Alloy Digest (1968) 17 (10): Ni-139.
Published: 01 October 1968
... NICKEL 201 is a low carbon version of Nickel 200 recommended for use in the electronic industries for service at temperatures between 600 F and 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1998) 47 (6): Ni-539.
Published: 01 June 1998
... Nickel 200 and Nickel 201 are wrought metals of commercially pure nickel that are used in specific corrosive service, such as caustic alkali environments, or for their unique physical properties, particularly in the electronics industry. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1988) 37 (11): Ni-364.
Published: 01 November 1988
... AL 200 and AL 201 alloys are wrought commercially pure nickel. They differ, as to composition, in maximum specified carbon levels (0.15 for AL 200 and 0.02 for AL 201). Strengths of both alloys in the annealed condition are similar to that of mild steel. The lower carbon AL 201 alloy has higher...
Journal Articles
Alloy Digest (1995) 44 (12): SS-624.
Published: 01 December 1995
... of carbide precipitation, and maintaining low temperature impact properties in welded sections. Chemical Composition Wt., %: Carbon Manganese Phosphorus Sulfur Silicon Chromium Nickel Nitrogen Type 201 Alloy to ASME SA-240 TvDical 0.15 max 5.50-7.50 0.060 max. 0.030 max. 1.00 max. 16.00-18.00 3.50-5.50 0.25...
Journal Articles
Alloy Digest (1995) 44 (10): SS-616.
Published: 01 October 1995
.... Aiby D@%t. k AU rights resewed. PuCfishdby: AIIoyDiga~. k/201.677.9161 hmshowlamtJpbLlnnmbolmdfw 27 CarhId Street. Or;mge. NJ. 07050 I USA sjx&amn CI fhd dasgn. ALLEGHENY LUDLUM TYPE 201 (Chromium-nickel-manganese stainless steel) ALLEGHENY LUDLUM TYPE 201 stainless steel is similar to Type 301 in many...
Journal Articles
Alloy Digest (2020) 69 (1): SS-1313.
Published: 01 January 2020
... AK Steel Type 201 is a chromium-manganese-nickel austenitic stainless steel that was developed to conserve nickel. Its properties are similar to those of Type 301. It is a lower cost alternative to Type 301 in certain environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2020) 69 (6): SS-1319.
Published: 01 June 2020
... CarTech 201 Modified is a nitrogen-strengthened, chromium-manganese-nickel, austenitic stainless steel that provides substantially higher yield and tensile strength than CarTech 304, and has general-corrosion resistance between that of CarTech 430 and CarTech 304. Compared with CarTech 201 (UNS...
Journal Articles
Alloy Digest (1985) 34 (6): Ni-316.
Published: 01 June 1985
... Nickel Welding Electrode 141 is used for shielded-metal-arc welding of Nickel 200 and Nickel 201, welding the clad side of nickel-clad steel and surfacing of steel. This electrode also is used for dissimilar welding, including joints between Nickel 200 and 201 and various iron-base and nickel-base...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-308.
Published: 01 January 1985
... Nickel Filler Metal 61 is a nickel-base alloy that is used for welding Nickel 200 and Nickel 201 to themselves and to other alloys such as stainless steel, carbon steels, copper-nickel alloys, INCONEL alloys, INCOLOY alloys and MONEL alloys. The weld metal has moderate strength and ductility...
Journal Articles
Alloy Digest (1986) 35 (10): SS-476.
Published: 01 October 1986
... AISI TYPE 201 MODIFIED is a chromium-nickel-manganese austenitic stainless steel whose composition is closely controlled to provide sufficient austenite stability for service at temperatures as low as 425 F (245 C). In the interest of minimizing sensitization (carbide precipitation) during welding...
Journal Articles
Alloy Digest (1974) 23 (2): Ni-201.
Published: 01 February 1974
... tensile properties UNITEMP 718 workability All OB UNITEMP 718 Filing Code: Ni-201 Nickel Alloy FEBRUARY 1974 DIGESTd - DATA ON WORLD WIDE METALS AND ALLOYS UNITEMP+ 718 (Precipitation-Hardenable High-Temperature Alloy) Pabhbd by Engineering Alloys Digest, 1~ Upper Montclair. New Jm UNITEMP 718...
Journal Articles
Alloy Digest (1957) 6 (7): SS-58.
Published: 01 July 1957
... ENDURO 201 is a non-hardenable austenitic chromium-nickel-manganese steel, capable of easily attaining high tensile strength and excellent ductility by moderate or severe cold working. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1967) 16 (10): SS-201.
Published: 01 October 1967
... INCOLOY nickel-iron-chromium alloy 801 is a modification of INCOLOY alloy 800. Its nominally 1% titanium content gives it improved tensile and rupture properties. It has excellent oxidation resistance up to 1600-1700 F and can be readily formed and welded. This datasheet provides information...
Journal Articles
Alloy Digest (1965) 14 (11): SS-174.
Published: 01 November 1965
... AISI 201 is a non-hardenable austenitic chromium-nickel-manganese steel, capable of easily attaining high tensile strength and excellent ductility by moderate or severe cold working. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2000) 49 (11): SS-809.
Published: 01 November 2000
... Armco 201 stainless steel is a non-hardenable austenitic chromium-nickel-manganese stainless steel that is capable of easily attaining high tensile strengths while maintaining excellent ductility when moderately or severely cold worked. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1999) 48 (11): SS-768.
Published: 01 November 1999
... J and L type 201 stainless steel is an austenitic alloy with approximately 6.5% manganese. The nickel and chromium contents are lower than typical to allow more work hardening and to obtain high tensile strengths with excellent ductility. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1999) 48 (12): SS-771.
Published: 01 December 1999
... J and L type 201LN is an austenitic chromium-nickel-manganese stainless steel with a lower carbon content and with added nitrogen compared to J and L type 201 (see Alloy Digest SS-768, November 1999). Type 201LN work hardens to high tensile strengths while maintaining good toughness, even...
Journal Articles
Alloy Digest (2007) 56 (9): SS-997.
Published: 01 September 2007
... 27.5 871 1600 96.66 14.020 130.5 18.925 55.0 DOI: 10.31399/asm.ad.ss0997 Weldability: Type 201 can be welded by all conventional methods applied to 18% Cr, 8% Ni steels. Filler wire or electrodes of the conventional chromium-nickel analyses can be used. Like other chromium-nickel 300 series austenitic...
Journal Articles
Alloy Digest (2002) 51 (2): Ni-579.
Published: 01 February 2002
... Nickel, Inc. Park 80 West-Plaza Two Saddle Brook, NJ 07663 (201) 368-4800 (201) 268-4858 (fax) or International Nickel, Inc. 400 N. Mountain Ave., Suite 218 Upland, CA 91786 (909) 946-2111 (909) 946-0197 (fax) ISSN: 002-614X INCOMAG ALLOY 1® Filing Code: Ni-579 Nickel February 2002 INCOMAG ALLOY 1®...
Journal Articles
Alloy Digest (2002) 51 (1): Ni-577.
Published: 01 January 2002
... as silver-gray pieces approximately 1.4 kg (3 lb) each. It is packaged in 345.25 kg (761 lb) steel drums, four drums per pallet, strapped, with a net weight of 1381 kg (3044 lb). Producer: International Nickel, Inc. Park 80 West-Plaza Two Saddle Brook, NJ 07663 (201) 368-4800 (201) 268-4858 (fax...