Alloy Digest (1958) 7 (5): SA-68.
Published: 01 May 1958
... Ferrovac-4340 is a vacuum melted chromium, nickel, molybdenum alloy steel having high endurance limit, high notched tensile strength, and high transverse ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2014) 63 (5): Ti-154.
Published: 01 May 2014
... 16.4) Typical tensile and notched tensile properties, STA condition, 0.2% yield strength, MPa (ksi) 25 °C (77 °F) 1034 1172 (150 170) 93.3 °C (200 °F) 931 998 (135 145) 204 °C (400 °F) 793 862 (115 125) 315 °C (600 °F) 758 827 (110 120) 371°C (700 °F) 689 758 (100 110) Ultimate tensile strength, MPa...
Journal Articles
Alloy Digest (1972) 21 (4): Ti-64.
Published: 01 April 1972
... FORGINGS (Heat Treatment: 1600°F, 1 hr, water quenched; 1 lOOoF, 8 hr, air cooled) LOcotiOll Notch-Tensile Strength Direction Notch-Tensile Strength/ psi Yield Strength Ratio Outer Tangential 217900 1.21 Center Tangential 218100 1.25 CenterAxial 227900 1.31 Center Diameter 235600 1.31 Center Radial 218800...
Journal Articles
Alloy Digest (1966) 15 (10): Al-159.
Published: 01 October 1966
... Notched tensile strength, psi 91100 86900 Notched-Unnotched tensile strength ratio 1.28 1.26 Test Temperature oF Longitudinal -320 -423 Transverse -320 -423 Table 2 - TYPICAL LOW TEMPERATURE PROPERTIES (T6 Temper) Notched Tensile Yield Tensile Notched-Unnotched Suer@ Suength Elongation Strength Tensile...
Journal Articles
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
... in. IS-20 Reduction of area, % 65-75 Rockwell hardness C28-30 Table 2 - TYPICAL MARAGED PROPERTIES (Annealed, then maraged at 9OOoF for 3 hours) Tensile strength, psi 265000-305000 Yield strength. psi (0.25,) 26000@300000 Elongation, % in 2 in. 3-10 Reduction of area, c*c 20-50 Notch T.S. to T.S. ratio...
Journal Articles
Alloy Digest (1990) 39 (12): SA-454.
Published: 01 December 1990
... 185700 181100 18.0 75.0 *Bars of small cross section, solution annealed 1 hr @ 1500°F, AC, aged 3 hrs @ 900°F. Copyright © ASM International® 1996DOI: 10.31399/asm.ad.sa0454 Table 4 -EFFECT OF STRESS CONCENTRATION FACTOR, Kt, ON TENSILE STRENGTH* Notch Tensile Strength Notch-to-Smooth Average Raw Tensile...
Journal Articles
Alloy Digest (1972) 21 (11): SS-282.
Published: 01 November 1972
... 285 Table 2 - SPECIFICATION REQUIREMENTS MET BY VARIOUS HEAT TREATMENTS Property Tensile strength, psi Yield strength (0.2% offset), psi Elongation (2 in % Reduction of area, % Izod impact, ft-lb Charpy impact (V-Notch), ft-lb Brinell hardness Heat Treatment 1925oF, oq; 18500F, oq; 19OOoF, oq; temper...
Journal Articles
Alloy Digest (1992) 41 (3): SA-314.
Published: 01 March 1992
... Orientation Property Longitudinal Tensile strength, psi 226000 h4Pa 1559 Yield strength (0.2% offset) psi 188000 MPa 1297 Elongation (4D), % 13.0 Reduction of area, % 58.3 Charpy V notch impact (8 samples) Average, ft-lb 26 Joules 35 Range, ft-lb 24l29 Joules 33139 Hardness, Rockwell C 45 *5 l/2 square; 1/2h...
Journal Articles
Alloy Digest (1965) 14 (4): SA-30.
Published: 01 April 1965
.... Table 9 - COMPARATIVE ROOM & LOW TEMPERATURE PROPERTIES (3; Rd. - oil hardened from 1550 F., tempered at 550°F.) Unootched Notched 7O*F -320°F. 70°F. 283000 294000 - Tensile strength, psi 231500 Yield strength, psi (0.2%) 196200 Elongation, % in 1.2 11.6 Elongation, c/c in x Reduction of area, % 44...
Journal Articles
Alloy Digest (1959) 8 (3): SA-81.
Published: 01 March 1959
... 32.0 :Eii: 17.5 3 2: 10.0 23:0 Table 2--TYPICAL MECHANICAL PROPERTkS- FORGING (Quenched in oil and tempered at 500°F.) I.ongitudinai Tensile strength. psi 297000 Notch tensile strength psi 303000 Yield strength, psi (0.2%) 242000 Elongation, % in 2 Reduceon of are& 70 2 cllarpy impa& ft. lbs. (V-notch...
Journal Articles
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... modulus, typical, 20 25 °C 107 (15.5) (68 78 °F), GPa (106 psi) approximate Shear modulus, typical, 20 25 °C 46 (6.7) (68 78 °F), GPa (106 psi) Notched tensile strength, Kt = 3 Air cooled and aged 1.4 1.64 × actual tensile strength Oil quenched and aged 1.33 1.52 × actual tensile strength See also Tables...
Journal Articles
Alloy Digest (1958) 7 (10): SA-76.
Published: 01 October 1958
... 34100 DOI: 10.31399/asm.ad.sa0076 Copyright © ASM International® 1996 Table 5 - FATIGUE RESISTANCE (Under rotary bending conditions) Normalized As Rolled Plain Notched Plain Notched Tensile strength, psi 90300 EE 100200 102500 Fatigue suength, psi 5 3700 56700 35800 Fatigue-Tensile ratio 0.60 0.32 0.57...
Journal Articles
Alloy Digest (1966) 15 (4): SA-193.
Published: 01 April 1966
... Hardness 575 555 540 525 500 425 Longitudinal Transverse Tensile strength, psi 277000 276000 Notch tensile strength, psi 303000 262000 Yield strength, psi (0.2%) 242000 237000 Elongation, % in 2 8.0 4.0 Reduction of area, % 23.0 7.4 Charpy impact, ft. Ibs. notch) 18 7 DOI: 10.31399/asm.ad.sa0193 Copyright...
Journal Articles
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... specimens unmachined with casting skin intact. As-cast specimens tested 1-3 days after casting. Standard ?4-in. diameter tensile specimens and standard Charpy impact specimens with cast-in V-notch) Tensile strength, psi Yield strength (0.2% offset), psi Elongation (2 in % Brinell hardness Charpy impact, ft...
Journal Articles
Alloy Digest (2001) 50 (2): SS-818.
Published: 01 February 2001
...) Tensile strength Yield strength, 0.2% Notched tensile strength, Kt = 3.0 Billet size, in. Specimen orientation MPa ksi MPa ksi Elongation in 4D, % Reduction in area, % MPa ksi Notch strength ratio 8 RCS Transverse 1365 198 1096 159 21 71 2186 317 1.60 8 RCS Transverse 1379 200 1076 156 20 70 2193 318 1.59...
Journal Articles
Alloy Digest (2005) 54 (7): SA-547.
Published: 01 July 2005
... in. Longitudinal 43.5 1437 208.4 1397 202.6 11.6 58.8 square Transverse 43.9 1427 206.9 1380 200.1 8.9 41.7 0.250 in. Transverse 42.9 1504 218.1 1469 213.0 11.0 45.0 sheet Table 2 Effect of Stress Concentration Factor, Kt, on Tensile Properties Notch tensile strength Notch-to-smooth Average Range tensile strength...
Journal Articles
Alloy Digest (2001) 50 (7): Ti-116.
Published: 01 July 2001
... (68 °F) 910 (132) 600 °C (1112 °F) 450 (65) Elongation, 5D, minimum, % 20 °C (68 °F) 6 600 °C (1112 °F) 9 Reduction in area, minimum, % 20 °C (68 °F) 15 600 °C (1112 °F) 20 Notched tensile strength, Kt = 3, minimum, 20 °C (68 °F) 1.45 × actual tensile strength Fracture toughness, KIc, minimum, 20 °C...
Journal Articles
Alloy Digest (1968) 17 (11): CS-28.
Published: 01 November 1968
... Lukens LT-75HS is a quenched and tempered, fine grain, notch-tough, carbon steel having good impact and notch-toughness properties. It is engineered specifically for use in pressure vessel and structural applications requiring high strength properties and guaranteed notch toughness. This datasheet...
Journal Articles
Alloy Digest (1972) 21 (4): SS-271.
Published: 01 April 1972
... in Figure 2 for specimens given the recommended solution treatment, then aged for four hours at various temperatures. It shows that smooth bar tensile and yield strengths peak slightly between aging temperatures of 100~1050oF (538.566oC). Notch tensile strength peaks between 1025.1075oF (552.58OoC) while...
Journal Articles
Alloy Digest (1986) 35 (8): SA-422.
Published: 01 August 1986
... ANNEALED PROPERTIES Tensile strength. psi 140000 Tabte g- EFFECT OF STRESS CONCENTRATION FACTOR, Kt, ON TENSILE STRENGTH* Yield strength (O.&G- offser. psi IooooO Elongation (4.5~ A). qc 21 Reduction of area. yc 92 Rockwell C hardness 27-29 KI Notch Tensile Strength Avg Notch Smooth Average Range Tensile...