Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1988) 37 (8): Fe-84.
Published: 01 August 1988
... ARMCO ORIENTED ELECTRICAL STEEL, nominally an iron 4% silicon soft magnetic alloy is available in four grades designated M-2, M-3, M-4, M-6. They have a much lower core loss in the rolling direction than nonoriented grades. Their permeability is high even at high inductions. This datasheet...
Journal Articles
Alloy Digest (1999) 48 (6): SS-748.
Published: 01 June 1999
... Carpenter SCF 19 alloy is a high-strength and low-magnetic permeability alloy developed for nonmagnetic drill collars. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes...
Journal Articles
Alloy Digest (2004) 53 (11): CS-144.
Published: 01 November 2004
... HP magnet steel is designed for use wherever high magnetic permeability or high saturation values are required. Its magnetic qualities result from careful control of sulfur and residual elements plus the special deoxidization practice, which minimizes nonmetallic inclusions. This datasheet...
Journal Articles
Alloy Digest (1968) 17 (8): Fe-35.
Published: 01 August 1968
... B and W IRON is a thoroughly killed, low carbon steel having a combination of ductility, toughness and high magnetic permeability. It is recommended for applications where good magnetic characteristics are of primary significance, such as in the manufacture of electric motor and generator housings...
Journal Articles
Alloy Digest (1969) 18 (8): Fe-38.
Published: 01 August 1969
... Permeability Magnetic Iron) AJfenol is an unoriented 125, to 16% aluminum-iron alloy which has high electrical resistivity and low eddy current losses. It is furnished in the 12% aluminum and in the 16% aluminum grades. The recommended uses are for relays, gyro mechanisms, servo-mechanisms and toroid tape...
Journal Articles
Alloy Digest (1953) 2 (6): Fe-1.
Published: 01 June 1953
... GLOBEIRON is a high purity, thoroughly killed, low carbon iron. It is ductile, tough, and has high magnetic permeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1967) 16 (4): Ni-123.
Published: 01 April 1967
... Carpenter Vacumet HyMu 800 is a vacuum melted nickel-molybdenum-iron alloy recommended as strip for laminations or torroids with a minimum permeability of 65,000 at 40 gauss in strip 0.010-0.001 inch thick. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
... Carpenter HYMU 80 is an unoriented 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability and maximum permeability with minimum hysteresis loss at low magnetic field strengths. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2019) 68 (6): SA-847.
Published: 01 June 2019
... for use as large fabricated DC magnets. Chemical Composition, wt.% (Maximum) HP magnet steel is fully killed. Carbon 0.08 Manganese 0.25 0.45 Phosphorus 0.025 Sulfur 0.025 Silicon 0.50 Cu+Ni+Cr+Mo 0.50 Physical Properties Permeability and hysteresis are noted in Fig. 1 and 2. Mechanical Properties...
Journal Articles
Alloy Digest (1956) 5 (4): Ni-25.
Published: 01 April 1956
... MUMETAL is a high permeability nickel iron alloy to be used where high permeability at flux densities well under 5000 gausses is desirable. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1957) 6 (10): Fe-15.
Published: 01 October 1957
... TEMPERATURE COMPENSATOR 30 and 32 are nickel-iron alloys whose magnetic permeability decreases proportionally with increasing temperatures within the usual range of atmospheric temperature variation. They are recommended for temperature compensation applications in electrical apparatus...
Journal Articles
Alloy Digest (1958) 7 (12): Ni-48.
Published: 01 December 1958
... 1 MONEL 403 Filing Code: Ni-48 Nickel Alloy DECEMBER 1958 DIGEST -DATA ON WORLD WIDE METALS AND ALLOYS- PcrblisbJ br Engineering Alloys I&es, Inc Upper Montclair. New Jersey MONEL* 403 (Low Permeability Nickel-Copper Alloy) MoneI 403 is a nickel-copper aIIoy having excellent combination of strength...
Journal Articles
Alloy Digest (1976) 25 (11): Ni-235.
Published: 01 November 1976
... METGLAS Alloy 2826 (Fe40Ni40P14B6) is a ferromagnetic, high permeability, nickel-iron metallic glass which, when appropriately annealed, yields a material similar to the higher nickel containing permalloys in magnetic properties. Alloy 2826 is a single phase, opaque metallic material with a glass...
Journal Articles
Alloy Digest (1974) 23 (7): Fe-51.
Published: 01 July 1974
... UNILOY 888 is an iron-base, age-hardenable alloy designed primarily for applications requiring low magnetic permeability and high strength. It is austenitic at all times and its essentially non-magnetic characteristics are not impaired by various combinations of heat treatment and cold working...
Journal Articles
Alloy Digest (1994) 43 (12): Fe-108.
Published: 01 December 1994
... CARPENTER SILICON CORE IRON A-FM (High Initial Permeability Magnetic Core ton) Caxpenter Silicon Core Iron A-FM , melted to exacting chemical specifications and carefuliy process controkd to produce a fine-grained uniform quality magnetic core iron. This alloy exhibits improved machining characteristics...
Journal Articles
Alloy Digest (1989) 38 (10): Ni-375.
Published: 01 October 1989
... CARPENTER HyMu 80 alloy is an unoriented soft magnetic alloy with extremely high initial permeability as well as maximum permeability with minimum hysteresis loss. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1990) 39 (9): Ni-385.
Published: 01 September 1990
... HYPERNOM alloy is a high-permeability, low-hysteresis nickel-base alloy which is provided with the correct temper for sheet metal cold formability for shielding components. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1991) 40 (1): Fe-94.
Published: 01 January 1991
... properties CARPENTER SILICON CORE IRON A Filing Code: Iron Alloy Fe-94 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1991 Ptiidhed byr Ahy Digeet. Inc /2[)1-6Z -9161 27 CaMeId Stmet. Orange. NJ. 07060 I U.SA CARPENTER SILICON CORE IRON A (High Initial Permeability Magnetic Core Iron...
Journal Articles
Alloy Digest (1994) 43 (1): SS-561.
Published: 01 January 1994
... CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY offers much of the properties of 430 stainless steel, but through composition and processing maintains consistently high magnetic permeability and low residual induction. This datasheet provides information on composition, physical properties...