Alloy Digest (2004) 53 (2): Ni-508.
Published: 01 February 2004
... Nicrofer 3033 is a high-chromium austenitic material for service in hot mineral acids and mixed acids. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1999) 48 (4): Ni-550.
Published: 01 April 1999
... Carpenter alloy C-276 is a Ni-Mo-Cr-W alloy with good fabricability. The alloy is balanced to provide excellent corrosion resistance to a variety of chemical process environments. This alloy has provided resistance to hot contaminated mineral acids, organic and inorganic chloride contaminated...
Journal Articles
Alloy Digest (1959) 8 (10): Ni-54.
Published: 01 October 1959
... NIONEL is a nickel-base alloy having high resistance to corrosive attack by oxidizing chemicals and to pitting attack by sea water. It is corrosion resistant to mixed mineral acids. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1995) 44 (8): SS-605.
Published: 01 August 1995
... URANUS B28 is an iron-31 nickel-27 chromium-3.5 molybdenum alloy for corrosion conditions, including mineral acids, even when they are contaminated with chlorides and fluorides. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (1993) 42 (1): Ni-421.
Published: 01 January 1993
... INCONEL ALLOY 686 has a higher Cr + Mo + W content than the current generation of corrosion-resistant nickel-base alloys and exhibits improved corrosion resistance over them. The alloy could be used in reducing mineral acids and FGD equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (8): Cu-443.
Published: 01 August 1982
... Copper Alloy No. C60800 is a medium-strength aluminum bronze containing nominally 95% copper and 5% aluminum. It has good resistance to atmospheric corrosion and its resists attack by nonoxidizing mineral acids such as sulfuric, hydrochloric and phosphoric. It is used widely for tubing in such...
Journal Articles
Alloy Digest (1964) 13 (10): Zr-1.
Published: 01 October 1964
... ZIRCONIUM GR. II is a hafnium bearing zirconium alloy recommended for industrial corrosion applications. It is a high strength alloy designed for service in alkalies and all but the strongest of mineral acids. This datasheet provides information on composition, physical properties, hardness, and...
Journal Articles
Alloy Digest (1963) 12 (5): Ni-82.
Published: 01 May 1963
... CORRONEL 220 is a high molybdenum nickel-base alloy having high strength and high acid resistance. It is a vanadium stabilised variant of the alloy formerly known as CORRONEL B. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1996) 45 (3): SS-5.
Published: 01 March 1996
... angles. 15-20 lip angle, and minimum clearance. Depth of cut and feed should be great enough to get below the work-hardened skin. Use chip curlers or chip breakers. Soluble oil or sulfurized mineral oil is recommended as the cutting fluid. Corrosion Resistance: Suhric Acid. Dmimet 20 is best known for...
Journal Articles
Alloy Digest (1966) 15 (6): SS-182.
Published: 01 June 1966
... Carpenter Stainless 20Cb-3 is an austenitic stainless steel designed for improved resistance to sulfuric acid. It finds wide use in all phases of the chemical industry. It has good mechanical properties and comparative ease of fabrication. Columbium stabilizes the alloy to minimize carbide...
Journal Articles
Alloy Digest (2002) 51 (4): SS-848.
Published: 01 April 2002
... corrosion resistance lies at the lower durability limit for stainless steels. The alloy therefore offers resistance only to dilute acids, water, and steam. The alloy possesses a higher resistance to corrosion when highly polished or precision ground. It is used principally as apparatus for the mineral oil...
Journal Articles
Alloy Digest (1971) 20 (8): Pd-1.
Published: 01 August 1971
... corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Pd-1. Producer or source: Engelhard Minerals and Chemicals Corporation. Producer or Source: Engelhard Minerals and Chemicals Corporation Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1996) 45 (9): Ni-516.
Published: 01 September 1996
... oxidizing media, such as nitric acid, and solutions containing ferric ions, cupric ions, or dissolved oxygen C-2000 alloy, with its high chromium content (23 wt exhibits excellent resis- tance. Figures 1.2, and 3 cover the above-noted mineral acids. Tables 2,3. and 4 are given to cover uniform corrosion...
Journal Articles
Alloy Digest (1957) 6 (8): Ni-36.
Published: 01 August 1957
... HASTELLOY ALLOY B is a nickel-molybdenum-iron alloy well suited for equipment handling boiling hydrochloric acid and wet hydrochloric acid gas. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... other highly oxidizing acids. Table 2 shows some comparative studies in several mineral acids. Table 3 shows the results of a stress-corrosion cracking test. Resistance to wet process phos- HASTELLOY® ALLOY G-35 Filing Code: Ni-622 Nickel July 2004 HASTELLOY® ALLOY G-35 (Corrosion-Resistant Nickel...
Journal Articles
Alloy Digest (2001) 50 (8): SS-828.
Published: 01 August 2001
... food. It shows good resistance to commercial grades of detergent and alkaline solutions, such as caustic soda, sodium carbonate, and ammonium hydroxide. It is not resistant to other mineral acids or to chlorides. Oxidation Resistance: The alloy has satisfactory resistance to 850 °C (1562 °F) for...
Journal Articles
Alloy Digest (1955) 4 (4): Fe-7.
Published: 01 April 1955
... should be carefully preheated to approxi- mately 1600 F. and after welding, the part should be given a controlled slow cooling. It is usually welded with the oxyacetylene flame. Has high resistance to such acids as sulphuric, nitric, hydrochloric, acetic and most other mineral and or- ganic acids. The...
Journal Articles
Alloy Digest (1956) 5 (11): Cu-44.
Published: 01 November 1956
... NI-VEE TYPE E is a precipitation hardening leaded-nickel bearing bronze suitable for bearings and acid-resisting castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as deformation. It also...
Journal Articles
Alloy Digest (1958) 7 (5): Cu-63.
Published: 01 May 1958
... REVERE No. 430 is an aluminum bronze having high strength, excellent corrosion resistance, and high resistance to sulfuric acid. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low and high...
Journal Articles
Alloy Digest (1993) 42 (1): Fe-98.
Published: 01 January 1993
.... Consult the producer for additional details. DOI: 10.31399/asm.ad.fe0098 Copyright © ASM International® 1996 Corrosion Resistance: Has high resistance to such acids as sulfuric, nitric, hy- drochloric, acetic and most other mineral and organic acids. The principal exceptions are hydrofluoric, sulfu- rous...