Alloy Digest (1986) 35 (12): Al-274.
Published: 01 December 1986
... cases, gear cases, oil pans, airframe fittings and instrument housings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1962) 11 (6): Al-8.
Published: 01 June 1962
... castings, machine frames, motor frames, internal combustion engine parts, truck wheels, oil pans, diesel engine crankcases, oil pans, rear axle housings, piano plates and frames, gasoline and oil tanks. Manufacturer: Apex Smelting Company Chicago, Illinois and Cleveland, Ohio ...
Journal Articles
Alloy Digest (1964) 13 (5): Al-137.
Published: 01 May 1964
... stressed castings, pressure tight castings, machine frames, motor frames, internal combustion engine parts, hand truck wheels, oil pans, and frames. Manufacturer: Apex Smelting Division, American Metal Climax Inc. Cleveland, Ohio Chicago, Illinois Long Beach, California ...
Journal Articles
Alloy Digest (1958) 7 (12): Al-74.
Published: 01 December 1958
... castings. Applications: Oil pans, crankcases, camshaft housings and other parts not highly stressed Manufacturer: Aluminum ComPany of America Pittsburgh, Pennsylvania ...
Journal Articles
Alloy Digest (1963) 12 (5): Al-125.
Published: 01 May 1963
... wheels, washing machine agitators. Oil pans, crankcases, camshaft hous- ings and other parts not highly stressed. Manufacturer: Aluminum Company of America, Pittsburgh, Pennsylvania Olin MathiesonMetals Division, New York, New York ...
Journal Articles
Alloy Digest (1956) 5 (3): Al-37.
Published: 01 March 1956
...% internal combustion engine parts, truck wheels, oil pans, die- sel engine crankam, rear a& housings, piano plates and frames, gasoline and oil tanks. Apex Smelting Company chicago, Illinois - aevw Ohio - Los finge!ies¶ California ...
Journal Articles
Alloy Digest (1961) 10 (7): Al-105.
Published: 01 July 1961
... casting properties which are superior to most foundry alloys. Forms Available: Ingots, sand and permanent mold castings. Applications: Typewriter frames, engine parts, water-cooled cylinder heads, piano plates and frames, gasoline and oil tanks, internal combustion and diesel engine crankcases, oil pans...
Journal Articles
Alloy Digest (1965) 14 (11): Al-149.
Published: 01 November 1965
... castings, machine frames, motor frames , internal combustion engine parts, hand truck wheels, oil pans, and frames. Manufacturer: Aluminum Co. of Canada Ltd., Montreal, Canada ...
Journal Articles
Alloy Digest (1960) 9 (12): Al-98.
Published: 01 December 1960
.... Forms Available: Die castings and ingots. Applications: Ornamental castings, highly stressed castings, pressure tight castings, machine frames, motor frames, internal combustion engine parts, hand truck wheels, oil pans, and frames. Manufacturer: Birmingham Aluminium Castings Co., Ltd. Smethwick...
Journal Articles
Alloy Digest (1964) 13 (1): Al-133.
Published: 01 January 1964
...- ings which have extremely large differences in section thickness are more readily cast in this alloy than in the alloys of high copper content. Forms Available: Ingots and castings. Applications: Manifold and valve bodies, ornamental cast- ings. machine frames, motor frames, truck wheels, oil pans...
Journal Articles
Alloy Digest (1967) 16 (5): Al-166.
Published: 01 May 1967
..., sand castings and permanent castings. Applications: Mag- mold Crankcases, camshaft housings, oil pans, hand wheels, washing machine agitators, and other highly stressed castings. Manufacturer: Apex Smelting Company Division American Metal Climax Inc. Chicago, Illinois Cleveland, Ohio Los Angeles...
Journal Articles
Alloy Digest (1956) 5 (12): Al-46.
Published: 01 December 1956
...-cooled cylinder heads, piano plates and frames, gasoline and oil tanks, internal combustion and diesel engine aankcases, oil pans, rear-axle housings, castings requiring leak tight- ness and other general purpose uses. Manufacturer: Bohn Aluminum and Brass Corporation Detroit 26, Michigan ...
Journal Articles
Alloy Digest (1957) 6 (4): Al-50.
Published: 01 April 1957
..., pressure tight castings, machine frames, motor frames, inter- nal combustion engine parts, hand truck wheels, oil pans, and frames. Manufacturer: Castings supplied by many die casters. ingot supplied by metal producers and ingot smelters. ...
Journal Articles
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
... as 1500 sfpm. For cutting fluids use a mixture of lard oil and kero- sene in general machining, pure lard oil in tapping, and soluble oil in milling, sawing and drilling. Castability: Aluminum A357 is readily cast in sand and permanent molds. Ic has excellent fluidity, excellent resistance to hot cracking...
Journal Articles
Alloy Digest (1988) 37 (12): Al-293.
Published: 01 December 1988
... for remelting. Applications: TypicalusesofAA380.0comprisevacuumcleaners, floor polishers, automotive parts, motor frames and housings, gear cases, cylinder heads for air-cooled engines, lawn- mower housings, pressure-tight castings, machine frames, hand-truck wheels, oil pans and ornamental castings...
Journal Articles
Alloy Digest (1969) 18 (11): Al-192.
Published: 01 November 1969
...: Permanent mold castings and sand castings. Applications: Stressed structural parts in aircraft. automotive and machine equipment. structural castings, gear cases. gear housings, crankcases. airframe fittings. oil pans. controls, superchargers. transmission cases, instrument housmgs. Generally, where high...
Journal Articles
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... fittings, oil pans, controls, superchargers, transmission cases, and instrument housings. Manufacturer: Federated Metals Division American Smelting and Refining Co. Somerville, NJ. 08876. ...
Journal Articles
Alloy Digest (1964) 13 (10): Al-140.
Published: 01 October 1964
... and at low temper. atures is good. Fortis Available: Sand casting and ingots. Also permanent mold castings. Applications: Piano places and frames, crankcases, housings, type. writer frames, engine parts, water-cooled cylinder heads, gasoline and oil tanks, oil pans, rear-axle housings, castings requiring...
Journal Articles
Alloy Digest (1975) 24 (5): Al-215.
Published: 01 May 1975
... bodies, truck wheels. rear-axle housings, oil pans, orna- mental castings, piano plates and frames. and many general-purpose uses. Manufacturers: Aluminum alloy foundries. ...
Journal Articles
Alloy Digest (1977) 26 (1): Al-118.
Published: 01 January 1977
...-relieved conditions. Forms Available: Sand castings and ingots. Applications: Machine frames, motor housings, valve and manifold bodies, truck wheels, rear-axle housings, oil pans, ornamental castings, piano plates and frames, and many general-purpose uses. Manufacturer: Federated Metals Corporation...