Alloy Digest (1984) 33 (8): SS-450.
Published: 01 August 1984
... 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as...
Journal Articles
Alloy Digest (1984) 33 (3): SS-441.
Published: 01 March 1984
... structures can be fabricated easily and it can be machined readily. It can be welded easily and gives strong, ductile welds. Some of its many applications are annealing boxes, boiler baffles, dryers, furnace parts, heat exchangers and oil-refining equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1976) 25 (8): TS-306.
Published: 01 August 1976
...% CO atmosphere for 20 min. at temperature and oil quenched) Hardening Rockwell Shepherd Temperature C Fracture oF Hardness Rating 1350 27-28 6 Coarse 1400 61-62 8 Slightly coarse 1450 64-65 9% Refined 1475 64.5 9 Refined 1500 65-65.5 8% Slightly coarse 1550 64.5 fj 2 Coarse 1600 63.5 5 Coarse...
Journal Articles
Alloy Digest (1965) 14 (8): SA-182.
Published: 01 August 1965
... fracture toughness hardness heat treatability joinability machinability physical properties SPEED ALLOY tensile properties workability SPEED ALLOY Filing Code: SA-182 Steel-Alloy AUGUST 1965 -DATA ON WORLD WIDE METALS AND ALLOYS SPEED ALLOY (Oil Hardening Alloy Steel) Puidisbed by Engineering...
Journal Articles
Alloy Digest (1970) 19 (4): SS-236.
Published: 01 April 1970
... FIRTH VICKERS FI (A1) is a chromium type heat and corrosion resistant alloy steel recommended for oil refining and chemical plant equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1997) 46 (11): SS-702.
Published: 01 November 1997
... ALLOY 00Cr18Ni5Mo3Si2 is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, these duplex stainless steels have substituted for austenitic stainless steels in many...
Journal Articles
Alloy Digest (1997) 46 (12): SS-704.
Published: 01 December 1997
... ALLOY 00Cr22Ni5Mo3N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1980) 29 (4): SA-371.
Published: 01 April 1980
.... Cabot ESR 4140 has outstanding fatigue strength and a good combination of strength and ductility. Its applications range from gas turbines to oil-field equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... remelting with the use of small-heat-size technology. Electroslag refining Improves cleanliness and lowers the sulfur content to provide improved isotropy. ductility and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for...
Journal Articles
Alloy Digest (1983) 32 (6): SA-391.
Published: 01 June 1983
... has outstanding fatigue strength and a good combination of strength and ductility. Its applications range from gas turbines to oil-field equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and...
Journal Articles
Alloy Digest (1984) 33 (10): Ni-304.
Published: 01 October 1984
... NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers and...
Journal Articles
Alloy Digest (1998) 47 (1): SS-705.
Published: 01 January 1998
... ALLOY 00Cr25Ni6Mo2N is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and...
Journal Articles
Alloy Digest (1998) 47 (2): SS-706.
Published: 01 February 1998
... ALLOY 0Cr25Ni6Mo3CuN is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves...
Journal Articles
Alloy Digest (1976) 25 (7): SS-330.
Published: 01 July 1976
... carbides. At high temperatures ACI Type HE has excellent corrosion resistance, good ductility and moderate strength. It is used in the steel, power, oil refining and smelting industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as...
Journal Articles
Alloy Digest (1969) 18 (2): SS-220.
Published: 01 February 1969
... Croloy 18 13 3 is a chromium-nickel-molybdenum stainless steel characterized as having high corrosion resistance to certain acidic solutions. It is recommended for paper, chemical, and oil refining industries. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-12.
Published: 01 May 1996
... readily. in general with slower speeds and lighter feeds than required with the austenitic stainless steels. Turning. facing. and boring with Stellite@ cobah-chro- mium-tungsten metalcutting tools can be done using a soluble-oil COOl~t. Production of Castings: Chlotimet 2 can be cast successfully with no...
Journal Articles
Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1978) 27 (5): Ni-255.
Published: 01 May 1978
...: Shot and ingots for remelting. Applications: Components for oil-refining, petrochemical and chemical equip- ment; heat-treating equipment such as trays, buckets and conveyor chains; and high-temperature components for con- ventional and jet aircraft. Manufacturer: Cannon-Muskegon Corporation Muskegon...
Journal Articles
Alloy Digest (1969) 18 (7): SS-227.
Published: 01 July 1969
... AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment. This...