Journal Articles
Alloy Digest (1958) 7 (12): SS-82.
Published: 01 December 1958
... TIMKEN 16-13-3 STEEL is an austenitic, non-magnetic alloy steel having high creep and rupture strength, and high oxidation resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1964) 13 (10): SA-169.
Published: 01 October 1964
... approximate- ly equal to that of mild steel. DOI: 10.31399/asm.ad.sa0169 Copyright © ASM International® 1996 Specification Equivalents: ASTM Al28 MIL-S-17758A General Characteristics: RoI-Man is n tough, non-magnetic alloy steel in which the usual hardening transformation during heat treatment has been...
Journal Articles
Alloy Digest (1974) 23 (4): SS-295.
Published: 01 April 1974
.... This alloy is also used in high-strength non-magnetic applications because it remains essentially non-magnetic even after severe cold working. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1970) 19 (8): SS-11.
Published: 01 August 1970
... RA-330 is an austenitic, non-magnetic, corrosion and heat resisting, high nickel-chromium alloy steel. It does not respond to any heat treatment for hardening. It has a greater resistance to heat and thermal shock than the other grades of austenitic steel. This datasheet provides information...
Journal Articles
Alloy Digest (1957) 6 (11): Ni-37.
Published: 01 November 1957
... Type HW is a nickel-base alloy containing chromium and iron. It is austenitic, non-magnetic, and has exceptionally high resistance to corrosion, cyclic heating, and oxidation. It is of the 60 Ni-12Cr type alloy. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2022) 71 (6): SS-1348.
Published: 01 June 2022
... ATI 219, also known by the more familiar 21-6-9 or XM-11 designations, is a nitrogen-bearing austenitic stainless steel that has substantially higher strength than the standard austenitic stainless steels. The alloy remains non-magnetic even after substantial cold forming and exposure to subzero...
Journal Articles
Alloy Digest (1954) 3 (12): SS-21.
Published: 01 December 1954
... DURALOY HU is an austenitic, non-magnetic chromium nickel alloy steel having high corrosion and heat resistance. It is of the 39 Ni-19 Cr type alloy, similar to ACI-HU. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1980) 29 (10): SS-376.
Published: 01 October 1980
... AL Tech 6X is an austenitie (non-magnetic) alloy developed for service in pitting environments containing chlorides. It was designed for resistance to pitting and crevice corrosion encountered in seawater, pulp and paper manufacture, petroleum refineries, chemical process equipment and sour oil...
Journal Articles
Alloy Digest (1962) 11 (2): SS-128.
Published: 01 February 1962
... DURALOY HT is an austenitic, non-magnetic corrosion and heat resistant alloy steel, having high resistance to thermal shock. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (1962) 11 (11): Ni-76.
Published: 01 November 1962
... Durco D-10 is a nonferrous, non-magnetic alloy containing nickel and chromium totaling about 80%. It is recommended for corrosion resisting castings where a higher corrosion resistance is required than that of stainless steel. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1953) 2 (6): SS-8.
Published: 01 June 1953
... CYCLOPS 17A Metal is a nickel-chromium austenitic alloy steel intended for uses where good general corrosion resisting, heat resisting and non-magnetic properties are of importance. It shows good resistance to scaling at temperatures up to 1500 F and has excellent physical properties and fatigue...
Journal Articles
Alloy Digest (1959) 8 (6): SS-89.
Published: 01 June 1959
... HOSKINS 502 is an austenitic, non-magnetic, high nickel-chromium alloy steel recommended for use on mechanical applications requiring high resistance to heat, corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1979) 28 (1): SA-353.
Published: 01 January 1979
... LOCORE M45 is a cold-rolled, non-oriented electrical steel used primarily for alternating current (AC) and direct current (DC) motors, generators and transformers. It is produced either semiprocessed (the consumer anneals to produce the desired magnetic properties) or fully processed (the steel...
Journal Articles
Alloy Digest (1978) 27 (6): SA-347.
Published: 01 June 1978
... LOCORE M43 is a cold-rolled, non-oriented electrical steel used primarily for alternating current (AC) and direct current (DC) motors, generators and transformers. It is produced either semiprocessed (the consumer anneals to produce the desired magnetic properties) or fully processed (the steel...
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
.... New Jm JESSOP No. 200 (Manganese-Nickel Alloy Steel I JESSOP No. 208 is a non-magnetic, austenitic steel developed especially for the electrical industry. It has low magnetic per- meability and high electrical resistance. Jessop NO. 200 is ideal for a great number of applications requiring low perme...
Journal Articles
Alloy Digest (1967) 16 (9): Co-52.
Published: 01 September 1967
... Covandur is a free-machining iron-cobalt-vanadium alloy designed for use in electrical equipment in which high magnetic permeability at very high flux densities is essential. This datasheet provides information on composition and physical properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1991) 40 (4): SA-457.
Published: 01 April 1991
... JESSOP No. 9, super high tensile steel, is one of the toughest and most wear resistant steels of its class in existence. Primarily developed as a high tensile, non-magnetic armor plate, it has since been widely used for equipment subject to severe battering. This datasheet provides information...
Journal Articles
Alloy Digest (1994) 43 (3): Fe-106.
Published: 01 March 1994
... NK SUPER-E CORE is a non-oriented silicon steel plate containing 6.5% Si with enhanced magnetic characteristics. Higher silicon level is attained by addition to existing silicon steel plate. This datasheet provides information on composition and physical properties. It also includes information...
Journal Articles
Alloy Digest (1965) 14 (2): Co-42.
Published: 01 February 1965
... is vanadium rich and non-magnetic. The precipitation of the second phase is associated with both a physical and magnetic hardening. Forms Available: Hoc rolled bar or sheet, cold rolled chin cape and drawn wire, cold rolled scrip, hoc rolled place, and forgings. Applications: This alloy can be readily hoc...
Journal Articles
Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
... is a non-hardenable austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Better machin- ability than that of standard AISI Type 316 stainless is obtained by the use of balanced chemistry and special manufacturing techniques. This grade is non-magnetic in the annealed...