1-20 of 53 Search Results for

ornamental products

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1987) 36 (2): Al-277.
Published: 01 February 1987
... many uses include aircraft components, gears, machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... properties. It has good castability, excellent machinability and high resistance to corrosion. TERNALLOY 7 has many uses including aircraft components, gears machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1983) 32 (1): Al-242.
Published: 01 January 1983
... ALUMINUM 518.0 is an aluminum die-casting alloy with an excellent combination of high strength and resistance to corrosion. It also has high ductility, good polishing characteristics, poor castability (it is hot short) and excellent machinability. Its uses include marine fittings, ornamental...
Journal Articles
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
... appearance, its pleasing color also finds use in cosmetic applications such as lipstick and compact cases, and in ornamental trim and costumed jewelry. Large-diameter tube production of this alloy also contributes to its varied uses. Projectile rotating bands are fabricated from the base stock cut from these...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... DZR Yellow Brass is a new, corrosion-resistant brass. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, marine hardware, ornaments and door handles. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2009) 58 (9): Cu-774.
Published: 01 September 2009
... Ansonia alloy C24000 is a 20% Zn alloy with the trade name of low brass. It is often used in musical instruments and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information...
Journal Articles
Alloy Digest (2009) 58 (8): Cu-773.
Published: 01 August 2009
... Ansonia alloy C23000 is a 15% Zn alloy with the previous trade name of Red Brass. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-450.
Published: 01 December 1982
... Copper Alloy No.1 C84200 is a free-machining copper-tin-lead-zinc alloy for castings; it was formerly identified as 80-5-2.5-12.5 alloy. It has good casting characteristics, good machinability, moderate strength and ductility and good corrosion resistance. Among its many uses are ornamental...
Journal Articles
Alloy Digest (1969) 18 (7): Cu-202.
Published: 01 July 1969
... COPPER Alloy No. 240 is a copper-zinc alloy having high ductility and malleability combined with good corrosion resistance and relative freedom from intergranular corrosion and embrittlement. It is recommended for pump lines, flexible hose and ornamental work. This datasheet provides information...
Journal Articles
Alloy Digest (1973) 22 (12): Sn-5.
Published: 01 December 1973
... ornamental uses. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, forming, heat...
Journal Articles
Alloy Digest (2009) 58 (7): Cu-772.
Published: 01 July 2009
... Ansonia alloy C22600 is a 12.5% Zn alloy with the previous trade name of jewelry bronze. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also...
Journal Articles
Alloy Digest (1961) 10 (12): Al-109.
Published: 01 December 1961
... ALCAN A320 is an aluminum casting alloy suitable for architectural, ornamental and marine uses. It has good finishing characteristics and excellent corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and...
Journal Articles
Alloy Digest (1977) 26 (10): Cu-342.
Published: 01 October 1977
..., valves and ornaments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-342. Producer or source: Copper...
Journal Articles
Alloy Digest (1978) 27 (1): Cu-346.
Published: 01 January 1978
... applications as plumbing goods, ornaments and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining...
Journal Articles
Alloy Digest (1980) 29 (1): Sn-8.
Published: 01 January 1980
... WHITE METAL is a low-strength tin-antimony alloy with a solidus temperature of 246 C (475 F); its liquidus temperature is only a few degrees higher. Because of its attractive appearance, it has a long history of ornamental uses. It is used widely for making costume jewelry. This datasheet provides...
Journal Articles
Alloy Digest (1982) 31 (7): Al-239.
Published: 01 July 1982
... engine parts, pressure-tight castings, ornamental castings and machine frames. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... characteristics. Product Forms Plate, sheet, strip Applications AC motors, base for gold plate, base for vitreous enamel, bullet jackets, coins, connectors, emblems, fasteners, firing pin support shells, fuse caps, jewelry, medallions, medals, ornamental trim, plaques, primers, rotor bars, tokens. Ap- plications...
Journal Articles
Alloy Digest (1960) 9 (6): Cu-89.
Published: 01 June 1960
... REVERE No. 140 is a copper-zinc alloy containing 20% zinc. It is recommended for deep drawn and cold formed products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
...) Product Forms Thermal 20 °C 189 Plate, sheet, strip. conductivity 10 6/K (68 °F) (109) Specific heat (10 6/°F) 20 °C 377 Applications Application capacity (68 °F) (0.09)(a) Electrical W/(m K) 0.0392 Category Etching bronze; grill work; ornamental trim; resistivity (Btu/(h·ft·°F)) (23.6) Architecture...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-411.
Published: 01 February 1981
... ANACONDA Alloy 220 is a copper-zinc alloy having good formability and good resistance to dezincification and stress-corrosion cracking. Among the binary brasses it holds a favored position where product appearance is an important factor; it possesses a rich and pleasing bronze color. Among its...