1-20 of 320 Search Results for

mining applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2004) 53 (4): CS-142.
Published: 01 April 2004
... Algoma 100 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for construction, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (2): CS-140.
Published: 01 February 2004
... AlgoTuf 440F is designed for wear resistance and is one in a full range of heat-treated plate products by Algoma Steel for construction, mining, manufacturing, and military applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2013) 62 (12): CS-176.
Published: 01 December 2013
... AlgoTuf 400F is designed for superior wear resistance and is one in a full range of heat-treated plate products for construction, mining, manufacturing, and military applications. This alloy is more formable with less preheat than the other abrasion-resistant heat-treated steel plates...
Journal Articles
Alloy Digest (2014) 63 (2): CS-179.
Published: 01 February 2014
... Swebor 450 (hardness 450 HBW) is a high-strength steel with good wear resistant qualities. It is used in applications where demands on wear resistance are high. These include loader buckets, mining truck bodies, wearing parts of agricultural machines, wearing parts of mining machines, waste...
Journal Articles
Alloy Digest (1982) 31 (8): Zn-38.
Published: 01 August 1982
... applications. It is particularly well suited to liquid and gas-pressure applications. l KIDD is a registered trademark of Kidd Creek Mines Ltd. Composition: (ASTM B 66980) Physical Constants: Aluminum 10.5-I 1.5 Copper 0.5-l .25 Magnesium 0.01 s-0.030 Iron 0.075 max. Lead 0.004 max. Cadmium 0.003 max. Tin...
Journal Articles
Alloy Digest (2004) 53 (3): CS-141.
Published: 01 March 2004
... AlgoTuf 500F is designed for applications that require extremely high abrasion resistance. It is one in a full range of heat treated plate products for mining and other industrial applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... Algoma 130 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for highway trailers, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (1982) 31 (9): Zn-39.
Published: 01 September 1982
... KIDD Alloy ZA-27 is a zinc-aluminum-copper high-strength foundry alloy. It is well suited to structural applications, once the exclusive domain of malleable cast iron, bronzes and aluminum. ZA-27 offers an as-sand-cast tensile strength of 58,000 to 64,000 psi at modest cost; also, it can be cast...
Journal Articles
Alloy Digest (1985) 34 (12): SA-413.
Published: 01 December 1985
.... It is hot formable without property loss and cold formable at high strength levels. The steel has good elevated- temperature properties. Applications which are based on wear resistance include dragline buckets, wear strips for continuous mining equipment, grizzly bars. drag chain and coal hopper docks...
Journal Articles
Alloy Digest (2004) 53 (1): CS-139.
Published: 01 January 2004
... AlgoTuf 450F is one of a full range of heat-treated plate products for construction, mining, manufacturing and military applications. This datasheet provides information on composition as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (2002) 51 (10): SA-510.
Published: 01 October 2002
... JS30B is a high-strength, deep-hardening alloy steel that combines the properties of strength, toughness, and fatigue resistance. Applications are in the downhole and mining tool industries. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1968) 17 (1): SA-221.
Published: 01 January 1968
... Bethlehem RQ-100A is a roller-quenched and tempered constructional alloy steel for applications such as bridges, buildings, derricks, mining equipment, earth moving equipment, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1966) 15 (7): SA-198.
Published: 01 July 1966
... STELCOLOY-S is a high-strength low-alloy steel recommended where high yield strength combined with toughness are required in such applications as earth moving equipment, railroad and mine cars and bridges. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1977) 26 (5): SA-332.
Published: 01 May 1977
... USS AR 360 is a quenched-and-tempered low-alloy steel designed to fit a broad range of applications where resistance to abrasion is a major consideration. It is used to produce components for mining and materials handling equipment and agricultural implements. This datasheet provides information...
Journal Articles
Alloy Digest (1983) 32 (8): SA-392.
Published: 01 August 1983
... for single and multiple-pass welding. It has outstanding low-temperature impact properties. Its applications including mining equipment, large vehicles and similar items. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2011) 60 (7): SA-628.
Published: 01 July 2011
..., and earth-moving applications include skimmers, crusher, bunkers and bulldozers. Cement plant applications include scrapers, crushers, and bunkers. Coal and other mine applications include winding and discharging machines, crushers, and conveyors. Iron and steel industry applications include bunkers...
Journal Articles
Alloy Digest (1991) 40 (6): TS-75.
Published: 01 June 1991
... Available: Billet, square and round bar, flats, hollow bar. Applications: Cam tracks, bar mill delivery guides, gages, various dies, large journal bushings for mining applications and others where high impact suength and wear resistance are im- portant. Manufacturer: Lauobe Steel Company Subsidiary...
Journal Articles
Alloy Digest (2003) 52 (4): CS-135.
Published: 01 April 2003
... Domex Wear is a wear-resistant, very-high-strength steel that can be cold formed. It is used in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1968) 17 (5): SA-226.
Published: 01 May 1968
... qualities. Forms Available: Hot rolled sheet and plate, coils and cut lengths. Applications: .\utomobile, truck, railroad, trailer, construction and mining equipment. Manufacturer: Jones 8i Laughlin Steel Corporation Pittsburgh, Pennsylvania 15230 Suggested Minimum Inside Bend Radius Thickness Inches...
Journal Articles
Alloy Digest (2014) 63 (2): SA-693.
Published: 01 February 2014
... from 8 mm (0.3 in.) and up. All plates are UT tested and controlled against class S2, E2, according to EN 10160. Applications: Quend 700 is recommended for the following applications: Truck chassis Lifting and hosting equipment Handling equipment Trailers Mining and earthmoving machinery...