1-19 of 19 Search Results for

ornamental trim

Sort by
Journal Articles
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
... Ansonia alloy C22000 is a 10% Zn alloy with the previous trade name of Commercial Bronze. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also...
Journal Articles
Alloy Digest (2009) 58 (7): Cu-772.
Published: 01 July 2009
... Ansonia alloy C22600 is a 12.5% Zn alloy with the previous trade name of jewelry bronze. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also...
Journal Articles
Alloy Digest (2009) 58 (8): Cu-773.
Published: 01 August 2009
... Ansonia alloy C23000 is a 15% Zn alloy with the previous trade name of Red Brass. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (2009) 58 (9): Cu-774.
Published: 01 September 2009
... Ansonia alloy C24000 is a 20% Zn alloy with the trade name of low brass. It is often used in musical instruments and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information...
Journal Articles
Alloy Digest (1980) 29 (11): Cu-406.
Published: 01 November 1980
... enough for use in industrial and engineering applications, yet exceptionally malleable for extensive use as the base metal for coins, costume jewelry, medallions and ornamental trim. It also provides an excellent base for coating with vitreous enamels and gold plating. Among this alloy s other noteworthy...
Journal Articles
Alloy Digest (2009) 58 (5): Cu-770.
Published: 01 May 2009
..., medallions, and ornamental trim. It is also an excellent base for coating with vitreous enamels, lacquer, and gold plating. Typical applications requiring these properties are fasteners, electrical equipment, and connectors. Producer: Ansonia Copper & Brass, Inc. Waterbury, CT 06708 Tel: 800/512-1703 or 203...
Journal Articles
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
...; lipstick tubes; marine hardware; metallic bellows; munitions; ornamental trim; pen; pencil; primer caps; rotating bands; vitreous enamel base. Supplier Austral Wright Metals 133 139 Cowpasture Road Wetherill Park, New South Wales 2164, Australia Tel: +61 02 9827 0790 Web: www.australwright.com.au All data...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... plate, base for vitreous enamel, bullet jackets, coins, connectors, emblems, fasteners, firing pin support shells, fuse caps, jewelry, medallions, medals, ornamental trim, plaques, primers, rotor bars, tokens. Applications information sourced from Copper Development Association. Copyright © 2020, ASM...
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
...) Product Forms Thermal 20 °C 189 Plate, sheet, strip. conductivity 10 6/K (68 °F) (109) Specific heat (10 6/°F) 20 °C 377 Applications Application capacity (68 °F) (0.09)(a) Electrical W/(m K) 0.0392 Category Etching bronze; grill work; ornamental trim; resistivity (Btu/(h·ft·°F)) (23.6) Architecture...
Journal Articles
Alloy Digest (2002) 51 (11): Cu-692.
Published: 01 November 2002
.... Other miscellaneous applications include compacts, lipstick cases, costume jewelry, ornamental trim, screen wire, a base for vitreous enamel, and waveguides. Producer: Wieland Metals, Inc. Wheeling, IL 60090 (847) 537-3990 (847) 537-4085 (fax) In Germany: Wieland-Werke AG D-89070 Ulm +49-0731-944-0 +49...
Journal Articles
Alloy Digest (1972) 21 (4): Cu-254.
Published: 01 April 1972
...: Etching bronze, grill work, screen cloth, weather stripping, compacts, costume jewelry, ornamental trim, primer caps, rotating bands, screw wheels, escutcheon plates, marine hardware, rivets, screws. Manufacturer: Practically all brass mills. ...
Journal Articles
Alloy Digest (1974) 23 (2): Cu-275.
Published: 01 February 1974
... applications. Forms Available: Castings. Applications: Marine castings, ship trimmings, furniture trim, hardware, valves, and ornamental castings. Manufacturer: Copper alloy foundries. ...
Journal Articles
Alloy Digest (1980) 29 (1): Sn-8.
Published: 01 January 1980
... and ornamental articles and trim for special uses. Manufacturers: Producers of tin alloys. ...
Journal Articles
Alloy Digest (1983) 32 (1): Al-242.
Published: 01 January 1983
... ALUMINUM 518.0 is an aluminum die-casting alloy with an excellent combination of high strength and resistance to corrosion. It also has high ductility, good polishing characteristics, poor castability (it is hot short) and excellent machinability. Its uses include marine fittings, ornamental...
Journal Articles
Alloy Digest (1980) 29 (10): Cu-405.
Published: 01 October 1980
... by the following methods: sand, per- manent mold, plaster, continuous and centrifugal. Ingots. Applications: General-purpose castings not subject to high internal pressure, furniture hardware, ornaments, radiator fittings, ship trimmings, gas cocks, battery clamps,valves, fittings. plumbing components, ferrules...
Journal Articles
Alloy Digest (1977) 26 (4): Cu-331.
Published: 01 April 1977
... Alloy No. 976 is reported to be 32,500 psi at 5000F and 22.200 psi at 5500F. Forms Available: Castings (sand and centrifugal) and ingots. Applications: Marine castings, ship trimmings, furniture trim, hardware, valves, ornamental castings, musical instrument components and flanges. Manufacturers: Copper...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-411.
Published: 01 February 1981
... many applications are architectural trim, cosmetics containers, hardware, munitions and miscellaneous. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1978) 27 (4): Al-121.
Published: 01 April 1978
... ALUMINUM 5457 is an aluminum sheet alloy that offers a lustrous, mirror-like appearance when polished, brightened and anodized. The brightness of the specially treated sheet makes it particularly desirable for decorative trim applications in the appliance and automotive industries. This datasheet...
Journal Articles
Alloy Digest (1978) 27 (11): Al-38.
Published: 01 November 1978
..., utensils, electrical conduction, ap pliances, trim, ornamental work, louvered refrigerator shelves, meat trays and light reflectors. Manufacturers: Aluminum alloy mills. ...