Journal Articles
Alloy Digest (1996) 45 (1): SS-629.
Published: 01 January 1996
... Märker G-4849 is a 18Cr-38Ni heat resistant alloy casting for the petrochemical plants. Applications include pyrolysis furnaces and furnace headers. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1995) 44 (9): Ni-485.
Published: 01 September 1995
...-procedures. No preheat or heat treatment. The fUer metal should be equivalent to basis material or ilighex alloyed. General Characteristks: MAERKER ET5ON is a nickel-base high tempemture carrosion resistant grade used in petrochemical plants, power plants, and ship boilers as tubes, hangers, supports, etc...
Journal Articles
Alloy Digest (1995) 44 (10): SS-617.
Published: 01 October 1995
... 29 Figure 2 - Creep rupture strength for cast material-hberker G-4848 mod. Weldability: Applications: Marker G-4848 can be welded by all electric procedures. Pressurized parts in petrochemical plants for tempera- This includes gas tungsten arc, plasma arc, and manual tures in the range of 1472-1922 F...
Journal Articles
Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
... in air-pollution control systems, pulp and paper plants, and chemical and petrochemical processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2012) 61 (8): Cu-810.
Published: 01 August 2012
.... Applications: This alloy is widely used in marine applications, seawater piping, desalination plants, power plants, and in condensers and evaporators in petrochemical plants. The alloy was originally developed as a cost-effective alternative to higher nickel alloys such as Electralloy s EC71500. The addition...
Journal Articles
Alloy Digest (2009) 58 (10): SS-1045.
Published: 01 October 2009
... International, Materials Park, OH 44073-0002, 440-338-5151 CustomerService@asminternational.org Fax 440-338-4634 www.asminternational.org AMINOX® AS-1 DOI: 10.31399/asm.ad.ss1045 Applications: Typical applications include the following: Components/equipment in oil and gas Chemical/petrochemical plant...
Journal Articles
Alloy Digest (2003) 52 (4): Ni-606.
Published: 01 April 2003
... 2.5 25 2.4 2.5 25 3.2 2.5 DOI: 10.31399/asm.ad.ni0606 Applications: This consumable is used for welding the alloys mentioned previ- ously and other similar heat-resistant grades to themselves for use in furnace equipment and petrochemical plants up to about 900 °C (1650 °F). In addition...
Journal Articles
Alloy Digest (2013) 62 (5): SS-1146.
Published: 01 May 2013
... corrosion and to stress corrosion cracking. Product Forms Available: This product is supplied in sheet and strip forms. Applications: Sulfuric acid plants, various types of chemical and petrochemical plants. Producer: Nippon Yakin Kogyo Co., Ltd. 1-5-8, Kyobashi, Chuo-ku, Tokyo 104-8365, Japan Tel: + 81-3...
Journal Articles
Alloy Digest (2007) 56 (8): SS-995.
Published: 01 August 2007
... include pumps and valves, corrosion/ wear-resistant parts, and process equipment for use in offshore oil and gas industries, pulp, paper and textile industries, and chemical and petrochemical plants. Producer: Metrode Products Ltd. Hanworth Lane, Chertsey Surrey, KT16 9LL United Kingdom +44 1932 566 721...
Journal Articles
Alloy Digest (2003) 52 (3): Ni-603.
Published: 01 March 2003
...: These consumables are used for welding the above-noted alloys and similar heat-resistant grades to themselves for use in fur- nace equipment and petrochemical plants up to about 900 °C (1652 °F). They are also suitable for dissimilar combinations of the above alloys and others such as NiCu alloy 400 and alloy 825...
Journal Articles
Alloy Digest (2011) 60 (2): Co-121.
Published: 01 February 2011
... and Praxair D-Gun LW-1N40 in many industries, e.g. in chemical and petrochemical plants on mechanical seal faces, gate valves, oil well drill bearings and pump casings, impellors, plungers and sleeves. They are also used on compressor shafts and feeds screws, In the aerospace industry, Jet Kote 117 protects...
Journal Articles
Alloy Digest (1995) 44 (3): SS-586.
Published: 01 March 1995
... PARALLOY CR39W is an austenitic heat resisting alloy with a combination of creep strength, carburization resistance and ductility. The alloy can be cast for fittings and centrifugally cast for tubing. Typical applications are within the petrochemical furnace arena. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (9): SS-654.
Published: 01 September 1996
... Wiscalloy 25-35Nb is a high-temperature cast heat-resistant stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1975) 24 (12): SS-321.
Published: 01 December 1975
... tubes, furnace containers for annealing. etc.. utility power plants, lead pots. thermowells. anchor bolts, combustion chambers and space heaters. retorts, and petrochemical equipment. Manufacturer: Rolled Alloys, Inc. Detroit, hlichigan 482 1 I. ...
Journal Articles
Alloy Digest (1988) 37 (4): Ni-330.
Published: 01 April 1988
... JESSOP JS Alloy 276 is a nickel-chromium alloy with high molybdenum and moderate tungsten but low iron and silicon contents. This composition provides superior corrosion resistance to a wide variety of environments. It has found wide acceptance in the chemical and petrochemical process industry...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... also has many applications in both the petrochemical and chemical area. Type 430 has moderate strength and good ductility. It can be cold worked readily for producing trim and can be joined successfully by several methods. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1970) 19 (12): SS-248.
Published: 01 December 1970
... and pickled. Applications: Superheater tubes in power generating plants; waste-gas-fired boilers, and high-pressure hydrocarbon crackers in the petrochemical industry. Manufacturer: The Sandvik Steel Works Sandviken, Sweden. In USA: Sandvik Steel Inc. Fair Lawn, New Jersey 074 10. ...
Journal Articles
Alloy Digest (2018) 67 (12): Ni-747.
Published: 01 December 2018
... Alloy 2120 MoN has a wide range of applications in the chemical, petrochemical, and pharmaceutical industries, as well as in energy production and environmental technologies. This alloy is also referred to as Nicrofer 5821 hMoN. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1995) 44 (11): SS-622.
Published: 01 November 1995
... in desulfurization and hydrotreating plants. In the petrochemical industry the steel is used in cracking furnaces for the production of ethylene and vinyl chloride. It is also frequently used for heat exchangers and piping in the chemical and petrochemical industries. Producer: AB Sandvik Steel Sandviken. Sweden +46...
Journal Articles
Alloy Digest (1997) 46 (11): SS-699.
Published: 01 November 1997
... coupled with good hot-strength make Sandvik a suitable material for applications such as tubes in heating furnaces and heat exchangers in desuhi&ation and hydroh%ing plants. In the petrochemical industry the steel is used in cracking furnaces for the production of ethylene and vinyl chloride. It is also...