1-20 of 276

Search Results for nickel powder

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2007) 56 (4): Ni-648.
Published: 01 April 2007
... Nistelle Super C is a nickel-base powder metallurgy alloy designed for corrosion resistance and developed for coating and overlaying purposes. The composition of Nistelle Super C, Ni-23Cr-18Mo, is similar to that of the traditional Nistelle alloy, which is Ni-16Cr-16Mo-4.5W, but the higher...
Journal Articles
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
... DELORO 15, 21, 22, and 25 are prealloyed, gas-atomized, nickel-base powders for repair of glass-forming molds. This datasheet provides information on composition, physical properties, and hardness. It also includes information on powder metal forms. Filing Code: Ni-689. Producer or source...
Journal Articles
Alloy Digest (1976) 25 (4): Ni-225.
Published: 01 April 1976
... METCO 447 is a nickel-aluminum-molybdenum powder developed to produce self-bonding, low-shrink, moderately hard coatings. It is recommended for resistance to wear and particle erosion, and for the buildup and salvage of both machinable and grindable carbon steels. It is applied in a one-step...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-555.
Published: 01 July 1999
... Crucible P/M N625 is a powder metallurgical nickel-base alloy with excellent corrosion resistance, high strength, chemical homogeneity, and thermal stability. Applications include use for highly corrosive situations in the marine, nuclear power, pulp and paper, and chemical process industries...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-504.
Published: 01 March 1996
... joinability machinability oxidation resistance physical properties powder metal products thermal properties I Filing Code: Ni-504 A a1 m Nickel Alloy COLMONOY@ NCI. 21 1 c t a- March 1996 -u DATA ON WORLD WIDE METALS AND ALLOYS - D/GE3 CCopy+@w 1996, AS.4 Inremarkmal. AU nghrs...
Journal Articles
Alloy Digest (1967) 16 (7): Ni-125.
Published: 01 July 1967
... powders into green scrip. This green strip is sintered and hot rolled under a pro- tective hydrogen atmosphere. It is fully dense and has typical mechanical properties for nickel (similar to mild steels). It is ductile and has excellent workability and formability. SG-100 has interesting magnetic...
Journal Articles
Alloy Digest (2018) 67 (1): SA-809.
Published: 01 January 2018
... Ancorsteel FLD-49HP is a nickel copper-molybdenum alloy steel powder developed for high-performance sinter-hardening applications. This alloy conforms to MPIF Material standard 35, designation FLDN4C2-4905. The nickel and copper are diffusion-alloyed to the molybdenum pre-alloyed powder during...
Journal Articles
Alloy Digest (1984) 33 (8): Ni-301.
Published: 01 August 1984
... NICKEL 290 is a high-purity grade of nickel made by a powder-metallurgy process. Its high purity makes it useful for electronic applications such as components of hydrogen thyratrons and for battery applications. The low annealing temperature of Nickel 290 makes it superior to other forms...
Journal Articles
Alloy Digest (2010) 59 (3): CS-153.
Published: 01 March 2010
... is atomized into irregular, homogeneous particles that are then annealed to produce uniform, dependable steel powders. Ancorsteel 50 HP is an ideal base powder for a wide range of nickel-copper and chromium-manganese hybrid alloy systems. This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (1975) 24 (9): Ni-221.
Published: 01 September 1975
... TRIBALOY T-700 consists of a hard, intermetallic phase in a softer, nickel-base matrix. It can be cast or hardfaced. As alloy powder it can be plasma sprayed or blended with other powders for P/M (Powder/Metallurgy) processing. It combines outstanding wear and corrosion resistance for use in pumps...
Journal Articles
Alloy Digest (1977) 26 (3): Ni-242.
Published: 01 March 1977
... COLMONOY No. 22 is a nickel-base alloy supplied as atomized powder, welding rod and investment castings. The powder is applied with Colmonoy's FUSEWELD process to repair cast-iron parts. The investment castings are used in the glass industry as forming tools (plungers, baffles and sleeves...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-495.
Published: 01 January 1996
... Colmonoy No. 635, a Nickel-base hard surfacing Alloy, contains a formulated mixture of both crushed and atomized powders. It achieves a hardness of RC 58-63 with tungsten carbide particles. Typical applications include hardfacing of pump components and shaft sleeves. It is supplied as a powder...
Journal Articles
Alloy Digest (1973) 22 (11): Ag-7.
Published: 01 November 1973
... wear and the electrical and thermal con- ductivity demanded for the application. They are powder metallurgy products. Composition: (Nominal) Ag-Ni-Con 2 Ag-N&Con 3 Ag-Ni-Con 4 Ag-Ni-Con 6 Ag-Ni-Con 8 Silver 90 85 80 70 60 Nickel 10 15 20 30 40 Physical Constants: Ag-Ni-Con 2 Ag-Ni-Con 3 Ag-Ni-Con 4 Ag...
Journal Articles
Alloy Digest (1974) 23 (6): Ni-205.
Published: 01 June 1974
... COLMONOY No. 62SA comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Colmonoy No. 62SA is supplied as atomized powder for application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (7): Ni-206.
Published: 01 July 1974
... fused deposits of Colmonoy No. 69. If used loose. they will cut the nickel matrix before the chromium carbides. giving the surface an etched appearance. Apply with a steady pressure and avoid overheating. Deposition and Fusing of Metal Powder: Colmonoy No. 69 Powder is apphed by use of the Spraywelder...
Journal Articles
Alloy Digest (1974) 23 (9): SA-308.
Published: 01 September 1974
..., microstructure, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on heat treating, machining, and powder metal forms. Filing Code: SA-308. Producer or source: International Nickel Company Inc.. Producer or Source: International Nickel Company...
Journal Articles
Alloy Digest (1975) 24 (5): Ni-217.
Published: 01 May 1975
... ductility elasticity galling resistance heat resistance heat treatability impact strength machinability physical properties powder metal products Rockwell hardness tensile properties wear resistance workability All mr COLMONOY No. 5 Filing Code: Ni-217 Nickel Alloy MAY 1975 DICESTfl - DATA...
Journal Articles
Alloy Digest (1975) 24 (6): Ni-218.
Published: 01 June 1975
... they are embedded in a cast-iron or steel wheel. Used loose, they will cut the nickel matrix before the chromium carbides, giving the surface an etched appear- ance. Apply with steady pressure and avoid overheating. Application Method: The Spraywelder is used. With this special powdered metal spraying tool...
Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... galling resistance heat resistance heat treatability impact strength joinability machinability physical properties powder metal products Rockwell hardness tensile properties wear resistance workability COLMONOY No. 4 Filing Code: Ni-222 Nickel Alloy DECEMBER 1975 DIGEST b9 - DATA ON WORLD...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-227.
Published: 01 May 1976
... they will cut the nickel matrix before the chromium borides and carbides, giving the surface an etched appearance. Apply with steady pressure and avoid overheating. Copyright © ASM International® 1996DOI: 10.31399/asm.ad.ni0227 Application Method: The Spraywelder is used. With this special powdered metal spray...