. The excellent resistance to sulfur attack makes this Ferro-Tic material an ideal candidate for petroleum industry applications. It can be machined in the solution-annealed condition...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... to elevated temperature sul- fide corrosion, Type 430 is widely used in feed effluent ex- changers in petroleum industry hydrodesulfurizer systems at temperatures up to 700°F (371 C). Other petroleum industry applications include reboilers for desulfurized naphtha. heat exchangers in sour water strippers...
Journal Articles
Alloy Digest (2001) 50 (5): Ni-566.
Published: 01 May 2001
... of UCI-472, HP Nb W Product Forms Available: Castings Applications: This alloy is used in the petrochemical and petroleum industries for applications such as radiant tubes, steam cracking tubes and fittings, refining tubes, and ethylene pyrolysis tubing. Producer: Ultra-Cast, Inc. P.O. Box 28, 401...
Journal Articles
Alloy Digest (2001) 50 (3): Ni-562.
Published: 01 March 2001
... SS-714) for steam cracking tubes and fittings. This alloy is weldable by commonly used procedures us- ing electrodes with a composition matching the base metal or as described in the welding section. Product Forms Available: Castings Applications: This alloy is used in the petrochemical and petroleum...
Journal Articles
Alloy Digest (1997) 46 (11): Ni-530.
Published: 01 November 1997
... Applications: This alloy is used in the petrochemical and petroleum industries for applications such as radiant tube& steam sacking tubes and fittings. reihing tubes, and ethylene pyrolysis tubing. Producer: ukla-casf Inc. P-0. Box 28 Pall. IN 46970 (800) 442-0288 (317) 472-3951 (317) 4724771 (fax) ISSN...
Journal Articles
Alloy Digest (2017) 66 (12): SS-1272.
Published: 01 December 2017
... industries: burner tips, rings, segments, and components for rotary and lepol kilns Mechanical engineering: grid bars, valves and spindles, stirrer arms and teeth, sheath tubes for thermocouples, fittings, drums, bolts, nuts, rivets Petroleum industry: tubes and tubular components Producer: In Austria...
Journal Articles
Alloy Digest (1957) 6 (3): Cu-48.
Published: 01 March 1957
...- tially a brazed and not a fusion joint. The bond is excellent, however, and the strength obtained is entirely satisfactory. Corrosion Resistance: Good resistance to industrial, rural and marine at- mospheres. petroleum products, alcohols, dry gases and sea water. Fairly good resistance to we& bases. Gen...
Journal Articles
Alloy Digest (1988) 37 (7): CI-55.
Published: 01 July 1988
.... alkalies and petroleum industry environments. Specification Equivalents: ASTM A43&72a. UNS No. F4lOOO(Type CRI); F4lOOl(Type CRiB);F4IOO2(Type CR2); F41003(Type CR2B); F41004(Type CR3); F41005(Type CR4); F41006(Type CRS). General Characteristics: The more highly alloyed Meehanite types have an austenitic...
Journal Articles
Alloy Digest (1998) 47 (4): SS-714.
Published: 01 April 1998
... is at least twice as long. The HP Mod alloys also offer good ductility and weldability. Field repairs by welding can be accomplished after a re-solution anneal to restore much of the elongation. Forms Available: castings Applications This ahoy is used in the petrochemical and petroleum industries...
Journal Articles
Alloy Digest (2017) 66 (10): SS-1270.
Published: 01 October 2017
..., bolts, nuts, rivets Petroleum industry: tubes and tubular components Producer: In Austria: Bohler Edelstahl GmbH A-8605 Kapfenberg, Austria Tel: +43-3862/20-7181 Fax: +43-3862/20-7576 www.bohler-edelstahl.at ISSN: 002-614X SS-1270B Table 1 Long time high-temperature properties condition: quenched 1...
Journal Articles
Alloy Digest (2017) 66 (11): SS-1271.
Published: 01 November 2017
..., enamel, cement, and ceramic industries: burner tips, rings, segments, and components for rotary and lepol kilns Mechanical engineering: grid bars, valves and spindles, stirrer arms and teeth, sheath tubes for thermocouples, fittings, drums, bolts, nuts, rivets Petroleum industry: tubes and tubular...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... mesh (63 m) + 15 m Applications: Coatings of Colmonoy 63HV are used for hard surfacing petroleum industry components such as gate valves, pump sleeves, pump shafts, bushings, wear rings, and compressor rods; they can also be used to restore dimensions. Coatings of Colmonoy 63HV are also used...
Journal Articles
Alloy Digest (2020) 69 (5): SS-1317.
Published: 01 May 2020
... Type 304 exhibits excellent resistance to corrosive environments such as those found in chemical, textile, and petroleum industries. Type 304 is suitable for use in the food and dairy industries and excels in rural and industrial atmospheric exposure. Oxidation Resistance The maximum temperature...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1324.
Published: 01 August 2020
... environments such as those found in chemical, textile, and petroleum industries. It is also used in the food and dairy industries, and excels in rural and industrial atmospheric exposure. By reducing the carbon content in Type 304L, welding operations will not cause carbide precipitation that can lead...
Journal Articles
Alloy Digest (1974) 23 (9): Co-71.
Published: 01 September 1974
...). It has proved highly effective in a number of applications, notably on expeller collars used in a@culture, meat and bone processing, and soap processing, as well as on hotoil pump sleeves in the petroleum industry. Wallex No. 50 aUoy is highly resistant to oxidation. When heated in air, it begins...
Journal Articles
Alloy Digest (1976) 25 (10): Co-74.
Published: 01 October 1976
... Data Sheet No. T-29 for corrosion-resistance information). It has proved highly effective in a number of applications, notably on expeller collars used in agriculture, meat and bone processing, and soap processing, as weU as on hot-oil pump sleeves in the petroleum industry. Wallex No. 40 alloy...