Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1984) 33 (6): TS-423.
Published: 01 June 1984
..., toughness. and wear resistance. The relatively large percentage of nickel contained in this grade produces an alloy with greater toughness than the standard oil-hardening types while retaining the necessary hardness and wear resistance. NDS is well suited for cold-work applications requir- ing this extra...
Journal Articles
Alloy Digest (2014) 63 (3): SA-694.
Published: 01 March 2014
... Condition. Docol 1000 LCE is supplied in the annealed and skin passed condition. The surface can be left as is or oiled (anticorrosion oil). Applications: Typical applications are car bodies. Some examples include bumper and seat reinforcements, door beams, and side impact beams or waistline reinforcements...
Journal Articles
Alloy Digest (1979) 28 (10): TS-354.
Published: 01 October 1979
... WANDO belongs to that class of oil-hardening tool steels known as non-deforming steels. It will develop full hardness on oil quenching from a relatively low temperature with minimum volume change, hence non-deforming. It is a general-purpose tool and die steel. Among its many applications are dies...
Journal Articles
Alloy Digest (1981) 30 (2): TS-377.
Published: 01 February 1981
... GUTERL 0-1 is a nondeforming, oil-hardening, general-purpose tool and die steel. It can be oil hardened safely even in complex sections and shapes. It has a good combination of hardeness, toughness and resistance to abrasion and wear. Its many applications include dies for numerous purposes...
Journal Articles
Alloy Digest (1986) 35 (1): TS-454.
Published: 01 January 1986
... GSN is an oil-hardening, high-carbon high-chromium die steel developed for high wear and abrasion resistance. It is outstanding among non-deforming oil-hardening steels, holding size almost as well as high-carbon high-chromium air-hardening die steels. It is used on specialized applications...
Journal Articles
Alloy Digest (1985) 34 (4): Cu-495.
Published: 01 April 1985
... characteristics and can be joined by several methods. Among its many applications are air conditioners, gas lines, heater lines, oil-burner and plumbing tubes, dairy tubes and oil lines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2020) 69 (9): TS-800.
Published: 01 September 2020
... CarTech L6 is an oil-hardening, high-carbon (0.70%), nickel-chromium, alloy cold-work tool steel. It is suitable for short run tooling in applications where a combination of high hardness and good toughness is required. The relatively high nickel content results in an alloy with greater impact...
Journal Articles
Alloy Digest (1987) 36 (4): TS-473.
Published: 01 April 1987
... high toughness with the advantages of oil-hardening non-deforming steels. Its relatively high hardenability coupled with high toughness makes it extremely useful for larges shear blades in severe service. Other applications include pneumatic tools, punches, hand chisels, rivet sets and pipe cutters...
Journal Articles
Alloy Digest (1977) 26 (6): SA-334.
Published: 01 June 1977
... AISI 5147 is a low-chromium (nominally 1% chromium), intermediate-hardenability alloy steel for medium-duty applications. It is normally hardened by quenching in oil. It has a wide range of applications for transportation equipment, farm implements, tools and industrial machinery. This datasheet...
Journal Articles
Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. This datasheet provides information on composition, physical properties, tensile properties, and compressive...
Journal Articles
Alloy Digest (1981) 30 (1): TS-375.
Published: 01 January 1981
... CYCLOPS L6 is an oil-hardening tool steel recommended for any tool-steel application requiring relatively great toughness, or where intricate shapes preclude the use of water-hardening steels. It is also recommended for machine parts and other components that require an excellent combination...
Journal Articles
Alloy Digest (1983) 32 (2): TS-411.
Published: 01 February 1983
... JESSOP TRUFORM is the general-purpose, oil-hardening, non-deforming alloy tool steel for applications where dimensional accuracy is required. It shows very low distortion in heat treating and very high safety (against cracking) in hardening. Truform has deep-hardening properties, a fine-grain...
Journal Articles
Alloy Digest (1985) 34 (2): TS-435.
Published: 01 February 1985
... AIRKOOL is a high-hardenability (deep-hardening) tool and die steel that is intermediate in abrasion resistance between the oil-hardening and high-carbon high-chromium tool steels. It possesses superior toughness to both of these types; furthermore, AIRKOOL can be machined readily and has...
Journal Articles
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... LESCO S-7 is an air or oil-hardening die steel with a unique combination of toughness and wear-resistance properties that makes it an ideal choice for many tooling applications. The outstanding properties of Lesco S-7 are provided by an intermediate carbon level balanced with moderate amounts...
Journal Articles
Alloy Digest (1987) 36 (9): TS-480.
Published: 01 September 1987
... CARPENTER O6 is an oil-hardening tool steel for cold-work applications. It is designed to have free graphite in the microstructure. This free graphite is responsible for the excellent machinability of this grade. Among the many applications of Carpenter O6 are dies for various uses, punches, gages...
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
... AL TECH HURON is a cold-work tool steel developed for applications requiring high resistance to wear or to abrasion and for resistance to heavy pressure rather than to sudden shock. Because of these qualities and its good nondeforming properties, it is unsurpassed (for an oil-hardening tool steel...
Journal Articles
Alloy Digest (1977) 26 (11): CS-70.
Published: 01 November 1977
... SAE 10053 is an oil or water-hardening machinery and tool steel for applications where a shallow-hardening steel of high strength with moderate toughness meets the requirements. It is commonly used for parts where induction hardening or austempering are employed. SAE 1053 is recommended...
Journal Articles
Alloy Digest (1976) 25 (1): TS-295.
Published: 01 January 1976
... APACHE is an air-hardening, cold-work die steel that exhibits less distortion during heat treatment than water or oil-hardening steel and many other air-hardening steels. Its low-distortion characteristic makes it attractive for applications where close size tolerance is important. This datasheet...
Journal Articles
Alloy Digest (1976) 25 (6): TS-302.
Published: 01 June 1976
... BRAKE DIE is a medium-alloy tool steel heat treated at the mill by oil-quenching and tempering to develop the best combination of properties. It is used for all types of dies on hand-operated and mechanically operated press brakes for the forming and bending of sheets, strip and other flat-rolled...