Journal Articles
Alloy Digest (2013) 62 (10): Nd-5.
Published: 01 October 2013
... NEOQUENCH-P GRADE NP-8 is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. This alloy is an isotropic...
Journal Articles
Alloy Digest (2013) 62 (5): Nd-4.
Published: 01 May 2013
... NEOQUENCH-P GRADE NP-7L is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. NP-7L is made by compression...