1-20 of 30 Search Results for

nickel copper cast alloy 410

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1963) 12 (8): Ni-85.
Published: 01 August 1963
... Nickel Copper Cast Alloy 410 is one of the most useful cast materials to withstand corrosives encountered in industry. It has tensile strength comparable to cast carbon steel and gives good performance under conditions of abrasion and erosion. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1975) 24 (1): Ni-214.
Published: 01 January 1975
... Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1962) 11 (8): Ni-73.
Published: 01 August 1962
... MONEL alloy 506 is an intermediate cast nickel-copper alloy that has higher hardness than cast Monel alloy 410 and better machinability than Monel alloy 505. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1976) 25 (11): Cu-322.
Published: 01 November 1976
... Copper Alloy No. 973 is a cast leaded nickel brass containing 12% nickel; it is and has been known commercially as 12% Leaded Nickel Silver. It has a pleasing whiteness and high resistance to corrosion. Among its many uses are ornamental and decorative applications and marine hardware...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-85.
Published: 01 August 2000
... are essentially the same as that of pure copper. CMW 3 sand cast- ings have a high impact strength, which is retained at elevated temperatures. Up to 410 °C (770 °F), the impact strength will not fall below 41 J (30 ft · lbf). The alloy has twice the creep strength of hard drawn copper wire at 100 °C (212 °F...
Journal Articles
Alloy Digest (1981) 30 (1): Cu-410.
Published: 01 January 1981
... as casting, heat treating, machining, and joining. Filing Code: Cu-410. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast bronze castability chemical composition compressive strength Copper...
Journal Articles
Alloy Digest (2018) 67 (4): Mg-83.
Published: 01 April 2018
... properties thermal properties UNS M11919 AZ91E is a general-purpose sand and investment casting alloy. Chemical Composition, wt.% (Nominal) Designation AZ91E UNS M11919 Aluminum 8.1 9.3 Copper 0.015 Manganese 0.17 0.35 Iron 0.005 Nickel 0.001 Silicon 0.2 Zinc 0.40 1.0 Total impurities, max 0.3 Magnesium...
Journal Articles
Alloy Digest (2006) 55 (9): Cu-746.
Published: 01 September 2006
... Hidurel 6 is a copper alloy with some chromium. It has high strength with high conductivity. The alloy has superior conductivity to Hidurel 5 (Alloy Digest Cu-607, July 1996) and is used for electrical applications where strength and brazing ability are major requirements. This datasheet provides...
Journal Articles
Alloy Digest (2006) 55 (10): Cu-747.
Published: 01 October 2006
... Hidurel 640 is a copper alloy with similar properties to Hidurel 6 (see Alloy Digest Cu-746, September 2006) with superior mechanical properties at high temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (1958) 7 (3): SS-71.
Published: 01 March 1958
... satisfactorily. After annealing, cast- ings can be hardened with good results. Although the alloy has good 0uidity and can be cast without internal porosity and internal cracking, it resembles Type 410 steel in its tendency toward surface stress cracking during cooling after solidification. Corrosion Resistance...
Journal Articles
Alloy Digest (2016) 65 (12): Pd-2.
Published: 01 December 2016
.../asm.ad.pd0002 It has now been found that the foregoing may be readily attained in a silver/palladium alloy for electrical applications that comprises, on a percent by width basis, 20 50 silver, 20 50 palladium, 20 40 copper, 0 0.5 nickel, 0.15 zinc, 0.1 0.3 boron, and up to one of modifying elements selected...
Journal Articles
Alloy Digest (1970) 19 (10): CI-36.
Published: 01 October 1970
...-36 cestlroIl OCTOBER 1970 DIGEST d - DATA ON WORLD WIDE METALS AND ALLOYS Pvbtirbd by Engineering Alloys Digest, Inc. Upper Monrclair. New Jersey MEEHANITE* AQ (Wear Resistant Iron) MEEHANITE AQ is a wear and abrasion resisting iron that is readily machinable as cast but may be ait hardened after...
Journal Articles
Alloy Digest (1985) 34 (6): Al-258.
Published: 01 June 1985
... properties. The alloy has a desirable combination of castabihty. pressure tightness. strength. corrosion resistance and weldability. The consequences of exceeding the impurity limits of Aluminum A3560 is as follows: (I) High copper or nickel decreases ductility and resistat,ce IO corrosion and (2) High iron...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-502.
Published: 01 March 1996
.... Producer or Source: VDM Technologies Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability joinability machinability physical properties tensile properties VDM LC-Nickel 99.2 workability...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... of Empire Steel Castings, Inc. Made under license from Carpenter Technology Corporation. U.S. Patent 3,574,601. Composition: Carbon Manganese Phosphorus Sulphur Silicon Chromium Nickel Molybdenum Copper Columbium 0.05 max 0.50 max 0.03 max 0.03 max 1 .OO max 14.50-16.50 5.50-7.00 0.50- 1 .oo 1.25-l .75 8 x...
Journal Articles
Alloy Digest (1954) 3 (11): SS-20.
Published: 01 November 1954
... and corrosion resisting stainless steel of the 18-8 type. Composition: &boll 0.07 max -ganese 0.50-0.75 sin 2.75-3.25 copper 2.00-225 Molybdenum 3.00-3.50 Beryllium 0.10-0.20 Nickel 9.75-1025 chromium 19.00-19.50 PROPERTIES Table 1 - TYPICAL TENSILE PROPERTIES -&P Qllench- Wl7Xlgilr Annealed nnsiIestren~psi...
Journal Articles
Alloy Digest (1954) 3 (10): Sn-1.
Published: 01 October 1954
... temperature, F Iron 0.08 Liquidus Temperature, F 669 Arsenic 0.10 Modulus of elasticity, psi 7,400,000 Zinc nonef Aluminum none# f Defined as 0.005% as determined on a 10 gram sample. (Small amounts of nickel and tellurium may be added.) PROPERTIES Table 1 - BRINELL HARDNESS Condition As-cast At 86°F after...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-356.
Published: 01 June 1978
.... It is readily corroded by nltrlc acid, ferric chloride, ferric sulfate, acid chromates, ammonium hydroxide, mercury or mercury compounds. Plating and Coloring: Brush Alloy 25 can be plated as easily as any commercial copper-base alloy. Copper, cadmium, chromium, gold, nickel, tin, rhodium, silver or other...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... Manganese 0.28 Magnetic permeability, at Silicon 0.60 100 oersteds Chromium 16.00 200 oersteds z: Nickel 4.25 maximum Modulus of elasticity, psi x 106 (torsion) 95 Columbium t Ta 0.27 10.5 Copper 3.30 Modulus of elasticity, psi x 106 (tension) 28.5 Iron Remainder Thermal conductivity, Btu/ftZ/in/hr...
Journal Articles
Alloy Digest (1954) 3 (1): W-1.
Published: 01 January 1954
... is an alloy charaaerized by its hi density. It is composed principally of tungsten, with & - cieot copper and nickel added ro impart desirabie properties of machinabi$y. Wherever maximum density, mass or in- ;d2 cubed in limited space+ Fansteel 77 Metal is an This alloy ca&ot be liquid cast or rolled...