Alloy Digest (1955) 4 (1): Cu-22.
Published: 01 January 1955
... OLYMPIC BRONZE Type A is a silicon bronze designed especially for structural and engineering purposes. It has the combination of high strength, workability, and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...