Skip Nav Destination
Close Modal
Search Results for
petrochemical applications
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 208 Search Results for
petrochemical applications
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
.... This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides information...
Abstract
View article
PDF
Cabot ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness. This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides information on composition, physical properties, and elasticity as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-358. Producer or source: Cabot Corporation, Machinery Division.
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... and toughness. This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides...
Abstract
View article
PDF
INGERSOLL-RAND ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness. This steel is capable of developing a minimum yield strength of 140,000 psi with an optimum combination of hardenability, temperability, weldability, formability, toughness and fatigue properties. It meets many special requirements for petrochemical applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-393. Producer or source: Ingersoll-Rand Oilfield Products Company.
Journal Articles
Alloy Digest (1993) 42 (12): SS-559.
Published: 01 December 1993
... INCOLOY alloy 803 is a high-temperature corrosion-resistant, nickel-iron-chromium alloy, developed by Inco Alloys International for pyrolysis in high-severity ethylene furnaces, and for other petrochemical applications where high levels of oxidation-, carburization-, and/or sulfidation-resistance...
Abstract
View article
PDF
INCOLOY alloy 803 is a high-temperature corrosion-resistant, nickel-iron-chromium alloy, developed by Inco Alloys International for pyrolysis in high-severity ethylene furnaces, and for other petrochemical applications where high levels of oxidation-, carburization-, and/or sulfidation-resistance are important. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as joining. Filing Code: SS-559. Producer or source: Inco Alloys International Inc.
Journal Articles
Alloy Digest (1996) 45 (5): Ni-512.
Published: 01 May 1996
... Märker G 4857W is a cast alloy for petrochemical applications such as furnace tubes. It compares favorably to the HP Modified grades. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-512...
Abstract
View article
PDF
Märker G 4857W is a cast alloy for petrochemical applications such as furnace tubes. It compares favorably to the HP Modified grades. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-512. Producer or source: Schmidt & Clemens Edelstahlwerke.
Journal Articles
Alloy Digest (1996) 45 (8): SS-650.
Published: 01 August 1996
... Uranus 800 is employed at temperatures above 600 deg C (1112 deg F). This austenitic alloy offers good oxidation and creep resistance and is used frequently in petrochemical applications such as for reformers and ethylene crackers. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Uranus 800 is employed at temperatures above 600 deg C (1112 deg F). This austenitic alloy offers good oxidation and creep resistance and is used frequently in petrochemical applications such as for reformers and ethylene crackers. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-650. Producer or source: Creusot-Marrel.
Journal Articles
Alloy Digest (1997) 46 (11): SS-702.
Published: 01 November 1997
... ALLOY 00Cr18Ni5Mo3Si2 is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, these duplex stainless steels have substituted for austenitic stainless steels in many...
Abstract
View article
PDF
ALLOY 00Cr18Ni5Mo3Si2 is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, these duplex stainless steels have substituted for austenitic stainless steels in many types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-702. Producer or source: Central Iron & Steel Research Institute.
Journal Articles
Alloy Digest (1997) 46 (12): SS-704.
Published: 01 December 1997
... ALLOY 00Cr22Ni5Mo3N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves...
Abstract
View article
PDF
ALLOY 00Cr22Ni5Mo3N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance, and corrosion resistance. Filing Code: SS-704. Producer or source: Central Iron & Steel Research Institute.
Journal Articles
Alloy Digest (1998) 47 (2): SS-706.
Published: 01 February 1998
... ALLOY 0Cr25Ni6Mo3CuN is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves...
Abstract
View article
PDF
ALLOY 0Cr25Ni6Mo3CuN is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS-706. Producer or source: Central Iron & Steel Research Institute.
Journal Articles
Alloy Digest (1998) 47 (4): SS-714.
Published: 01 April 1998
... properties heat treatability high-temperature alloys joinability machinability petrochemical applications physical properties stainless steel tensile properties thermal properties - D/GEST d DATA ON WORLD WIDE METALS AND ALLOYS Published bjc ASM Inemaknal Malerlak piuk. all0 44773-ml2 alT-33&5151...
Abstract
View article
PDF
UCI-193 is an HP + Nb grade material for use in the petrochemical arena. The HP + Nb grade resists carburization, oxidation, and creep up to 1093 C (2000 F). This improvement over the HP grade, UCI-190 (Alloy Digest SS-689, July 1997), is due to the addition of niobium. UCI-190 has been used for many years for consistent and predictable results in high temperature applications. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-714. Producer or source: Ultra-Cast Inc.
Journal Articles
Alloy Digest (1984) 33 (11): SS-454.
Published: 01 November 1984
... chemical composition corrosion-resistant alloys creep properties CROLOY 800 elasticity food processing applications heat treatability heat treating equipment joinability machinability oxidation resistance petrochemical applications physical properties steam generators superheaters tensile...
Abstract
View article
PDF
CROLOY 800 is an austenitic stainless steel intended for high-temperature service. In addition to its excellent resistance to corrosion in various media, it exhibits excellent strength and resistance to oxidation at elevated temperatures. Among its many applications are high-temperature processing of hydrocarbons in refinery or petrochemical services, superheater and reheater tubin8g, nuclear reactor steam generators, heat-treating equipment and food processing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-454. Producer or source: Babcock & Wilcox Company.
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Abstract
View article
PDF
HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-317. Producer or source: Cabot Wrought Products.
Journal Articles
Alloy Digest (1993) 42 (10): Ni-442.
Published: 01 October 1993
... ALTEMP HX is an austenitic nickel-base alloy designed for outstanding oxidation and strength at high temperatures. The alloy is solid-solution strengthened. Applications include uses in the aerospace, heat treatment and petrochemical markets. This datasheet provides information on composition...
Abstract
View article
PDF
ALTEMP HX is an austenitic nickel-base alloy designed for outstanding oxidation and strength at high temperatures. The alloy is solid-solution strengthened. Applications include uses in the aerospace, heat treatment and petrochemical markets. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-442. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1998) 47 (1): SS-705.
Published: 01 January 1998
... ALLOY 00Cr25Ni6Mo2N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves...
Abstract
View article
PDF
ALLOY 00Cr25Ni6Mo2N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS-705. Producer or source: Central Iron & Steel Research Institute.
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... also has many applications in both the petrochemical and chemical area. Type 430 has moderate strength and good ductility. It can be cold worked readily for producing trim and can be joined successfully by several methods. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy also has many applications in both the petrochemical and chemical area. Type 430 has moderate strength and good ductility. It can be cold worked readily for producing trim and can be joined successfully by several methods. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-384. Producer or source: Carpenter. Originally published March 1981, revised April 1995.
Journal Articles
Alloy Digest (1995) 44 (4): SS-591.
Published: 01 April 1995
... resistance cast metal products castability chemical composition creep properties high-temperature alloys oxidation resistance PARALLOY H39W petrochemical applications physical properties tensile properties thermal properties A%a#yy piiiEGq EEizl .,ly;;5 - DIGEST- DATA ON WORLD WIDE METALS...
Abstract
View article
PDF
PARALLOY H39W is commonly known as HP Nb(Cb) modified and has excellent high temperature mechanical strength as well as resistance to carburization and oxidation. It is used in severe petrochemical service up to 1100 C (2010 F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-591. Producer or source: Paralloy Ltd.
Journal Articles
Alloy Digest (1995) 44 (11): SS-619.
Published: 01 November 1995
... & Clemens Inc. Producer or Source: Schmidt & Clemens Inc. Copyright © ASM International® 1996 1996 ASM International cast metal products castability chemical composition creep properties joinability MAERKER G-4855 petrochemical applications physical properties tensile properties...
Abstract
View article
PDF
MAERKER G-4855 is a heat resistant alloy casting for the petro chemical field. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-619. Producer or source: Schmidt & Clemens Inc.
Journal Articles
Alloy Digest (1983) 32 (10): Ni-293.
Published: 01 October 1983
... environments. The many corrosion-resistant properties of JS825 make the alloy a suitable choice for a variety of difficult applications. It is suitable for such applications as chemical and petrochemical processing, pulp and paper manufacturing, flue gas desulfurization systems and metal pickling operations...
Abstract
View article
PDF
JESSOP JS825 is a wrought nickel-iron-chromium-molybdenum-copper alloy for use in extremely corrosive environments. The many corrosion-resistant properties of JS825 make the alloy a suitable choice for a variety of difficult applications. It is suitable for such applications as chemical and petrochemical processing, pulp and paper manufacturing, flue gas desulfurization systems and metal pickling operations. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-293. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... SUPERTHERM is a cast nickel-chromium-iron alloy stabilized with cobalt and tungsten. It is used worldwide in extremely high-temperature applications and has unexcelled performance to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace...
Abstract
View article
PDF
SUPERTHERM is a cast nickel-chromium-iron alloy stabilized with cobalt and tungsten. It is used worldwide in extremely high-temperature applications and has unexcelled performance to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace tubes and refining furnace tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-228. Producer or source: Abex Corporation, Engineered Products Division. Originally published July 1969, revised November 1977.
Journal Articles
Alloy Digest (1970) 19 (12): SS-248.
Published: 01 December 1970
... SANDVIK 12R72HV is an austenitic chromium-nickel-molybdenum-titanium stainless steel suitable for metal temperature up to about 308 in the power industry and the petrochemical industry. Typical applications are superheater tubes and hydrocarbon crackers. This datasheet provides information...
Abstract
View article
PDF
SANDVIK 12R72HV is an austenitic chromium-nickel-molybdenum-titanium stainless steel suitable for metal temperature up to about 308 in the power industry and the petrochemical industry. Typical applications are superheater tubes and hydrocarbon crackers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: SS-248. Producer or source: Sandvik.
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries...
Abstract
View article
PDF
ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-252. Producer or source: Armco Steel Corporation, Advanced Materials Division.