Alloy Digest (1987) 36 (11): Be-7.
Published: 01 November 1987
... BRUSH WELLMAN I-220 is an instrument grade of beryllium strengthened by a dispersion of 2.2% beryllium oxide maximum. It has a micro-yield strength of 5000 psi minimum. I-220B is manufactured from impact ground powder and therefore is more isotropic than BRUSH WELLMAN S-200E. I-220 is often used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (10): SA-733.
Published: 01 October 2015
... PERFORM 500 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 500 in the title refers to the minimum yield strength in MPa (72.5 ksi). The USA equivalent is Perform 72.5. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (11): SA-734.
Published: 01 November 2015
... PERFORM 550 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 550 in the title refers to the minimum yield strength in MPa (80 ksi). The USA equivalent is Perform 80. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (12): SA-737.
Published: 01 December 2015
... PERFORM 600 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 600 in the title refers to the minimum yield strength in MPa (87 ksi). The USA equivalent is Perform 78. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (1): SA-739.
Published: 01 January 2016
... PERFORM 650 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 650 in the title refers to the minimum yield strength in MPa (94 ksi). The USA equivalent is Perform 94. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (2): SA-741.
Published: 01 February 2016
... PERFORM 700 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 700 in the title refers to the minimum yield strength in MPa (102 ksi). The USA equivalent is Perform 102. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (5): SA-725.
Published: 01 May 2015
... PERFORM 315 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 315 in the title refers to the minimum yield strength in MPa. The USA equivalent is Perform 45. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (6): SA-726.
Published: 01 June 2015
... PERFORM 355 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 355 in the title refers to the minimum yield strength in MPa (51 ksi). The USA equivalent is Perform 50. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (7): SA-727.
Published: 01 July 2015
... PERFORM 380 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 380 in the title refers to the minimum yield strength in MPa (55 ksi). The USA equivalent is Perform 55. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (8): SA-729.
Published: 01 August 2015
... PERFORM 420 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 420 in the title refers to the minimum yield strength in MPa (61 ksi). The USA equivalent is Perform 60. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (9): SA-730.
Published: 01 September 2015
... PERFORM 460 is one of the Perform series of steels, which are low carbon micro-alloyed steels that are thermomechanically rolled. The 460 in the title refers to the minimum yield strength in MPa (67 ksi). The USA equivalent is Perform 67. This datasheet provides information on composition, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (3): SS-1117.
Published: 01 March 2012
... and Custom 465 are registered trademarks of CRS Holdings Inc. Table 1 Typical room temperature mechanical properties Micro-Melt BioDur Custom 470 Stainless Condition 0.2% yield strength, MPa (ksi) Ultimate tensile strength, MPa (ksi) Hardness, HRC Annealed/CT 779 (113) 979 (142) Annealed + CT + H900 (480...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (3): SS-1137.
Published: 01 March 2013
.../m·K (Btu/h·ft·°F)) 14.6 (8.4) Mechanical Properties: 0.2% yield strength, MPa (ksi) 230 (33) Ultimate tensile strength, MPa (ksi) 450 (65) Elongation, l = 5d 8% for centrifugal tubes 6% for static castings Elastic modulus, 20 ºC (68 ºF), GPa (106 psi) 160 (23) Tensile properties (for wall thickness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Ni-708.
Published: 01 May 2013
..., see Table 1. Mechanical Properties: Tensile properties (for wall thickness less than 25 mm, or 1.0 in., in the as cast condition). Minimum properties at 20 °C (68 °F). For additional mechanical properties see figures 1-3. 0.2% yield strength, MPa (ksi) 290 (42) Ultimate tensile strength, MPa (ksi) 490...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (7): SS-1148.
Published: 01 July 2013
... H101 Micro is similar to that of other heat resistant alloys with low carbon. Oxidation Resistance: See Fig. 4. Specification Equivalents: EN GX13NiCrSiNbTi37-25 Centralloy is a registered trademark of Schmidt + Clemens GmbH. Fig. 1 Typical tensile strength and 0.2% yield strength vs. temperature Fig...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (7): Ni-587.
Published: 01 July 2002
...), as-cast, wall thickness less than 25 mm Yield strength, 0.2%, MPa (ksi) 245 (35.5) min Tensile strength, MPa (ksi) 450 (65.3) min Elongation, l = 5d, % Centricast tubes 6 min Static castings 3 min See also Fig. 2 and 3. Machinability: In general terms, the machinability of ET 45 Micro is similar...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (9): SA-633.
Published: 01 September 2011
... JFE880NH increases (Fig. 1). The yield point and elongation gradually decrease as the diameter increases. Guaranteed properties: Tensile strength at any diameter, 880 MPa (128 ksi) or greater Elongation, 15% or greater Hardness, 258 or greater in Brinell Hardness Scale The hardness distribution...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (8): SA-478.
Published: 01 August 1994
...-0.0150 n/a Tensile requirement for Class 2 Plate to A387 Tensile strength, KS1 (MPa) 85 to 110 (585 to 760) Yield strength, mm. KS1 (MPa) 60 (415) Elongation in inches (50mm). min. % 18 Reduction of area, min. % 45 (40) round (flat) Specimen Toughness min. charpy v-notch at OF 40 Ave. (3 specimens...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (11): SS-1231.
Published: 01 November 2015
... or final design. NCORR is a trademark, while Micro-Melt is a registered trademark of CRS Holdings, Inc. Table 1 Typical room temperature mechanical properties Condition 0.2% yield strength, MPa (ksi) Ultimate tensile strength, MPa (ksi) Elongation in 4D, % Reduction of area, % Charpy V-notch, J (ft·lbf...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (10): SS-979.
Published: 01 October 2006
... EnduraMet 33 is a high-manganese austenitic stainless steel with high yield strength. It is also nitrogen strengthened. This data sheet covers its use as rebar. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...