Alloy Digest (1957) 6 (7): Cu-52.
Published: 01 July 1957
... NICKEL SILVER, 65-12 is a copper-nickel-zinc alloy having excellent workability, weldability and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (10): Cu-242.
Published: 01 October 1971
... Montclair. New Jew COPPER ALLOY No. 757 (Nickel Silver 65-12) COPPER ALLOY No. 757 is a copper-zinc-nickel alloy having excellent cold working properties and good corrosion resistance. Composition: Copper Nickel Manganese Iron Lead Total other impurities zinc Physical Constants: 63.5-66.5 11.0-13.0 0.50 max...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (9): Ag-2.
Published: 01 September 1956
... 65500-68500 28000-34000 50000-55000 Yield strength, psi (0.2%) 53500-56500 Elastic limit, psi (0.2%) Elongation, % in 2 4350E!500 30-40 b 60-65 (15T) 5t:O (301) Rockwell hardness Electrical conductivity, %IACS 66.g9.5 (301: 70 70 Table 2 - PROPERTIES OF AIR HARDRNED ALLOY AT ELEVATED TEMPERATURES (0.27...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (11): Ni-140.
Published: 01 November 1968
... (at 25°C) 800 Thermal coef. expansion/c (20-200°C) 13.3 x 10-6 Temperature coef. resistivity/oC (-65 to +150X) 0 x 5 x 10B6 Max. thermal emf. vs. copper, millivolts/ C (-65 to +150X) to.003 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES (Heat treated) Tensile strength, psi 130000-180000 Elongation...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (12): Al-230.
Published: 01 December 1977
...), psi 22000 23000 Elongation (2 in Z 2.0 5.0 Brine11 hardness (500.kg load, 1 O-mm ball) 65 70 Fatigue strength (5 x 108 cycles), *psi 10000 11000 *R.R. Moore type specimens. Table 2 - EFFECT OF TEMPERATURE ON HARDNESS AND TENSILE PROPERTIES (Condition: TS remwr1 Temperature Brine11 Hardness oF (SOO/ I...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (5): Cu-743.
Published: 01 May 2006
... for 2 h; results obtained from 25 mm rolled bar Table 2 Typical Mechanical Properties Alloy Comparison Yield strength, 0.2% Tensile strength MPa ksi MPa ksi Elongation on 5.65 _ So, % Hiduron 130, to DTD 900/4805 680 99 880 128 12 Hiduron 191 510 74 800 116 25 Nickel aluminum bronze to DGS 1043 310 45...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (7): Cu-143.
Published: 01 July 1964
... 55000 22 20 235 103000 82000 11 40 260 115000 90000 2.5 50 270 12oooo 96000 1.5 80 285 128000 101000 1.0 90 300 130000 113000 0.5 Table 3 - EFFECT OF .4GE HARDENING AT 750°F ON VICKERS HARDNESS Cold Reduction .4ged .4ged Aged Aged Aged % 2 hrs 4 hrs 12 hrs 16 hrs 24 hrs 0 190 315 430 440 450 10 310 420...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (8): Cu-707.
Published: 01 August 2003
... Tensile strength Yield strength, 0.2% offset Minimum bend radius Temper MPa ksi MPa ksi Elongation, 50 mm, % Hardness, HV Bad way Good way R480 480 550 70 80 250 36 12 R540 540 620 78 90 450 65 4 R600 600 690 87 100 550 80 2 R700 700 800 102 116 660 96 1 H115...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (5): Ni-34.
Published: 01 May 1957
...%) Elongacios % in 2 2YEim 3sTsF0 85000.115000 Reduaionofurp,% 70-55 sY:F 70-50 Brin+ hiudness (3000/10/30) 110-140 65-50 k lhs. 12%2 13Z70 160-240 187 1% 800 :Ei :z 1800 bndidon cold drawn . - ;4$%7;; zz~~ 81000-100000 84500-105000 Table 4 - l DFSION IMPACT FROFERTES ft. Ihs. fLll?s. per q. in. -dg 3 iit...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (2): Cu-185.
Published: 01 February 1968
.... Workability: Specification Equivalents: ASTM B122 Alloy 4 ASTM B151-B ASTM B206-B General Characteristics: High resistance to corrosion and tarnish, and has high fatigue resistance. This alloy has a yellower color than the nickel silver 65-18 type and does not form as easily, but possesses greater strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (12): Fe-142.
Published: 01 December 2007
... strength Young s modulus Condition Hardness, HV MPa ksi MPa ksi Elongation on 50 mm, % GPa 106 psi Annealed 140 315 46 510 74 30 145 21 Quarter hard 180 450 65 580 84 17 Half hard 205 600 87 670 97 10 Values depend on the thickness and application. Table 3 Deep Drawing Thickness, mm Erichsen cupping index...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (7): W-5.
Published: 01 July 2000
... °C (68 1472 °F) 5.05 (2.81) Thermal conductivity, W/m · K (Btu/ft · h · °F) 137 (79.2) Electrical resistivity, µ · m ( circular-mil/ft) 0.1078 (65) Electrical conductivity, 106 S/m (%IACS) 9.3 (16) Magnetic residual induction Nil Coercive force Nil Mechanical Properties: Tensile strength, MPa (ksi...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (3): Ni-122.
Published: 01 March 1967
... or zinc. It has fair co poor resistance co endo- thermic atmospheres, fair co good resistance co exo- chermic atmospheres, and excellent resistance co hydrogen or cracked ammonia atmospheres. ASTM B344-65 ASTM B267-65 Fed. QQ-R-175 General Characteristics: Chromic-C is nickel-base electrical resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (8): Fe-58.
Published: 01 August 1979
.... *TECHALLOY is a registered trademark of Techalloy Company, Inc. Composition: Carbon Manganese Silicon Nickel Iron 8-E 0:12 36.0 Remainder Physical Constants: Density, lb/cu in. Specific gravity Melting point, oF Specific heat, Btu/lb/oF (77-2120F) Thermal coef. expansion/OF (0 to 3500F) oc y to 175OC...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (11): Cu-642.
Published: 01 November 1999
... or forming. The strength level will be roughly doubled by opti- mum heat treatment. Age hardenable temper designations are as follows: ASTM designation Description Name TB00 Annealed A TD01 Quarter hard 14 H TD02 Half hard 12 H TD04 Hard H Heat Treated Tempers. These tempers describe the resulting strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (9): Cu-514.
Published: 01 September 1986
... Annealing: Heat to 850 F. hold at temperature for 1-3 hours. air cool. Hardening: This alloy can be hardened by cold working. Machinability: Copper Alloy No. C67300 has a machinability rating of about 65 to 85 where Free-Cutting Brass equals 100; the range in machinability corresponds to the wide range...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (9): Cu-219.
Published: 01 September 1970
... Brass (the most susceptible) is rated at 1000 with immunity being represented by 0; ratings of various alloys including Alloy 688 are as follows: .Alloy 260 Cartndge Brass 1000 Alloy 766 57-12 Nickel Silver 300 4Uoy 230 85-15 Red Brass 200 4lloy 770 55-18 Nickel Silver 175 Alloy 4 11 Tin Brass (9.5% Zn...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (8): Cu-79.
Published: 01 August 1959
...) (Hardened at 750°F.) Time in Hours No Gold Work 80 % Reduction i! 97-100 30 300-320 450 6 375 480 9 415 495 12 435 510 15 450 515 :Y 465 70 521 18 24 475 524 Table 5 -EFFECT OF AGING TEMPEIUTURE ON VICKERS HARDNESS (Samples had no cold work before hardening) (Hardness for Various Times at Indicated...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (4): Ni-41.
Published: 01 April 1958
... necessary ro produce bright wire.) DOI: 10.31399/asm.ad.ni0041 Copyright © ASM International® 1996 Table S-TENSILE STRENGTH AT VARIOUS TEMPERATURES (CStilUS) iii2 1292 1472 hii 700 800 1652 900 20000 7.5 83 :Ei 12 15 0 1: 2012 6000 20.0 18 Heat Treatment: ANNXWING: Heat to 1600-2000 F., air cool or water...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (3): Fe-12.
Published: 01 March 1957
..., elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Fe-12. Producer or source: Allied Products Division. Producer or Source: Allied Products Division Copyright © ASM International® 1996...