1-20 of 111 Search Results for

mining industry

Sort by
Journal Articles
Alloy Digest (2003) 52 (4): CS-135.
Published: 01 April 2003
... Domex Wear is a wear-resistant, very-high-strength steel that can be cold formed. It is used in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also...
Journal Articles
Alloy Digest (2003) 52 (10): SA-523.
Published: 01 October 2003
... Domex 100XF is a very-high-strength steel that can be cold formed. It finds use in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2004) 53 (3): CS-141.
Published: 01 March 2004
... AlgoTuf 500F is designed for applications that require extremely high abrasion resistance. It is one in a full range of heat treated plate products for mining and other industrial applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2002) 51 (10): SA-510.
Published: 01 October 2002
... JS30B is a high-strength, deep-hardening alloy steel that combines the properties of strength, toughness, and fatigue resistance. Applications are in the downhole and mining tool industries. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... 2004 ASM International Algoma 130 chemical composition formability hardness heat treatability highway trailers joinability machinability military applications mining industry notch toughness tensile properties weldability workability Chemical Composition, wt Composition...
Journal Articles
Alloy Digest (2009) 58 (10): SA-609.
Published: 01 October 2009
... 14NiCrMo13-4 General Characteristics: Ovako 253 is a group of carburizing steels with high hardenability. High strength combined with excellent toughness and high fatigue strength makes them well suited for applications in the mining industry. Tight alloying windows provide the grades with excellent...
Journal Articles
Alloy Digest (1976) 25 (9): SA-324.
Published: 01 September 1976
.... General Characteristics: USS AR steel is used in applications involving smooth- sliding abrasion which comprises erosion of the wear surface by friction where gouging, spalling or cutting caused by impact are absent. USS AR is intended primarily for use in the materials handling and mining industries...
Journal Articles
Alloy Digest (1977) 26 (12): CI-45.
Published: 01 December 1977
... chromium as an alloying element rather than more expensive alloying elements. HC-250 has been particularly successful in meeting the abrasion control requirements of industries such as steel, oil refining, cement, mining, asphalt, paper, chemical and pump manu- facturing. This wide variety of applications...
Journal Articles
Alloy Digest (1962) 11 (12): Cu-123.
Published: 01 December 1962
... of steel, together with resistance to corrosion of the ele- ments, is desired, this manganese bronze is applicable if oo other factor is present. Forms Available: Rods, bats aod extrusions. Applications: Slotted and perforated screens in the paper and mining industries, valve stems and disks, clutch disks...
Journal Articles
Alloy Digest (2007) 56 (7): SA-569.
Published: 01 July 2007
...-mixed concrete turbine mixer in the cement and mining industries; agitators for asphalt plants and finishers in the chemical industry; and between frame (BF) top swivel chutes and stationary chutes, liners, upper- hopper liners, and gate liners in the steel and gas industry. Producer: JFE Steel...
Journal Articles
Alloy Digest (2007) 56 (8): SA-570.
Published: 01 August 2007
.... Applications: Examples include bulldozer shovels and buckets, slush plates for bulldozers, and exterior linings of bulldozer buckets in the construc- tion and automotive industries; lining material for ready-mixed concrete turbine mixer in the cement and mining industries; agitators for asphalt plants...
Journal Articles
Alloy Digest (2007) 56 (11): SA-576.
Published: 01 November 2007
... include bulldozer shovels and buckets, slush plates for bulldozers, and exterior linings of bulldozer buckets in the construction and automotive industries; lining material for ready- mixed concrete turbine mixers in the cement and mining industries; agitators for asphalt plants and finishers...
Journal Articles
Alloy Digest (1976) 25 (4): SA-322.
Published: 01 April 1976
... USED IN MINING INDUSTRY Carbon Rockwell B Jaw Crusher Charpy Impact (700F) Material Range, % Hardness Wear Ratio* (V-Notch), ft-lb A-R 360 Wrought 0.28-0.30 360 0.72 2040 Cr-Ni-Mo Cast 0.28-0.33 500 0.29 lo-15 Pearlitic Cr-Mo 0.60-0.70 345 0.377 2-3 Pearlitic Cr-Mo 0.80-0.90 365 0.379 1.5-2.0 6Mn-1 MO...
Journal Articles
Alloy Digest (2015) 64 (3): SA-720.
Published: 01 March 2015
... resistance is from two to three times longer than S355 grade. Moreover, Fora 360 is very easily welded and has good forming properties, thereby contributing to ease of fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel...
Journal Articles
Alloy Digest (1982) 31 (8): Zn-38.
Published: 01 August 1982
...-resistant anti-galling parts, valves, industrial pulleys and sheaves, components for various types of industrial and farm equipment, lock hardware, electrical components and bushings. Manufacturer: Kidd Creek Mines Ltd. Toronto, Canada. In USA: Kidd Creek Mines Ltd. Edison. New Jersey 08837. ...
Journal Articles
Alloy Digest (1982) 31 (9): Zn-39.
Published: 01 September 1982
... bearing components, high- strength thin-wall castings, wear-resistant anti-galling parts, valves, industrial pulleys and sheaves, components for various types of in- dustrial and farm equipment, lock hardware, and electrical com- ponents. Manufacturer: Kidd Creek Mines Ltd. Toronto, Canada. In USA: Kidd...
Journal Articles
Alloy Digest (2019) 68 (10): Cu-898.
Published: 01 October 2019
..., pressure blocks for the steel industry gears, cams, high-temperature applications, mining machine parts. Producer Concast Metal Products Co. Wakeman, OH 44889, USA Tel: +1-800-626-7071 Fax: +1-724-538-3956 www.concast.com ISSN: 002-614X DOI: 10.31399/asm.ad.cu0898 ...
Journal Articles
Alloy Digest (1985) 34 (12): SA-413.
Published: 01 December 1985
... are based on wear resistance include dragline buckets, wear strips for continuous mining equipment, grizzly bars, drag chain and coal hopper docks. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (2011) 60 (3): SA-622.
Published: 01 March 2011
... is very easily welded and has good forming properties thereby contributing to ease of fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel industry, etc. Product Availability: Plate from 4 mm (3/16 in.) to 60 105 mm (2.4...
Journal Articles
Alloy Digest (1983) 32 (8): SA-392.
Published: 01 August 1983
... temperatures. Industry applications are mining equipment, large vehicles, cranes, earth moving equipment and others. It also is used to weld other low-alloy steels and carbon steels for a variety of uses. Manufacturer: Tri-Mark Inc. Piqua. Ohio 45356. ...