Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1967) 16 (11): SS-202.
Published: 01 November 1967
... Croloy 16-13-3 is a molybdenum-containing 18-12 type austenitic stainless steel having better corrosion resistance than the 18-8 type stainless steels. It is recommended for corrosion resisting applications in the chemical and oil refinery industries, paper pulp processing, etc. In addition...
Journal Articles
Alloy Digest (1968) 17 (2): SS-205.
Published: 01 February 1968
... COPPER Alloy 31 is an iron-chromium-molybdenum casting alloy having good resistance to oxidation at temperatures up to about 1200 F. It is recommended for furnace parts and oil refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1969) 18 (2): Cr-2.
Published: 01 February 1969
... UNILOY 50Cr/50Nj is an improved corrosion-resistant, wrought alloy with outstanding resistance to a wide variety of corrosive media. It is recommended for oil refinery heaters, incinerator components, metallurgical heat treating furnace components and reactor vessels for treating pulping liquors...
Journal Articles
Alloy Digest (1969) 18 (6): Cu-200.
Published: 01 June 1969
... Cupro Nickel, 30%-716 is a high strength copper-nickel-iron alloy for heat exchanger tubes in power plant feed water heaters, and also for oil refinery service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1969) 18 (8): Cu-204.
Published: 01 August 1969
... Revere No. 464 is a copper-zinc alloy having good strength, toughness, and resistance to corrosion. It is recommended for steam condensers, marine equipment and oil refinery equipment, most especially in the form of sheet and plate, the latter as the heads for condensers and similar heat...
Journal Articles
Alloy Digest (1969) 18 (7): SS-227.
Published: 01 July 1969
... AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment...
Journal Articles
Alloy Digest (1967) 16 (2): SS-191.
Published: 01 February 1967
... Type CK-20 is the 25-20 type corrosion resisting casting alloy. It has high degree of stability against intergranular corrosion. It is recommended for chemical plant equipment, oil refinery components and paper and pulp industry parts. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (8): SA-215.
Published: 01 August 1967
... SICROMO 9M is a chromium-molybdenum, low-carbon alloy steel having good corrosion resistance and high temperature strength. It is recommended for still tubes and piping in oil refineries, heat exchanger and super-heater tubes when a greater degree of corrosion resistance is required than provided...
Journal Articles
Alloy Digest (1974) 23 (9): SS-301.
Published: 01 September 1974
... Type HA is an air-hardening iron-chromium-molybdenum alloy containing sufficient chromium to provide good resistance to oxidation at temperatures up to about 1200 F. Castings of type HA alloy are used widely in oil refinery service and in the glass industry. This datasheet provides information...
Journal Articles
Alloy Digest (1956) 5 (4): SA-40.
Published: 01 April 1956
... CROLOY 7 is a 7% chromium-molybdenum low-carbon steel recommended for oil refinery corrosion resistance applications. It has very good corrosion resistance with good high temperature strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1978) 27 (5): Ni-255.
Published: 01 May 1978
... components and oil-refinery equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2007) 56 (4): Ni-648.
Published: 01 April 2007
... finishing characteristics make Nistelle Super C an ideal alloy for HVOF spraying imprinting, papermaking, oil refinery, and chemical processing industries. It can also be used as a plasma transferred arc weld overlay. Applications: Nistelle Super C is best used as HVOF coating in printing, paper- making...
Journal Articles
Alloy Digest (1961) 10 (7): SS-119.
Published: 01 July 1961
... resistance to mine and sea water, poor resistance to all inorganic acids of 5-l 5% concentration, good resistance to l-20% alkaline solutions, good resistance to oil refinery crudes below 400 deg. F., good resistance to mineral and vegetable oils, poor resistance to ammonium and hot sulphite liquors. Table 6...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-380.
Published: 01 September 1979
.... It is used most widely in marine service, oil refineries and tidewater power plants and in the chemical process industries. Ampcoloy 525 is used in the as-cast condition without further heat treatment, except that stress relieving is optional after heavy machining. Ampcoloy 525 is suit- able for many...
Journal Articles
Alloy Digest (1969) 18 (12): SS-232.
Published: 01 December 1969
... fair resistance to rural, seashore and industrial atmospheres, fair resistance to wet steam and domestic water, poor resistance to mine and sea water, poor resistance to all inorganic acids of 5-15% concentration, good resistance to l-20% alkaline solutions. good resistance to oil refinery crudes below...
Journal Articles
Alloy Digest (1976) 25 (9): Cu-319.
Published: 01 September 1976
... flow of water containing air bubbles and silt flowing at a high velocity. The alloy has good strength at moderately elevated temperatures and can be joined by welding, brazing and soldering. It is used most widely in marine service. oil refineries and tidewater power plants and in the chemical process...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... lines, alloy 706 is not especially adapted to handle heavily polluted waters containing sewage and industrial wastes. Alloy 706 finds its greatest application in marine service, in oil refineries for condensers and evaporators, in tide- water steam power plants, in sugar refmeries, in dis- tilleries...
Journal Articles
Alloy Digest (1980) 29 (10): SS-376.
Published: 01 October 1980
... AL Tech 6X is an austenitie (non-magnetic) alloy developed for service in pitting environments containing chlorides. It was designed for resistance to pitting and crevice corrosion encountered in seawater, pulp and paper manufacture, petroleum refineries, chemical process equipment and sour oil...
Journal Articles
Alloy Digest (1957) 6 (12): SA-64.
Published: 01 December 1957
... resistance ro mine and sea water, poor resistance to all inor- ganic acids of 5-15% concenuation, good resistance to oil refinery crudes below 400┬░F.. good resistance to mineral and vegetable oils, poor resistance to ammonium and hot sulphire liquors. General Characteristics: Sicromo 3 is a slicon-chromium...