Alloy Digest (1990) 39 (1): SA-444.
Published: 01 January 1990
... 6260,6267. ASTM A29, A322, A33 1. General Characteristics: SAE 9310 is a tough carburizing steel. Fig. 1 shows a comparison of Charpy V-notch impact at various test temperatures as compared to that of AISI 8620 steel. The steel has good fatigue characteristics. Compressive stress (calculated by the Hertz...
Journal Articles
Alloy Digest (1964) 13 (11): SA-170.
Published: 01 November 1964
... (Austenitited 1650oF, water quenched, tempered) _ . . Brine11 Hardness 350-375 300-325 Tempering Charpy Impact ft. lbs., (V-notch) at Test Temperature of Temperature OF R.T. OoF -800F -1200F 1050 80 80 65 55 1150 110 105 105 75 Heat Treatment: Anneal: Heat to 16500F and furnace cool. Harden: Heat to 1650oF...
Journal Articles
Alloy Digest (1962) 11 (4): SA-127.
Published: 01 April 1962
... COLTUF 28 is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1989) 38 (7): P-6.
Published: 01 July 1989
...) Elongation at yield ASTM D638 Dry 9% 10 Conditioned % 10 Elongation at break ASTM D638 Dry % 115 Conditioned % 210 Flexurai strength at yield ASTM D790 Dry PWW Conditioned psi(Mpa) Eig; Flexurai modulus ASTM D790 Dry Psi(Mpa) 300000(2068) Cord tioned psi0 180000(1241) Impact strength, notched ASTM D256 Dry...
Journal Articles
Alloy Digest (1990) 39 (3): P-16.
Published: 01 March 1990
...) Flexural modulus 0.125 (3.2mm) Compressive strength Compressive modulus Shear strength, yield Shear modulus hod impact strength Notched, 0.125 (32mm) 73 F(23 C) Unnotched, 0.125 (32mm) 73 F(23OC) Tensile impact strength, S type Falling dart impact strength, l/8 thick Fatigue strength @ 2.5 x 106 cycles...
Journal Articles
Alloy Digest (1993) 42 (1): TS-515.
Published: 01 January 1993
... 0.012-.04 0.30- 1 P.20-P-30 330490 loo-150 Finish Turning 0.08 max. 2max 0.012 max 0.30max P-10 460-690 140-2 10 DOI: 10.31399/asm.ad.ts0515 Copyright © ASM International® 1996 t 54 HARDNESS tic 51 I L I I I I I 1 200 500 800 1100 Tempering Temp + OF t IMPACT ;TRENGTH (Chaw U Notch) FLUS. 20 Fig. 1...
Journal Articles
Alloy Digest (2008) 57 (10): SA-586.
Published: 01 October 2008
... for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 CustomerService@asminternational.org Fax 440-338-4634 www.asminternational.org TIMKEN® IMPACT STEEL DOI: 10.31399/asm.ad.sa0586 Table 2 Typical transverse Charpy v-notch impact toughness...
Journal Articles
Alloy Digest (1989) 38 (6): P-4.
Published: 01 June 1989
... strength ASTM D 638 Elongation at yield ASTM D 638 Psi O$Ql Elongation at break ASTM D638 % FIexuraI strength ASTM D790 psi 0 Flexural modulus ASTM D790 psi (MPa) Izod impact strength, notched ASTM D256 At 73OF (23°C) ft-lb/in (J/m) At -4OF (-20°C) ft-lb/m (J/m) Hardness Shore D __ Value 7300 (50) 10 10400...
Journal Articles
Alloy Digest (1967) 16 (12): Ti-53.
Published: 01 December 1967
... area, % 20 min. Charpy impact, ft. lbs. (V-notch) @ -80°F 25 YP. Rockwell hardness c31 vp. Tensile yield strength, psi (0.2%) 95OOomin. Table 2 - TYPICAL ELEVATED TEMPERATURE PROPERTIES Test Tensile Yield Reductioa Temperature suengdl Strength E loagacioa of Area OF psi psi (0.2%) % in 2 % 600 85000...
Journal Articles
Alloy Digest (1970) 19 (8): SA-255.
Published: 01 August 1970
... HY-100 is a low-carbon, hardenable alloy steel for ultra-service applications requiring excellent notch toughness and high strength. It can be welded to provide tough weldments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (1968) 17 (4): TS-204.
Published: 01 April 1968
... F C As-quenched 56-58 400 54-56 500 54-56 600 54-56 700 53-54 Charpy Impact (V-notch) fr. lbs. 19-20 18-19 15-16 15-16 NOTE: The hardness values given in the above table are represenca- tive. Variations in size, conditions of heat rreatmenr and method of cooling may cause slight deviations from...
Journal Articles
Alloy Digest (1952) 1 (2): SA-2.
Published: 01 October 1952
... B95 B94 Bl10 Tablo 3 AVERAGECHARPY IMPACT TESTS (Specimau machined from 3 rounds, keyhole notch) Longitudinsl T-C Loll- Normslied 1575 F. Nomalized 1575 F. Normalid 157S F Tempered 1oWF Tempered 10So°F Room at Brind Room at Bridl Room at Brinell Temp. -320°F Hardness Temp. -32O F Hardness Temp...
Journal Articles
Alloy Digest (1975) 24 (10): TS-291.
Published: 01 October 1975
.... Quenched 1 60 2 59 4 56 6 52 Illllllllllllill~ 100 200 a00 400 SW wo 700°c I I I 1 I I I I 200 400 600 800 loo0 12OOOF Tempering temperature Fig. 1 Room-temperature Charpy V-notch impact data on l-inch diameter bars hardened in oil from 16900F and tempered as shown. Oil Martemper Quenched Treatment 58 53...
Journal Articles
Alloy Digest (1991) 40 (11): TS-507.
Published: 01 November 1991
... die steel at a working hardness of 49150 Rc has superior thermal fatigue resistance to H13 tool steel at a working hardness of 46147 Rc. Its Charpy V notch impact toughness is also superior to that of H13 tool steel. Forms Available: Bar, billet, other forms on request. Applications: Hotworking...
Journal Articles
Alloy Digest (1965) 14 (4): SA-30.
Published: 01 April 1965
... combines high tensile strength and good ducrility with relatively high impact strength and hardness. It possesses Iow notch sensitivity at relatively high hardness. Test data by independent laboratories indicate that Hy-Tuf has better notched bar strength, better ductility, better notched tensile strength...
Journal Articles
Alloy Digest (1993) 42 (3): SS-541.
Published: 01 March 1993
... 35 Reduction of area, % 35 55 Hardness, Brinell 230 max. 217 Impact strength, Charpy V-notch ft. lbs. (Joules) 40 (53) Charpy V-notch impact resistance at -100°F (-73°C) 75 ft-lbs (1OOJ) 110 ft. lbs Table 2 - TYPICAL TENSILE PROPERTIES OF ESCOLOY 45D AND IN-625-TYPE WELD DEPOSITS ENiCrMo3 ERNiCrMo3...
Journal Articles
Alloy Digest (1963) 12 (3): TS-131.
Published: 01 March 1963
... elasticity, psi x 10 29-O-30.0 PROPERTIES Table 1 - TYPICAL HARDNESS DATA AFTER TEMPERING (Air cooled from 1550oF and tempered) (4 square section) Rockwell Hardness Tempering Temperature oF As-hardened Table 2 - RELATIVE TOUGHNESS DATA (C-Notch Charpy impact specimen with radius, heared 1 hr. 16OOoF, air...
Journal Articles
Alloy Digest (1959) 8 (10): SA-90.
Published: 01 October 1959
... strength, psi 96000 Yield point, psi 71000 Brinell hardness 200 Table 3- TYPICAL IMPACT PROPERTIES ( 1 Rd., heated to 1475 F., quenched in oil and tempered) Rockwell Hardness C J Distance Rockwell C Tempering Charpy Impact Izod Impact Temperature Unnotched Notched-Square Section OF. ft. Ibs. ft. Ibs...
Journal Articles
Alloy Digest (1978) 27 (2): SA-343.
Published: 01 February 1978
...% 230000 183000 14.0 45.9 5% 232000 194000 15.0 525 5% 230000 190000 15.0 51.7 *RCS = Round-Cornered Square. Table 2 - TYPICAL TRANSVERSE CHARPY V-NOTCH IMPACT DATA AT ACTUAL CENTER. (AlI specimens homogenized 17000F, austenitized 1525oF, quenched, and tempered 2 + 2 hours at 1OOOoF) Size of RCS Charpy...
Journal Articles
Alloy Digest (1960) 9 (9): SA-103.
Published: 01 September 1960
... surface hardnesses. Table 3 - HARDENABILITY DATA ( J distance in l/16 inch) J. Distance Rockwell c 6: 6: 6: 6; 6; 12 G ii 57 Brinell Hardness 7.84 0.283 0.11 0.102 22.3 30.0 6.5 Normalized 150000 100000 2 302 Izod Impact ft. lbs. notched 444 11 363 34 293 47 363 (388) 311 (340) 255 (269) 293 (363) 262...