Skip Nav Destination
Close Modal
Search Results for
oil refinery equipment
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 65
Search Results for oil refinery equipment
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
CANNON-MUSKEGON NICKEL ALLOY C: Cast Corrosion and Heat Resistant Alloy, AMS 5388
Available to Purchase
Alloy Digest (1978) 27 (5): Ni-255.
Published: 01 May 1978
... components and oil-refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining...
Abstract
View articletitled, CANNON-MUSKEGON NICKEL ALLOY C: Cast Corrosion and Heat Resistant Alloy, AMS 5388
View
PDF
for article titled, CANNON-MUSKEGON NICKEL ALLOY C: Cast Corrosion and Heat Resistant Alloy, AMS 5388
CANNON-MUSKEGON Nickel Alloy C is a cast nickel-base alloy with exceptionally high resistance to corrosion and with excellent high-temperature properties. It also has outstanding oxidation resistance and strength at elevated temperatures. Its many uses include heat-treating equipment, aerospace components and oil-refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Ni-255. Producer or source: Cannon-Muskegon Corporation.
Journal Articles
REVERE No. 464: Naval Brass
Available to Purchase
Alloy Digest (1969) 18 (8): Cu-204.
Published: 01 August 1969
... Revere No. 464 is a copper-zinc alloy having good strength, toughness, and resistance to corrosion. It is recommended for steam condensers, marine equipment and oil refinery equipment, most especially in the form of sheet and plate, the latter as the heads for condensers and similar heat...
Abstract
View articletitled, REVERE No. 464: Naval Brass
View
PDF
for article titled, REVERE No. 464: Naval Brass
Revere No. 464 is a copper-zinc alloy having good strength, toughness, and resistance to corrosion. It is recommended for steam condensers, marine equipment and oil refinery equipment, most especially in the form of sheet and plate, the latter as the heads for condensers and similar heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-204. Producer or source: Revere Copper and Brass Inc..
Journal Articles
COOPER ALLOY 31: Heat Resisting Steel
Available to Purchase
Alloy Digest (1968) 17 (2): SS-205.
Published: 01 February 1968
... COPPER Alloy 31 is an iron-chromium-molybdenum casting alloy having good resistance to oxidation at temperatures up to about 1200 F. It is recommended for furnace parts and oil refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View articletitled, COOPER ALLOY 31: Heat Resisting Steel
View
PDF
for article titled, COOPER ALLOY 31: Heat Resisting Steel
COPPER Alloy 31 is an iron-chromium-molybdenum casting alloy having good resistance to oxidation at temperatures up to about 1200 F. It is recommended for furnace parts and oil refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-205. Producer or source: Cooper Alloy Corporation.
Journal Articles
AISI TYPE 502: Corrosion Resisting Steel
Available to Purchase
Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Abstract
View articletitled, AISI TYPE 502: Corrosion Resisting Steel
View
PDF
for article titled, AISI TYPE 502: Corrosion Resisting Steel
AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-211. Producer or source: Stainless steel mills.
Journal Articles
AISI TYPE 430: Non Hardenable Chromium Stainless Steel
Available to Purchase
Alloy Digest (1969) 18 (7): SS-227.
Published: 01 July 1969
... AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment...
Abstract
View articletitled, AISI TYPE 430: Non Hardenable Chromium Stainless Steel
View
PDF
for article titled, AISI TYPE 430: Non Hardenable Chromium Stainless Steel
AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-227. Producer or source: Stainless steel mills.
Journal Articles
AL TECH 6X: Austenitic Stainless Steel
Available to Purchase
Alloy Digest (1980) 29 (10): SS-376.
Published: 01 October 1980
... AL Tech 6X is an austenitie (non-magnetic) alloy developed for service in pitting environments containing chlorides. It was designed for resistance to pitting and crevice corrosion encountered in seawater, pulp and paper manufacture, petroleum refineries, chemical process equipment and sour oil...
Abstract
View articletitled, AL TECH 6X: Austenitic Stainless Steel
View
PDF
for article titled, AL TECH 6X: Austenitic Stainless Steel
AL Tech 6X is an austenitie (non-magnetic) alloy developed for service in pitting environments containing chlorides. It was designed for resistance to pitting and crevice corrosion encountered in seawater, pulp and paper manufacture, petroleum refineries, chemical process equipment and sour oil-well components. Alloy 6X also provides good resistance to general corrosion in a number of media. It possesses good ductility, high impact values and good weldability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-376. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
ACI TYPE CK-20: Corrosion and Heat Resisting Steel
Available to Purchase
Alloy Digest (1967) 16 (2): SS-191.
Published: 01 February 1967
... Type CK-20 is the 25-20 type corrosion resisting casting alloy. It has high degree of stability against intergranular corrosion. It is recommended for chemical plant equipment, oil refinery components and paper and pulp industry parts. This datasheet provides information on composition, physical...
Abstract
View articletitled, ACI TYPE CK-20: Corrosion and Heat Resisting Steel
View
PDF
for article titled, ACI TYPE CK-20: Corrosion and Heat Resisting Steel
Type CK-20 is the 25-20 type corrosion resisting casting alloy. It has high degree of stability against intergranular corrosion. It is recommended for chemical plant equipment, oil refinery components and paper and pulp industry parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-191. Producer or source: Stainless steel foundries.
Journal Articles
AISI TYPE 501: Corrosion Resisting Steel
Available to Purchase
Alloy Digest (1961) 10 (7): SS-119.
Published: 01 July 1961
..., strips and wires. Applications: Oil cracking steel tubes, oil refinery equipment, oil pump impellers, flow line headers, pipe fittings, valve trim, equipment for processing very sour crude oil containing large amounts of sulphur as in superheaters. Manufacturer: All stainless steel milis make this type...
Abstract
View articletitled, AISI TYPE 501: Corrosion Resisting Steel
View
PDF
for article titled, AISI TYPE 501: Corrosion Resisting Steel
AISI Type 501 is a low-chromium type corrosion steel that is used for its heat resistance and good mechanical properties at elevated temperatures as well as for its corrosion resistance at moderately elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-119. Producer or source: Stainless steel mills.
Journal Articles
NICLOY 400: Nickel Copper Alloy
Available to Purchase
Alloy Digest (1984) 33 (10): Ni-304.
Published: 01 October 1984
... NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers...
Abstract
View articletitled, NICLOY 400: Nickel Copper Alloy
View
PDF
for article titled, NICLOY 400: Nickel Copper Alloy
NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers and numerous machined parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-304. Producer or source: Babcock & Wilcox Company.
Journal Articles
ARMCO 309 and 309S: Stabilized Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2002) 51 (5): SS-853.
Published: 01 May 2002
... aircraft components, radiant superheaters, bellows, and oil refinery equipment. Producer: AK Steel, Inc. Specialty Flat-Rolled Steels Butler Operations Butler, PA 16003-0832 (800) 381-5663 (412) 284-2874 (fax) Coshocton Operations Coshocton, OH 43812 (800) 422-4422 (614) 829-2684 (fax) ISSN: 002-614X SS...
Abstract
View articletitled, ARMCO 309 and 309S: Stabilized Austenitic Stainless Steel
View
PDF
for article titled, ARMCO 309 and 309S: Stabilized Austenitic Stainless Steel
Types 309 and 309S are austenitic chromium-nickel stainless steels that provide excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. Type 309S is identical to Type 309 except for a lower carbon content that minimizes carbide precipitation and improves weldability. Typical uses include furnace parts, heating elements, aircraft and jet engine parts, heat exchangers, carburizing-annealing boxes, sulfite liquor handling equipment, kiln liners, boiler baffles, refinery and chemical processing equipment, and auto exhaust parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-853. Producer or source: AK Steel Inc.
Journal Articles
ARMCO 434: Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2000) 49 (6): SS-792.
Published: 01 June 2000
..., steam iron bases, and flatware. Commercial and industrial appli- cations range from interior architectural uses to nitric acid plant equipment, oil refinery equipment, roofing, siding, and restaurant equipment. Producer: Armco Inc. Specialty Flat-Rolled Steels Coshocton Operations Coshocton, OH 43812...
Abstract
View articletitled, ARMCO 434: Ferritic Stainless Steel
View
PDF
for article titled, ARMCO 434: Ferritic Stainless Steel
Armco 434 is a ferritic stainless steel with good corrosion resistance to mildly corrosive environments and the atmosphere. The alloy is oxidation resistant at temperatures up to 871 deg C (1600 deg F) for intermittent service and up to 788-816 deg C (1450-1500 deg F) for continuous service. It is used for automotive trim and other exterior environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-792. Producer or source: Armco Inc.
Journal Articles
ARMCO 430: Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2000) 49 (9): SS-803.
Published: 01 September 2000
... architectural applications to nitric acid plant equipment, oil refinery equipment, roofing and siding, and restau- rant equipment. Producer: AK Steel Specialty Flat-Rolled Steels Coshocton Operations Coshocton, OH 43812 (800) 422-4422 (614) 829-2684 (fax) AK Steel International Sales Houston, TX 77060 (281) 872...
Abstract
View articletitled, ARMCO 430: Ferritic Stainless Steel
View
PDF
for article titled, ARMCO 430: Ferritic Stainless Steel
Armco Type 430 is one of the most widely used of the “nonhardenable” ferritic stainless steels. It combines good corrosion resistance and heat and oxidation resistance up to 816 deg C (1500 deg F) with good mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-803. Producer or source: AK Steel Inc.
Journal Articles
SICROMO 5S: Corrosion and Heat Resisting Steel
Available to Purchase
Alloy Digest (1969) 18 (12): SS-232.
Published: 01 December 1969
.... It is suitable for cracking tubes in oil refineries under conditions demanding an extraordinary combination of oxidation resistance and corrosion resistance at high operating temperatures. It is used for the higher temperature zones in mercury boilers. Forms Available: Tubes Applications: Oil refinery equipment...
Abstract
View articletitled, SICROMO 5S: Corrosion and Heat Resisting Steel
View
PDF
for article titled, SICROMO 5S: Corrosion and Heat Resisting Steel
SICROMO-5S is a low-carbon, 5% chromium alloy steel recommended for applications in which a high degree of surface stability under oxidizing conditions is required for temperatures up to 1500 F. It is used in air prehealer tubes, recuperater and superheater tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-232. Producer or source: Timken Company Steel Division.
Journal Articles
AISI TYPE 308: Corrosion and Heat Resistant Steel
Available to Purchase
Alloy Digest (1963) 12 (1): SS-140.
Published: 01 January 1963
... is for weldiog rod to compensate for alloying elements chat may be lost by oxi- datioo duriog weldiog. Forms Available: Sheet, scrip, plate, wire and bars. Applications: Welded structures, architectural trim, valve trim, oil refinery equipment, equipment for handling food and dairy products, high temperature...
Abstract
View articletitled, AISI TYPE 308: Corrosion and Heat Resistant Steel
View
PDF
for article titled, AISI TYPE 308: Corrosion and Heat Resistant Steel
AISI Type 308 is an austenitic chromium nickel steel with corrosion and heat resistance superior to Type 304. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-140. Producer or source: Alloy steel mills and foundries.
Journal Articles
ENDURO AA-FM: Free Cutting Stainless Steel, Type 430F
Available to Purchase
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
... will be greatly reduced. Forms Available: Bars, rods and forgiogs. Applications: Chemical plant equipment, ice making machinery, nitric acid plant equipment, nitrogen fixation apparatus, oil burner parts and heaters, oil refinery equipment, rubber plant machinery, soot blowers, tanks, bolts, low temperature...
Abstract
View articletitled, ENDURO AA-FM: Free Cutting Stainless Steel, Type 430F
View
PDF
for article titled, ENDURO AA-FM: Free Cutting Stainless Steel, Type 430F
ENDURO AA-FM is a free-machining chromium type stainless steel equivalent to AISI Type 430-F. It is ferritic and non-hardenable. It is corrosion and heat resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-35. Producer or source: Republic Steel Corporation.
Journal Articles
DARWINS 18/8 W.P.D.: Welding Grade Stainless Steel
Available to Purchase
Alloy Digest (1967) 16 (6): SS-195.
Published: 01 June 1967
... aircraft components, radiant superheaters, oil refinery equipment. Manufacturer: Darwins Ltd., Fitzwilliam Works, Sheffield, England ...
Abstract
View articletitled, DARWINS 18/8 W.P.D.: Welding Grade Stainless Steel
View
PDF
for article titled, DARWINS 18/8 W.P.D.: Welding Grade Stainless Steel
DARWINS 18/8 W.P.D. is a titanium stabilized 18/8 type stainless steel being free of weld decay. It is recommended for welded equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-195. Producer or source: Darwin's Ltd.
Journal Articles
HASTELLOY ALLOY B: Corrosion and Heat Resistant Alloy
Available to Purchase
Alloy Digest (1957) 6 (8): Ni-36.
Published: 01 August 1957
.... Applications: Chemical and oil refinery equipment, valves, pumps, pipe connections, equipment handling hydrochloric acid and wet HCL gas, gas turbine applications, turbine blades and wheels. high temperature bolting and shafting. Manufacturer: Haynes Stellite Company, A Division of Union Carbide & Carbon...
Abstract
View articletitled, HASTELLOY ALLOY B: Corrosion and Heat Resistant Alloy
View
PDF
for article titled, HASTELLOY ALLOY B: Corrosion and Heat Resistant Alloy
HASTELLOY ALLOY B is a nickel-molybdenum-iron alloy well suited for equipment handling boiling hydrochloric acid and wet hydrochloric acid gas. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-36. Producer or source: Haynes Stellite Company.
Journal Articles
USS 17: Corrosion Resistant Steel, Type 430
Available to Purchase
Alloy Digest (1960) 9 (6): SS-104.
Published: 01 June 1960
..., builders hardware, nitrogen fixation apparatus, oil burner parts and heaters, oil refinery equipment, bolts-nuts and studs in corrosive service, low temperature annealing furnace pares, septic tanks, kitchen sinks, soot slowers, television cones and tubing, food handling equipment, and dairy equilxnent...
Abstract
View articletitled, USS 17: Corrosion Resistant Steel, Type 430
View
PDF
for article titled, USS 17: Corrosion Resistant Steel, Type 430
U.S.S. 17 is high-chromium, corrosion resistant steel of the Type 430 classification. It is moderately ductile and non-hardenable through heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-104. Producer or source: United States Steel Corporation.
Journal Articles
ENDURO AA: High-Chromium, Non Hardening Stainless Steel
Available to Purchase
Alloy Digest (1953) 2 (6): SS-9.
Published: 01 June 1953
... Available: Cold drawn shapes, wire, welding rod, tubing, bars, slabs, billets, forging blanks, plates, sheets, and strip. Applications: Automotive trim, interior architectural trim, builders hardware, nitrogen fixation apparatus, oil burner park and heaters, oil refinery equipment, bolts - nuts and studs...
Abstract
View articletitled, ENDURO AA: High-Chromium, Non Hardening Stainless Steel
View
PDF
for article titled, ENDURO AA: High-Chromium, Non Hardening Stainless Steel
ENDURO AA is a ductile, non-hardening alloy containing 14 to 18 percent chromium with carbon under 0.12 per cent. It has mechanical properties equal to high grade medium carbon steel, with high resistance to general corrosion and oxidation at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-9. Producer or source: Republic Steel Corporation.
Journal Articles
SILCROME-RA: Corrosion Resisting Steel
Available to Purchase
Alloy Digest (1958) 7 (10): SS-79.
Published: 01 October 1958
... Forms Available: Bars, rods, sheet, wire. Applications: Automotive trim, interior archirectural trim, builders hard- ware, nitrogen fixation apparatus, oil burner parts and heaters, oil refinery equipment, bolts, nuts and studs in corrosive service, low temperature annealing furnace parts, septic tanks...
Abstract
View articletitled, SILCROME-RA: Corrosion Resisting Steel
View
PDF
for article titled, SILCROME-RA: Corrosion Resisting Steel
SILCROME-RA is a chromium type stainless steel having good corrosion resistance and mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-79. Producer or source: Allegheny Ludlum Corporation.
1