1-20 of 214 Search Results for

nuclear applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1976) 25 (11): Ni-236.
Published: 01 November 1976
... is derived from the presence of hard nickel borides (and to a lesser extent chromium carbides) tightly held in a tough nickel-rich matrix. Among its many uses are cylinder liners, glass plant applications and valve components for nuclear applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1974) 23 (1): Zr-6.
Published: 01 January 1974
... Zr-3Nb-1Sn was developed to provide improved elevated temperature mechanical properties over the Zircaloys without reducing corrosion resistance. It is used in nuclear applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2019) 68 (9): SS-1309.
Published: 01 September 2019
... Sandvik 12R10L is fully austenitic with a very low cobalt content for nuclear applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength as well as fatigue. It also includes information on high temperature...
Journal Articles
Alloy Digest (1997) 46 (7): SS-688.
Published: 01 July 1997
... Tristelle Alloy 5183 is a stainless steel-base hardfacing alloy designed to replace the traditional cobalt alloys for use in nuclear-plant applications. This datasheet provides information on composition, and physical properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1996) 45 (12): SS-664.
Published: 01 December 1996
... for uses involving severe corrosive conditions. The alloy has high strength and good resistance to creep at elevated temperatures. Its many applications include the nuclear, chemical, food, paper, and textile industries. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1979) 28 (8): Co-76.
Published: 01 August 1979
... application chemical composition corrosion-resistant alloys ductility elasticity hardness heat treatability joinability machinability nuclear applications oxidation resistance physical properties tensile properties workability AU Filing Code: Co-76 ALLOY 188 cobalt Alloy OY AUGUST 1979 DIcrsTa...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
... Nickel Alloy 600 is a nickel-base alloy intended for use in a wide range of applications from cryogenic to temperatures above 2000 F, where high-temperature properties and resistance to oxidation or corrosion are desired. This alloy has been used in nuclear, petroleum, chemical, food-processing...
Journal Articles
Alloy Digest (1981) 30 (11): Cb-10.
Published: 01 November 1981
... of fabrication associated with columbium. Fansteel 80 Metal can be fabricated easily at room temperature and high-quality ductile welds are possible. Its applications include nuclear, liquid metal loops and structures for high-temperature environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (2): SS-420.
Published: 01 February 1983
... involving severed corrosive conditions. In addition, Type 316 has high strength and high resistance to creep at elevated temperatures. Its many applications include the nuclear, chemical, food, paper and textile industries. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... in chloride-containing solutions and to sodium hydroxide solutions. INCONEL Alloy 690 is useful for various applications involving nitric or nitric/hydrofluoric acid solutions, sulfur-containing gases and various types of high-temperature water such as in nuclear generators. This datasheet provides...
Journal Articles
Alloy Digest (1999) 48 (4): Mo-17.
Published: 01 April 1999
...-48 RHENIUM nuclear applications physical properties sheets space applications tubes wires thermal properties - DIGEST DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: MO-17 Molybdenum r, January 1999 b Corrected April 1999 MOLYBDENUM 4448 RHENIUM (Refractory Alloy) Molybdenum-rhenium...
Journal Articles
Alloy Digest (1997) 46 (6): Ni-528.
Published: 01 June 1997
... NUCALLOY ALLOYS 453 and 488 are nickel-base hardfacing alloys designed to replace the traditional cobalt alloys for nuclear plant applications. These alloys have been used in Japanese commercial nuclear power plant service. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2023) 72 (6): Ni-783.
Published: 01 June 2023
... 0.05 0.5 0.5 0.015 (a) Typical values unless indicated otherwise. (b) Very low Co levels are guaranteed for nuclear applications Physical Properties See Tables 1 4. Mechanical Properties See Table 5 7. Table 1 Density Temperature °C °F 20 68 Typical value kg/m3 8190 Density lb/in.3 0.296...
Journal Articles
Alloy Digest (1966) 15 (12): SS-189.
Published: 01 December 1966
... are recom- mended. For metal-arc welding use Incoloy Weiding Electrode 138; for TIG welding use Inconel Filler Metal 92 or 82 (for nuclear applications and heavy gauge material) and Incoloy Filler Metal 65 (for light gauge material); for use at high temperature applications with no risk for wet-corrosion...
Journal Articles
Alloy Digest (1983) 32 (4): Ni-285.
Published: 01 April 1983
.... It is outstanding in resistance to corrosion either general or localized (pitting/crevice), is virtually immune to chloride-ionstress-corrosion cracking, and is highly resistant to oxidation. Among its many uses are aerospace applications, heat exchangers, nuclear-reactor components and power-plant flue-gas...
Journal Articles
Alloy Digest (1982) 31 (4): Zr-7.
Published: 01 April 1982
... (except nuclear). Because of its excellent resistance to many corrosive media and its good mechanical and heat-transfer properties, Zircadyne 702 has found widespread use in many chemical process applications. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1987) 36 (1): Be-3.
Published: 01 January 1987
... BRUSH WELLMAN S-65B is a grade of beryllium strengthened by a dispersion of beryllium oxide. It has moderate strength and fairly low ductility (a minimum of 3% elongation). Its uses include optical applications, nuclear reactors, instrumentation, X-ray windows, high-speed computer parts, audio...
Journal Articles
Alloy Digest (1984) 33 (12): Ni-306.
Published: 01 December 1984
... 1982 Absence of boron allous minimal erosion of thin gauge parts being joined. The alloy is also suitable for some nuclear applications where absence of boron is a requirement. As mentioned above. the recommended brazing atmospheres are pure. dry hydrogen. inert gases. or vacuum. Because it isan...
Journal Articles
Alloy Digest (1971) 20 (11): W-17.
Published: 01 November 1971
... CRM TUNGSTEN-35 Re-18 Mo is a high-melting alloy for applications such as electronic tube components, electrical contacts, nuclear equipment, rocket thrusters, thermocouples and heating elements. All products are produced by powder metallurgy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (12): Zr-9.
Published: 01 December 1982
... in chemical applications. Zircadyne 704 is used for high-pressure, high-temperature water and steam environments such as those in the nuclear power industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes...